Jeferson Freitas
Research Subjects
Jeferson Freitas has a total of 7 co-authors. Here are the top co-authors by number of shared publications:
- Diego Bagnis
CSEM Brasil
1 shared publication - Francisco Anderson de Sousa Lima
CSEM Brasil
1 shared publication - Gerson Santos
Universidade de São Paulo
1 shared publication - Givaldo Reis
Universidade de São Paulo
1 shared publication - Grzegorz Potoczny
CSEM Brasil
1 shared publication - Roberto Zilles
University of São Paulo
1 shared publication
Latest Publications
- Open Access
- 13 December 2016
- Published by Associação Brasileira de Energia Solar in Anais Congresso Brasileiro de Energia Solar - CBENS
- p. 1-6
ESTUDO DO PROCESSO DE DEGRADAÇÃO DE CÉLULAS SOLARES ORGÂNICAS DE HETEROJUNÇÃO INVERTIDAS
This study shows the main results related to the degradation process of Inverted Bulk Heterojunction Organic Solar Cells (OSC) based on poly(3-hexylthiophene-2,5-dyl) regioregular:Phenyl-C60-butyric acid methyl ester (P3HT:PCBM) photoactive blend. The large area modules were fabricated via roll-to-roll (R2R) process in ambient atmosphere and laminated using flexible barrier. The samples were submitted to accelerated degradation through the climatic chamber at 85°C and 85% of relative humidity for a period of 1000 hours followed by electrical characterization in solar simulator system. With obtained results, we noticed a 15% decrease in organic cell efficiency as already reported elsewhere. However, there are not significant changes in the parameters such as open-voltage circuit and shot-current circuit; therefore, to the best of our best knowledge the aged devices exhibit higher stability in comparison with reported data in literature. No presente trabalho são apresentados resultados relativos ao estudo do processo de degradação em células solares orgânicas de heterojunção invertidas, cujas amostras são submetidas a um processo de degradação acelerada utilizando-se câmara climática a 85 graus Célsius e 85% de umidade relativa por um período superior a 1000 horas, seguido de caracterização elétrica realizada em simulador solar. Com os resultados obtidos observa-se que após um período superior a 1000 horas de exposição as amostras apresentam decréscimo relativo na eficiência do módulo de aproximadamente 15%, que por sua vez enquadra-se em valores apontados na literatura, porém com melhoras levando-se em consideração que praticamente não houve redução significativa nos níveis de tensão de circuito aberto e corrente de curto-circuito.
- 13 December 2016
- Published by Associação Brasileira de Energia Solar in Anais Congresso Brasileiro de Energia Solar - CBENS
- p. 1-6
Open AccessESTUDO DO PROCESSO DE DEGRADAÇÃO DE CÉLULAS SOLARES ORGÂNICAS DE HETEROJUNÇÃO INVERTIDAS
This study shows the main results related to the degradation process of Inverted Bulk Heterojunction Organic Solar Cells (OSC) based on poly(3-hexylthiophene-2,5-dyl) regioregular:Phenyl-C60-butyric acid methyl ester (P3HT:PCBM) photoactive blend. The large area modules were fabricated via roll-to-roll (R2R) process in ambient atmosphere and laminated using flexible barrier. The samples were submitted to accelerated degradation through the climatic chamber at 85°C and 85% of relative humidity for a period of 1000 hours followed by electrical characterization in solar simulator system. With obtained results, we noticed a 15% decrease in organic cell efficiency as already reported elsewhere. However, there are not significant changes in the parameters such as open-voltage circuit and shot-current circuit; therefore, to the best of our best knowledge the aged devices exhibit higher stability in comparison with reported data in literature. No presente trabalho são apresentados resultados relativos ao estudo do processo de degradação em células solares orgânicas de heterojunção invertidas, cujas amostras são submetidas a um processo de degradação acelerada utilizando-se câmara climática a 85 graus Célsius e 85% de umidade relativa por um período superior a 1000 horas, seguido de caracterização elétrica realizada em simulador solar. Com os resultados obtidos observa-se que após um período superior a 1000 horas de exposição as amostras apresentam decréscimo relativo na eficiência do módulo de aproximadamente 15%, que por sua vez enquadra-se em valores apontados na literatura, porém com melhoras levando-se em consideração que praticamente não houve redução significativa nos níveis de tensão de circuito aberto e corrente de curto-circuito.