Yu-Cheng Li
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Yu-Cheng Li has a total of 2 co-authors. Here are the top co-authors by number of shared publications:
- Yang-Zhan Lin
Department of Electrical Engineering, National Chung Hsing University, Taichung 40227, Taiwan
2 shared publications - Yeu-Long Jiang
Graduate Institute of Optoelectronic Engineering, Department of Electrical Engineering, National Chung Hsing University, Taichung 40227, Taiwan
2 shared publications
Latest Publications
- Open Access
The Influence of a-SiCx:H and a-SiOx:H Barrier Layers Embedded in the p/i and i/n Interfaces on the Performance of a-Si:H p-i-n Solar Cells
In this work, hydrogenated amorphous silicon carbide (a-SiCx:H) and hydrogenated amorphous silicon oxide (a-SiOx:H) films with similar optical bandgaps (Eg), refractive indices (n), and extinction coefficients (k) were fabricated using pulse-wave modulation (PWM) plasma technology by controlling the plasma turn-on to turn-off time ratio (ton/toff). These films were placed at the 1/5 position of the p/i and i/n interfaces of hydrogenated amorphous silicon (a-Si:H) p-i-n solar cells to investigate their influence on solar cell performance. The experimental results confirmed that the deviations in Eg, n, and k were controlled to within 0.2%, 1.4%, and 4.1%, respectively. Under these conditions, placing a-SiCx:H and a-SiOx:H films at the p/i and i/n interfaces successfully increased the open-circuit voltage (Voc). However, this also led to a decrease in the short-circuit current due to valence band (ΔEv) or conduction band (ΔEc) offsets. The reduction in cell fill factor (FF) and efficiency (η) caused by placing a-SiCx:H and a-SiOx:H films at the p/i interface was greater than that caused by placing them at the i/n interface. Placing the a-SiCx:H film at the p/i interface significantly improved the Voc to 0.8998 V. Due to the n-type doping effect of oxygen atoms, the a-SiOx:H film exhibited the lowest FF of 43.99% and η of 4.850% at the p/i interface; however, when placed at the i/n interface, it yielded an FF of 67.38% and an η of 7.43%, which are comparable to the standard cell. Appropriately placing the a-SiCx:H film at the p/i interface and the slightly n-type a-SiOx:H film at the i/n interface can effectively improve the Voc, FF, and η of p-i-n solar cells.
Open AccessThe Influence of a-SiCx:H and a-SiOx:H Barrier Layers Embedded in the p/i and i/n Interfaces on the Performance of a-Si:H p-i-n Solar Cells
In this work, hydrogenated amorphous silicon carbide (a-SiCx:H) and hydrogenated amorphous silicon oxide (a-SiOx:H) films with similar optical bandgaps (Eg), refractive indices (n), and extinction coefficients (k) were fabricated using pulse-wave modulation (PWM) plasma technology by controlling the plasma turn-on to turn-off time ratio (ton/toff). These films were placed at the 1/5 position of the p/i and i/n interfaces of hydrogenated amorphous silicon (a-Si:H) p-i-n solar cells to investigate their influence on solar cell performance. The experimental results confirmed that the deviations in Eg, n, and k were controlled to within 0.2%, 1.4%, and 4.1%, respectively. Under these conditions, placing a-SiCx:H and a-SiOx:H films at the p/i and i/n interfaces successfully increased the open-circuit voltage (Voc). However, this also led to a decrease in the short-circuit current due to valence band (ΔEv) or conduction band (ΔEc) offsets. The reduction in cell fill factor (FF) and efficiency (η) caused by placing a-SiCx:H and a-SiOx:H films at the p/i interface was greater than that caused by placing them at the i/n interface. Placing the a-SiCx:H film at the p/i interface significantly improved the Voc to 0.8998 V. Due to the n-type doping effect of oxygen atoms, the a-SiOx:H film exhibited the lowest FF of 43.99% and η of 4.850% at the p/i interface; however, when placed at the i/n interface, it yielded an FF of 67.38% and an η of 7.43%, which are comparable to the standard cell. Appropriately placing the a-SiCx:H film at the p/i interface and the slightly n-type a-SiOx:H film at the i/n interface can effectively improve the Voc, FF, and η of p-i-n solar cells.
- Open Access
- 29 December 2025
- Published by MDPI AG in Preprints.org
A-SiCx:H and A-SiOx:H Barrier Layers Embedded in the P/I and I/N Regions on the Performance of A-Si:H P-I-N Solar Cells
In this work, hydrogenated amorphous silicon carbide (a-SiCx:H) and hydrogenated amorphous silicon oxide (a-SiOx:H) films with similar optical bandgaps (Eg), refractive indices (n), and extinction coefficients (k) were fabricated using pulse-wave modulation plasma technology by controlling the plasma turn-on and turn-off time ratio (ton/toff). These films were placed at the 1/4 position of the p/i and i/n interfaces of hydrogenated amorphous silicon (a-Si:H) p-i-n solar cells to investigate their influence on solar cell performance. Experimental results showed that when deviations in Eg, n, and k were less than 0.2%, 1.4%, and 4.1%, respectively, placing a-SiCx:H and a-SiOx:H films at the p/i and i/n interfaces increased the open-circuit voltage (Voc) and decreased the short-circuit current due to valence band (ΔEv) or conduction band (ΔEc) offsets. The reduction in cell fill factor (FF) and efficiency (η) caused by placing a-SiCx:H and a-SiOx:H films at the p/i interface was greater than that caused by placing them at the i/n interface. Placing the a-SiCx:H film at the p/i interface significantly improved the Voc. Due to the n-type doping effect of oxygen atoms, the a-SiOx:H film exhibited the lowest FF and η at the p/i interface; however, when placed at the i/n interface, it yielded FF and η values second only to the a-Si:H standard reference cell. Appropriately placing the a-SiCx:H film at the p/i interface and the slightly n-type a-SiOx:H film at the i/n interface can effectively improve the Voc, FF, and η of p-i-n solar cells.
- 29 December 2025
- Published by MDPI AG in Preprints.org
Open AccessA-SiCx:H and A-SiOx:H Barrier Layers Embedded in the P/I and I/N Regions on the Performance of A-Si:H P-I-N Solar Cells
In this work, hydrogenated amorphous silicon carbide (a-SiCx:H) and hydrogenated amorphous silicon oxide (a-SiOx:H) films with similar optical bandgaps (Eg), refractive indices (n), and extinction coefficients (k) were fabricated using pulse-wave modulation plasma technology by controlling the plasma turn-on and turn-off time ratio (ton/toff). These films were placed at the 1/4 position of the p/i and i/n interfaces of hydrogenated amorphous silicon (a-Si:H) p-i-n solar cells to investigate their influence on solar cell performance. Experimental results showed that when deviations in Eg, n, and k were less than 0.2%, 1.4%, and 4.1%, respectively, placing a-SiCx:H and a-SiOx:H films at the p/i and i/n interfaces increased the open-circuit voltage (Voc) and decreased the short-circuit current due to valence band (ΔEv) or conduction band (ΔEc) offsets. The reduction in cell fill factor (FF) and efficiency (η) caused by placing a-SiCx:H and a-SiOx:H films at the p/i interface was greater than that caused by placing them at the i/n interface. Placing the a-SiCx:H film at the p/i interface significantly improved the Voc. Due to the n-type doping effect of oxygen atoms, the a-SiOx:H film exhibited the lowest FF and η at the p/i interface; however, when placed at the i/n interface, it yielded FF and η values second only to the a-Si:H standard reference cell. Appropriately placing the a-SiCx:H film at the p/i interface and the slightly n-type a-SiOx:H film at the i/n interface can effectively improve the Voc, FF, and η of p-i-n solar cells.