    Tracking Carbonation-Induced Structural Decomposition of Synthesized Tobermorite

    by Ryusei Igami, Go Igarashi, Daisuke Minato, Ryo Kurihara, Kunio Matsui, Takayoshi Fujimura, Abudushalamu Aili, Tsuyoshi Saito, Ippei Maruyama

    Calcium-(aluminate)-silicate-hydrate (C-(A)-S-H) is the main binding phase in hardened cement paste and is the major phase responsible for CO2 uptake during carbonation. Previous studies on synthesized C-(A)-S-H and hardened cement paste have mainly focused on the decalcification of high-Ca/(Si+Al) C-(A)-S-H and the transition from decalcification to decomposition under carbonation or Ca-leaching conditions. However, the structural evolution of C-(A)-S-H during the decomposition stage and after nearly complete carbonation remains insufficiently understood. In this study, synthesized tobermorite was selected as a crystalline structural model of C-(A)-S-H, and its carbonation-induced structural evolution was investigated using X-ray diffraction, 29Si MAS NMR, 1H-29Si HETCOR NMR, 1H NMR relaxometry, and water vapor sorption measurements. During decalcification and decomposition, the original silicate environments of tobermorite transformed into silica-gel-like structures. Simultaneously, the tobermorite (002) reflection shifted and broadened, indicating an increase in mean basal spacing and stacking disorder. These changes were attributed to the removal of Ca from the interlayer spaces and the Ca–O layer, weakening Ca-based charge compensation and the structural constraints that maintain periodic layer stacking. The eventual disappearance of the (002) reflection indicated the loss of periodic layered ordering. Near complete carbonation, the NBO (non-bridging oxygen)/Si ratio showed a transient increase followed by a decrease, indicating transient depolymerization and subsequent repolymerization of the silicate structure. Even after the degree of carbonation reached approximately 100 %, pore coarsening continued despite the nearly constant NBO/Si ratio, suggesting continued rearrangement of the silica-gel-like structure without substantial further changes in the average silicate connectivity.

  • Open Access

    Application of acid digestion-based total inorganic carbon measurement for carbonated cement-based materials

    by Ryo Kurihara, Luge Cheng, Ryusei Igami, Zhenzhen Wang, Abudushalamu Aili, Kiyuki Noto, Minako Tanaka, Haruka Takahashi, Ippei Maruyama