Honghui Liu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Honghui Liu has a total of 21 co-authors. Here are the top co-authors by number of shared publications:
- Jingya Cui
Qinghai Provincial Key Laboratory of Nanomaterials and Technology, School of Chemistry and Materials Science, Qinghai Minzu University, Xining 810007, China
3 shared publications - Tong Mu
Key Laboratory of Green and High-End Utilization of Salt Lake Resources, Key Laboratory of Salt Lake Resources Chemistry of Qinghai Province, Qinghai Institute of Salt Lakes, Chinese Academy of Sciences, Xining 810008, China
3 shared publications - Lingyun An
Qinghai Provincial Key Laboratory of Nanomaterials and Technology, School of Chemistry and Materials Science, Qinghai Minzu University, Xining 810007, China
2 shared publications - Xiushen Ye
Key Laboratory of Green and High-End Utilization of Salt Lake Resources, Key Laboratory of Salt Lake Resources Chemistry of Qinghai Province, Qinghai Institute of Salt Lakes, Chinese Academy of Sciences, Xining 810008, China
2 shared publications - Yao Li
Qinghai Provincial Key Laboratory of Nanomaterials and Technology, School of Chemistry and Materials Science, Qinghai Minzu University, Xining 810007, China
2 shared publications - Yongcai Zhang
AECC South Industry Company Limited, Zhuzhou 412002, China
2 shared publications
Latest Publications
- Open Access
Effect of Sr Microalloying on the Microstructure, Solution-Treatment Response, and Age-Hardening Behavior of Mg-Nd-Gd-Zn-Zr Alloy
Mg-Nd-Gd-Zn-Zr alloys containing 0, 0.20, and 0.75 wt.% Sr were prepared by gravity casting to investigate the effects of Sr microalloying on as-cast microstructure, solution-treatment response, and age-hardening behavior. The alloys were characterized by XRD, OM, SEM/EDS, DSC, and Brinell hardness testing. Sr was mainly enriched at grain boundaries and in secondary-phase regions, and Mg17Sr2-related diffraction peaks appeared in the Sr-containing alloys. The as-cast grain size varied non-monotonically among the three compositions investigated, with the 0.20 wt.% Sr alloy exhibiting the finest grains, whereas the area fraction of secondary phases increased continuously with Sr content. Under the selected solution-treatment conditions, the Sr-containing alloys retained smaller grains but contained larger amounts of residual secondary phases. Under the respective selected solution-treated starting states, the 0Sr alloy achieved the highest measured hardness at 200 °C, while the 0.20Sr alloy showed an earlier hardening response and a more gradual subsequent hardness evolution; the 0.75Sr alloy showed a more pronounced post-peak hardness decrease. The retained Sr-containing secondary phases may indicate incomplete dissolution of part of the Nd, Gd, and Zn, potentially reducing the effective solute reservoir in α-Mg available for subsequent aging. Within the three compositions investigated, the results indicate a trade-off between grain refinement/retention and age-hardening potential.
Open AccessEffect of Sr Microalloying on the Microstructure, Solution-Treatment Response, and Age-Hardening Behavior of Mg-Nd-Gd-Zn-Zr Alloy
Mg-Nd-Gd-Zn-Zr alloys containing 0, 0.20, and 0.75 wt.% Sr were prepared by gravity casting to investigate the effects of Sr microalloying on as-cast microstructure, solution-treatment response, and age-hardening behavior. The alloys were characterized by XRD, OM, SEM/EDS, DSC, and Brinell hardness testing. Sr was mainly enriched at grain boundaries and in secondary-phase regions, and Mg17Sr2-related diffraction peaks appeared in the Sr-containing alloys. The as-cast grain size varied non-monotonically among the three compositions investigated, with the 0.20 wt.% Sr alloy exhibiting the finest grains, whereas the area fraction of secondary phases increased continuously with Sr content. Under the selected solution-treatment conditions, the Sr-containing alloys retained smaller grains but contained larger amounts of residual secondary phases. Under the respective selected solution-treated starting states, the 0Sr alloy achieved the highest measured hardness at 200 °C, while the 0.20Sr alloy showed an earlier hardening response and a more gradual subsequent hardness evolution; the 0.75Sr alloy showed a more pronounced post-peak hardness decrease. The retained Sr-containing secondary phases may indicate incomplete dissolution of part of the Nd, Gd, and Zn, potentially reducing the effective solute reservoir in α-Mg available for subsequent aging. Within the three compositions investigated, the results indicate a trade-off between grain refinement/retention and age-hardening potential.
- 13 March 2026
- Published by Springer Nature in China Foundry
- Vol. 23 (2) , 186-196
Effect of grain size on fatigue behaviors of Mg-2.6Nd-0.35Zn-xZr alloys
- 13 March 2026
- Published by Springer Nature in China Foundry
- Vol. 23 (2) , 186-196
Effect of grain size on fatigue behaviors of Mg-2.6Nd-0.35Zn-xZr alloys
- Open Access
Optimization of T6 Heat Treatment for Enhanced Microstructural Stability and Mechanical Properties of EV31A Magnesium Alloy
This study systematically optimizes the T6 heat treatment of a commercial EV31A magnesium alloy and evaluates the resulting microstructural evolution and mechanical properties. Optical microscopy, scanning electron microscopy combined with energy-dispersive X-ray spectroscopy (SEM-EDS), X-ray diffraction (XRD), and transmission electron microscopy (TEM) were used to characterize the microstructure and phase constitution, while differential scanning calorimetry (DSC) was employed to determine appropriate solution treatment parameters. Brinell hardness measurements and tensile tests at room temperature and 150 °C were carried out to quantify the mechanical response. The as-cast alloy consists of α-Mg equiaxed grains, bone-shaped Mg12(Nd,Gd) eutectic phases at grain boundaries, and minor intragranular lath-shaped Mg12Nd phases. After T6 treatment (520 °C/10 h solution treatment + 200 °C/16 h aging), the grain boundary eutectic phases partially dissolve and transform into Mg41(Nd,Gd)5, while intragranular nano-scale β′ precipitates and stable Zn2Zr3 particles form, achieving multi-scale synergistic strengthening. Compared to the as-cast condition, the T6-treated alloy exhibits room-temperature ultimate tensile strength and yield strength of 309 ± 40.5 MPa (31% increase) and 180 ± 14.2MPa (45% increase), respectively. At 150 °C, the strength reaches 241 ± 7.5 MPa (39% increase) and 154 ± 16.8 MPa (52% increase), while maintaining an elongation of 10.9± 0.7%, demonstrating an excellent strength–ductility balance.
Open AccessOptimization of T6 Heat Treatment for Enhanced Microstructural Stability and Mechanical Properties of EV31A Magnesium Alloy
This study systematically optimizes the T6 heat treatment of a commercial EV31A magnesium alloy and evaluates the resulting microstructural evolution and mechanical properties. Optical microscopy, scanning electron microscopy combined with energy-dispersive X-ray spectroscopy (SEM-EDS), X-ray diffraction (XRD), and transmission electron microscopy (TEM) were used to characterize the microstructure and phase constitution, while differential scanning calorimetry (DSC) was employed to determine appropriate solution treatment parameters. Brinell hardness measurements and tensile tests at room temperature and 150 °C were carried out to quantify the mechanical response. The as-cast alloy consists of α-Mg equiaxed grains, bone-shaped Mg12(Nd,Gd) eutectic phases at grain boundaries, and minor intragranular lath-shaped Mg12Nd phases. After T6 treatment (520 °C/10 h solution treatment + 200 °C/16 h aging), the grain boundary eutectic phases partially dissolve and transform into Mg41(Nd,Gd)5, while intragranular nano-scale β′ precipitates and stable Zn2Zr3 particles form, achieving multi-scale synergistic strengthening. Compared to the as-cast condition, the T6-treated alloy exhibits room-temperature ultimate tensile strength and yield strength of 309 ± 40.5 MPa (31% increase) and 180 ± 14.2MPa (45% increase), respectively. At 150 °C, the strength reaches 241 ± 7.5 MPa (39% increase) and 154 ± 16.8 MPa (52% increase), while maintaining an elongation of 10.9± 0.7%, demonstrating an excellent strength–ductility balance.
- Open Access
Effect of Heat Treatment on the Microstructure and Mechanical Properties of Mg-3.2Nd-2.5Gd-0.4Zn-0.5Zr (wt.%) Alloy
This study systematically examines the influence of heat treatment on the microstructure and mechanical properties of the Mg-3.2Nd-2.5Gd-0.4Zn-0.5Zr (wt.%) alloy using optical microscopy (OM), scanning electron microscopy (SEM), transmission electron microscopy (TEM), and mechanical testing. The as-cast alloy consists mainly of an α-Mg matrix and Mg3RE intermetallic phases. Solution treatment markedly improves microstructural homogeneity by dissolving most Mg-RE phases into the α-Mg matrix. Subsequent aging induces the formation of finely dispersed rare-earth precipitates, which contribute significantly to the improvement in hardness and strength. The optimal heat-treatment parameters are a solution treatment at 520 °C for 10 h followed by aging at 200 °C for 16 h (T6). After T6 treatment, the alloy exhibits an ultimate tensile strength (UTS) of 322 ± 2.0 MPa, a yield strength (YS) of 220 ± 23.0 MPa (increases of 53% and 88% relative to the as-cast alloy), and an elongation (EL) of 8.7 ± 0.2% at room temperature. At 150 °C, the UTS, YS, and EL reach 292 ± 2.6 MPa, 185 ± 1.1 MPa (41% and 62% improvements over the as-cast state), and 16 ± 1.0%, respectively, indicating excellent mechanical performance at elevated temperatures.
Open AccessEffect of Heat Treatment on the Microstructure and Mechanical Properties of Mg-3.2Nd-2.5Gd-0.4Zn-0.5Zr (wt.%) Alloy
This study systematically examines the influence of heat treatment on the microstructure and mechanical properties of the Mg-3.2Nd-2.5Gd-0.4Zn-0.5Zr (wt.%) alloy using optical microscopy (OM), scanning electron microscopy (SEM), transmission electron microscopy (TEM), and mechanical testing. The as-cast alloy consists mainly of an α-Mg matrix and Mg3RE intermetallic phases. Solution treatment markedly improves microstructural homogeneity by dissolving most Mg-RE phases into the α-Mg matrix. Subsequent aging induces the formation of finely dispersed rare-earth precipitates, which contribute significantly to the improvement in hardness and strength. The optimal heat-treatment parameters are a solution treatment at 520 °C for 10 h followed by aging at 200 °C for 16 h (T6). After T6 treatment, the alloy exhibits an ultimate tensile strength (UTS) of 322 ± 2.0 MPa, a yield strength (YS) of 220 ± 23.0 MPa (increases of 53% and 88% relative to the as-cast alloy), and an elongation (EL) of 8.7 ± 0.2% at room temperature. At 150 °C, the UTS, YS, and EL reach 292 ± 2.6 MPa, 185 ± 1.1 MPa (41% and 62% improvements over the as-cast state), and 16 ± 1.0%, respectively, indicating excellent mechanical performance at elevated temperatures.