Şenol Avcı
Research Subjects
Şenol Avcı has a total of 5 co-authors. Here are the top co-authors by number of shared publications:
- Kelani G. K. Elattousi1 shared publication
- Onur Yiğit Özger
Vocational School, Bilecik Şeyh Edebali University , 11100 , Bilecik , Turkey
1 shared publication Recep Artır
Marmara University
1 shared publicationSakin Zeytin
Sakarya University
1 shared publication- Özkan Küçük
Bilecik Şeyh Edebali Üniversitesi
1 shared publication
Latest Publications
- 9 July 2026
- Published by Taylor & Francis in Canadian Metallurgical Quarterly
- p. 1-17
Influence of sodium phosphate additives on densification, phase evolution and mechanical properties of hydroxyapatite
Hydroxyapatite (HA, Ca₁₀(PO₄)₆(OH)₂) is one of the most widely used bioceramics in biomedical applications due to its excellent biocompatibility, bioactivity, and close chemical and crystallographi...
- 9 July 2026
- Published by Taylor & Francis in Canadian Metallurgical Quarterly
- p. 1-17
Influence of sodium phosphate additives on densification, phase evolution and mechanical properties of hydroxyapatite
Hydroxyapatite (HA, Ca₁₀(PO₄)₆(OH)₂) is one of the most widely used bioceramics in biomedical applications due to its excellent biocompatibility, bioactivity, and close chemical and crystallographi...
- 30 November 2025
- Published by Bilecik Seyh Edebali Universitesi Fen Bilimleri Dergisi in Bilecik Şeyh Edebali Üniversitesi Fen Bilimleri Dergisi
- Vol. 12 (2) , 547-554
Investigation of Microstructure and Mechanical Properties of X70M Steels Welded by Submerged Arc Welding
In this study, X70M PSL 2 (API 5L) steel used in oil pipelines was welded by submerged arc welding method. Weld seam and HAZ were characterized by optical microscopy, scanning electron microscopy (SEM), tensile test, hardness test and Charpy impact test methods. As a result of the optical inspection, it was observed that no welding defects had occurred within the structure. The weld zone, base metal, and HAZ are distinct, and columnar grain growth has occurred in the weld metal. In the SEM study, it was observed that the base material consists of ferrite grains (angular ferrite, polygonal ferrite), the HAZ consists of coarser grains, and the weld metal consists of fine columnar ferrite. As a result of the tensile test, it was determined that the tensile strength of the base material is approximately 648 MPa, while the tensile strength of the welded joint is approximately 695 MPa. The obtained results indicate that the fracture in the welded joint occurred in the base material. The highest average hardness value was measured as 229 HV in the weld metal. In contrast, the average hardness values in the base material and HAZ are 218 HV and 221 HV, respectively. The average impact energy value obtained in the base material is 428 J. The lowest impact energy was obtained in the weld metal. The average impact energy value obtained in the weld metal is approximately 94 J. As one moves from the weld metal towards the base material, the increase in impact energy is remarkable.
- 30 November 2025
- Published by Bilecik Seyh Edebali Universitesi Fen Bilimleri Dergisi in Bilecik Şeyh Edebali Üniversitesi Fen Bilimleri Dergisi
- Vol. 12 (2) , 547-554
Investigation of Microstructure and Mechanical Properties of X70M Steels Welded by Submerged Arc Welding
In this study, X70M PSL 2 (API 5L) steel used in oil pipelines was welded by submerged arc welding method. Weld seam and HAZ were characterized by optical microscopy, scanning electron microscopy (SEM), tensile test, hardness test and Charpy impact test methods. As a result of the optical inspection, it was observed that no welding defects had occurred within the structure. The weld zone, base metal, and HAZ are distinct, and columnar grain growth has occurred in the weld metal. In the SEM study, it was observed that the base material consists of ferrite grains (angular ferrite, polygonal ferrite), the HAZ consists of coarser grains, and the weld metal consists of fine columnar ferrite. As a result of the tensile test, it was determined that the tensile strength of the base material is approximately 648 MPa, while the tensile strength of the welded joint is approximately 695 MPa. The obtained results indicate that the fracture in the welded joint occurred in the base material. The highest average hardness value was measured as 229 HV in the weld metal. In contrast, the average hardness values in the base material and HAZ are 218 HV and 221 HV, respectively. The average impact energy value obtained in the base material is 428 J. The lowest impact energy was obtained in the weld metal. The average impact energy value obtained in the weld metal is approximately 94 J. As one moves from the weld metal towards the base material, the increase in impact energy is remarkable.
- Open Access
- 1 January 2025
- Published by Walter de Gruyter GmbH in Open Chemistry
- Vol. 23 (1)
Growth kinetics and mechanical characterization of boride layers formed on Ti6Al4V
Although Ti6Al4V alloy is used in a wide variety of engineering fields such as automotive, aerospace, chemical, marine, and medical, it has significant disadvantages such as low hardness and wear resistance. The boriding process, which is one of the methods applied to improve the surface properties of the material, is based on the principle of increasing the surface quality of the material by creating a TiB 2 and TiB layer on the surface of the material by boron diffusion. Although many methods are used for boriding of Ti6Al4V alloy, the pack boriding method preferred in this study attracts attention because it is a cheap and easy method. This present study focuses on the characterization of the boride layer formed on Ti6Al4V alloy borided at 950, 1,050, and 1,150°C for 5 and 15 h using two different recipes (M-1 and M-2). In addition, the activation energies of boron diffusion calculated using the TiB 2 layer thicknesses measured from optical images of all samples, including 10 h borided samples, are included in the article.
- 1 January 2025
- Published by Walter de Gruyter GmbH in Open Chemistry
- Vol. 23 (1)
Open AccessGrowth kinetics and mechanical characterization of boride layers formed on Ti6Al4V
Although Ti6Al4V alloy is used in a wide variety of engineering fields such as automotive, aerospace, chemical, marine, and medical, it has significant disadvantages such as low hardness and wear resistance. The boriding process, which is one of the methods applied to improve the surface properties of the material, is based on the principle of increasing the surface quality of the material by creating a TiB 2 and TiB layer on the surface of the material by boron diffusion. Although many methods are used for boriding of Ti6Al4V alloy, the pack boriding method preferred in this study attracts attention because it is a cheap and easy method. This present study focuses on the characterization of the boride layer formed on Ti6Al4V alloy borided at 950, 1,050, and 1,150°C for 5 and 15 h using two different recipes (M-1 and M-2). In addition, the activation energies of boron diffusion calculated using the TiB 2 layer thicknesses measured from optical images of all samples, including 10 h borided samples, are included in the article.