ZYZhenyuan Yang

Zhenyuan Yang

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Zhenyuan Yang has a total of 8 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Behaviors of damaged GFRP-confined concrete columns subjected to eccentric compression

    by Qingping Jin, Jinfeng Fan, Dian Zhou, Aihua Du, Zhenyuan Yang

    To investigate the mechanical response of a concrete-filled glass fiber-reinforced polymer (GFRP) tube with initial damage under eccentric compression, a total of 21 specimen types were designed and fabricated, incorporating slenderness ratio, eccentricity, damage length, and damage location as variable parameters. Static eccentric compression loading tests were performed. A comprehensive comparative study was undertaken focusing on the mechanisms of damage nucleation and evolution, load–displacement curves, and the variation patterns of ultimate load-bearing capacity. Additionally, the ultimate load-bearing capacity of GFRP-confined concrete columns with initial damage was calculated. The findings reveal that damage on the compression side is particularly detrimental, exerting a substantially greater adverse effect than damage on the tension side. Stress concentration at the damage tip initiates the propagation of complex cracks, forming plastic hinges and altering the stress transfer path. Despite the damage, the internal concrete retains partial confinement through the arching effect. The presented study introduces reduction coefficients for slenderness ratio and eccentricity, resulting in a formula for predicting the ultimate load-bearing capacity of GFRP-confined concrete columns, considering the influence of damage location on strength. The calculated results are generally consistent with the experimental results.

  • Axial compression behavior of concrete columns with mixed reinforcement of GFRP bars and steel bars

    by Qingping Jin, Zhenyuan Yang, Guangbo Wang, Aihua Du

    Concrete columns reinforced with GFRP bars, partially or fully replacing steel, can effectively meet the durability requirements of structures in corrosive environments. Axial compression tests were conducted on four groups of concrete columns with hybrid (mixed) reinforcement and single-type reinforcement. The results show that all specimens failed by concrete splitting, with several longitudinal bars buckling and extensive the concrete cover spalling at failure. In terms of ductility, specimens with hybrid longitudinal reinforcement and GFRP stirrups exhibited the highest value. Under conventional steel stirrup conditions, variations in longitudinal reinforcement configuration minimally affected ductility, whereas specimens reinforced entirely with GFRP bars exhibited the lowest ductility. The ultimate load capacity formula, which comprehensively accounts for the contributions of both longitudinal and transverse reinforcement, yielded theoretical values in close agreement with the experimental results. The test results indicate that the utilization rate of stirrups at the mid-height of hybrid reinforcement columns is greater than that in columns with only ordinary steel or only GFRP reinforcement. The reinforcement configuration showed little influence on the mechanical performance of the concrete itself in the columns. In terms of longitudinal reinforcement utilization, the hybrid steel-GFRP-reinforced columns performed better than those reinforced with GFRP bars alone.

  • Axial compression performance and calculation model of GFRP tube-concrete-steel tube composite columns

    by Qingping Jin, Zhenyuan Yang, Bowen Yang, Zongjian Lei

    This study systematically investigates the axial compression behavior of double-skin tubular short columns incorporating an external glass fiber-reinforced polymer (GFRP) tube, machine-made sand concrete, and an internal steel tube. Through axial compression tests on seven specimen groups with varying design parameters, the effects of GFRP tube thickness, hollow ratio, steel tube diameter-to-thickness ratio, and concrete core strength were examined. The results demonstrate a remarkable synergistic interaction among the constituent materials, enabling the composite columns to achieve an ultimate load capacity 1.27 to 2.05 times the sum of their individual nominal capacities. Among all parameters, GFRP tube thickness exhibited the most pronounced influence: increasing the thickness from 3 mm to 4 mm and 5 mm enhanced the ultimate load capacity by 32.2% and 58.3%, respectively. While reducing the steel tube diameter-to-thickness ratio from 16 to 8 improved load capacity, its effect on ultimate strain enhancement remained relatively limited. A predictive model for ultimate load capacity was developed using the superposition principle, comprehensively accounting for the lateral confinement contributions from both the GFRP and steel tubes. Validation against experimental results and existing literature data confirms the model’s high predictive accuracy.

  • Degradation Mechanism and Predictive Model of GFRP Bar‐Concrete Interfacial Bonding Behavior Under Alkaline Conditions

    by Zhenyuan Yang, Qingping Jin, Peixia Chen, Zongjian Lei

    This study examined the degradation of GFRP bars and their bond behavior with concrete under alkaline conditions. Two specimen types were prepared: a damaged group preloaded to 25% of the ultimate bond load and an undamaged group. Both were exposed to alkaline environments via static immersion and wet‐dry cycling. Macroscopic mechanical properties and interfacial micro‐morphology were evaluated after 30, 90, 150 days of aging. Results show that after 150 days, compared to non‐immersed specimens, the tensile strength of GFRP bars decreased by 20.44%–25.76% in the undamaged group and by 28.17%–29.83% in the damaged group. Bond strength was most significantly influenced by immersion duration, decreasing by up to 62.67% and 44.3% for the damaged and undamaged groups, respectively, compared to non‐corroded specimens. Microscopic analysis revealed that prolonged immersion loosened the bar‐concrete interface, accelerating OH − penetration. This promoted resin matrix hydrolysis (N content decreased from 14.84% to 0%) and fiber damage (Si content increased from 1.81% to 21.10%), resulting in continuous bond deterioration. Based on the results, a bond strength prediction model was developed using a 16 mm bar diameter threshold; a time‐dependent bond strength model under natural exposure in an alkaline environment was developed using cumulative heat, and a single‐logarithmic model.