Tong Lv
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Tong Lv has a total of 6 co-authors. Here are the top co-authors by number of shared publications:
- Chuanhao Cao
Harbin university of science and technology, China
1 shared publication - Lizhu Liu
School of Materials Science and Engineering, Harbin University of Science and Technology, Harbin, People’s Republic of China
1 shared publication - Xiaorui Zhang
School of Material Science and Chemical Engineering, Harbin University of Science and Technology, Harbin, China
1 shared publication - Xinyu Ma
Jiangsu Engineering Laboratory of Novel Functional Polymeric Materials, Jiangsu Key Laboratory of Advanced Negative Carbon Technologies College of Chemistry, Suzhou Key Laboratory of Soft Material and New Energy, College of Chemistry, Chemical Engineering and Materials Science
1 shared publication Yanmei Ren
Tianjin Polytechnic Univ. (China)
1 shared publicationZhenxing Tian
Tianjin Polytechnic Univ. (China)
1 shared publication
Latest Publications
- 13 January 2020
- Published by Taylor & Francis in Journal of Macromolecular Science, Part A
- Vol. 57 (5) , 398-407
Thermal conductivity of polyimide/AlN and polyimide/(AlN + BN) composite films prepared by in-situ polymerization
A series of polyimide/AlN composite films and polyimide/AlN/BN composite films with different contents were prepared by using polyimide as organic matrix, AlN and BN as inorganic fillers. The filling of the ALN + BN particles increases the dielectric constant, the breakdown strength, and the thermal conductivity of the film. After filling in 9 vol% AlN content, the thermal conductivity of the polyimide/AlN composite film was 0.675 W/(m·K), which was three times that of the pure PI film. The PI/AlN/BN composite film had a thermal conductivity of 0.711 W/(m·K) when the content of AlN and BN was 3 vol% and 6 vol%, When the inorganic packing particles are 3%, the tensile strength loss is small and the breakdown strength is increased to 180 kV/mm. The SEM image of PI film showed that when different contents of AlN particles were added to the matrix, whitening phenomenon may occur due to poor interface bonding ability, and the problem was improved after KH560 modification. The result showed that two fillers with different particle sizes formed a close-packing, which was beneficial to increase the number of thermal conduction paths, thereby improving the thermal conductivity. Overall, this paper prepared a series of PI thin films with high thermal conductivity and high insulation.
- 13 January 2020
- Published by Taylor & Francis in Journal of Macromolecular Science, Part A
- Vol. 57 (5) , 398-407
Thermal conductivity of polyimide/AlN and polyimide/(AlN + BN) composite films prepared by in-situ polymerization
A series of polyimide/AlN composite films and polyimide/AlN/BN composite films with different contents were prepared by using polyimide as organic matrix, AlN and BN as inorganic fillers. The filling of the ALN + BN particles increases the dielectric constant, the breakdown strength, and the thermal conductivity of the film. After filling in 9 vol% AlN content, the thermal conductivity of the polyimide/AlN composite film was 0.675 W/(m·K), which was three times that of the pure PI film. The PI/AlN/BN composite film had a thermal conductivity of 0.711 W/(m·K) when the content of AlN and BN was 3 vol% and 6 vol%, When the inorganic packing particles are 3%, the tensile strength loss is small and the breakdown strength is increased to 180 kV/mm. The SEM image of PI film showed that when different contents of AlN particles were added to the matrix, whitening phenomenon may occur due to poor interface bonding ability, and the problem was improved after KH560 modification. The result showed that two fillers with different particle sizes formed a close-packing, which was beneficial to increase the number of thermal conduction paths, thereby improving the thermal conductivity. Overall, this paper prepared a series of PI thin films with high thermal conductivity and high insulation.
- 13 July 2010
- Published by SPIE-Intl Soc Optical Eng
- Vol. 7749, 77490N-77490N-6
Synthesis and performance evaluation of the new thickening agent of acidizing fluid
An acid thickener, poly (AMPS-co -DMC) was synthesized using water aqueous solution polymerization of these monomers such as 2-acrylamide-2-methylpropanesulfonic acid (AMPS) and [2-(Methacryloyloxy) ethyl] trimethylammonium chloride (DMC), with ammonium persulfate and sodium sulfite redox system as initiator, while at 65°C, 25% of the total concentration of monomer, initiator dosage of 1.6% for the monomer mass and nitrogen protection condition. The paper discussed the property evaluation of poly(AMPS-co -DMC), it was shown that poly (AMPS-co -DMC) had good acid solubility (time for dissolving in acid is 21 min); acid containing 5.0% of poly(AMPSco -DMC) had a viscosity of greater than 25.0mPa•s; the shearing stability and heat resistance of the system was good and over 90% at a shear rate of 170s-1; poly(AMPS-co -DMC) performed well in the presence of standard saline at a total concentration of 40000mg/L.
- 13 July 2010
- Published by SPIE-Intl Soc Optical Eng
- Vol. 7749, 77490N-77490N-6
Synthesis and performance evaluation of the new thickening agent of acidizing fluid
An acid thickener, poly (AMPS-co -DMC) was synthesized using water aqueous solution polymerization of these monomers such as 2-acrylamide-2-methylpropanesulfonic acid (AMPS) and [2-(Methacryloyloxy) ethyl] trimethylammonium chloride (DMC), with ammonium persulfate and sodium sulfite redox system as initiator, while at 65°C, 25% of the total concentration of monomer, initiator dosage of 1.6% for the monomer mass and nitrogen protection condition. The paper discussed the property evaluation of poly(AMPS-co -DMC), it was shown that poly (AMPS-co -DMC) had good acid solubility (time for dissolving in acid is 21 min); acid containing 5.0% of poly(AMPSco -DMC) had a viscosity of greater than 25.0mPa•s; the shearing stability and heat resistance of the system was good and over 90% at a shear rate of 170s-1; poly(AMPS-co -DMC) performed well in the presence of standard saline at a total concentration of 40000mg/L.