Haiqiang Shi
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Haiqiang Shi has a total of 10 co-authors. Here are the top co-authors by number of shared publications:
- Jian Wu
Center for Rubber Composite Materials and Structures, Harbin Institute of Technology, Weihai 264209, China
2 shared publications - Benlong Su
Center for Rubber Composite Materials and Structures, Harbin Institute of Technology, Weihai 264209, China
1 shared publication - Di Chen
Center for Rubber Composite Materials and Structures, Harbin Institute of Technology, Weihai 264209, China
1 shared publication - Li Qi
State Key Laboratory of Environmental Adaptability for Industrial Products, China National Electric Apparatus Research Institute Co., Ltd., Guangzhou 510663, China
1 shared publication - Pengtao Cao
Center for Rubber Composite Materials and Structures, Harbin Institute of Technology, Weihai 264209, China
1 shared publication - Tianxiao Zhou
Center for Rubber Composite Materials and Structures, Harbin Institute of Technology, Weihai 264209, China
1 shared publication
Latest Publications
- Open Access
Contact Behavior of Phenyl Silicone Rubber Material Under the Condition of High-Altitude Environment
Phenyl silicone rubber is widely used in aircraft seals for its high- and low-temperature tolerance and chemical stability. However, intense UV radiation and elevated ozone at high altitudes accelerate aging, threatening seal reliability. The accelerated aging tests of phenyl silicone rubber seals have been carried out under UV and ozone to examine their mechanical, microstructural, and chemical evolution. Then, a finite element contact model of phenyl silicone rubber seals was developed considering the influence of UV and ozone aging. Both conditions increased hardness and elastic modulus but reduced tensile strength and elongation at break, with UV degradation markedly more severe. UV exposure caused a 29% maximum loss in elongation (compared to 16% under ozone) and a hardness rise of 2.30 HA, roughly 1.7 times that of ozone aging (1.35 HA). The contact pressure increases by approximately 15.2% and 10.7%. These findings provide a theoretical basis for performance evaluation and service-life prediction of these seals in high-altitude environments.
Open AccessContact Behavior of Phenyl Silicone Rubber Material Under the Condition of High-Altitude Environment
Phenyl silicone rubber is widely used in aircraft seals for its high- and low-temperature tolerance and chemical stability. However, intense UV radiation and elevated ozone at high altitudes accelerate aging, threatening seal reliability. The accelerated aging tests of phenyl silicone rubber seals have been carried out under UV and ozone to examine their mechanical, microstructural, and chemical evolution. Then, a finite element contact model of phenyl silicone rubber seals was developed considering the influence of UV and ozone aging. Both conditions increased hardness and elastic modulus but reduced tensile strength and elongation at break, with UV degradation markedly more severe. UV exposure caused a 29% maximum loss in elongation (compared to 16% under ozone) and a hardness rise of 2.30 HA, roughly 1.7 times that of ozone aging (1.35 HA). The contact pressure increases by approximately 15.2% and 10.7%. These findings provide a theoretical basis for performance evaluation and service-life prediction of these seals in high-altitude environments.
- Open Access
Sealing Performance of Phenyl-Silicone Rubber Based on Constitutive Model Under Thermo-Oxidative Aging
Phenyl-silicone rubber is the elastomer of choice for cryogenic and high-temperature static seals, yet quantitative links between thermo-oxidative aging and sealing reliability are still lacking. Here, sub-ambient (−70 °C to 25 °C) and room-temperature mechanical tests, compression set aging, SEM, FT-IR, and finite-element simulations are integrated to trace how aging translates into contact-pressure decay of an Omega-profile gasket. Compression set rises monotonically with time and temperature; an Arrhenius model derived from 80 to 140 °C data predicts 34 d (10% set) and 286 d (45% set) of storage life at 25 °C. SEM reveals a progressive shift from ductile dimple fracture to brittle, honeycomb porosity, while FT-IR confirms limited surface oxidation without bulk chain scission. Finite element analyses show that contact pressure always peaks at the two lateral necks; short-term aging increases in the shear modulus C10 from 1.87 to 2.27 MPa, raising CPRESS by 8~21%, yet this benefit is ultimately offset by displacement loss from compression set (8.0 mm to 6.1 mm), yielding a net pressure reduction of 0.006 MPa. Critically, even under the most severe coupled condition (56 days aging with compression set), the predicted CPRESS remains above the 0.1 MPa leak-tightness criterion across the entire cryogenic service envelope. This framework provides deterministic boundaries for temperature, aging duration, and allowable preload relaxation, enabling risk-informed maintenance and replacement scheduling for safety-critical phenyl-silicone seals.
Open AccessSealing Performance of Phenyl-Silicone Rubber Based on Constitutive Model Under Thermo-Oxidative Aging
Phenyl-silicone rubber is the elastomer of choice for cryogenic and high-temperature static seals, yet quantitative links between thermo-oxidative aging and sealing reliability are still lacking. Here, sub-ambient (−70 °C to 25 °C) and room-temperature mechanical tests, compression set aging, SEM, FT-IR, and finite-element simulations are integrated to trace how aging translates into contact-pressure decay of an Omega-profile gasket. Compression set rises monotonically with time and temperature; an Arrhenius model derived from 80 to 140 °C data predicts 34 d (10% set) and 286 d (45% set) of storage life at 25 °C. SEM reveals a progressive shift from ductile dimple fracture to brittle, honeycomb porosity, while FT-IR confirms limited surface oxidation without bulk chain scission. Finite element analyses show that contact pressure always peaks at the two lateral necks; short-term aging increases in the shear modulus C10 from 1.87 to 2.27 MPa, raising CPRESS by 8~21%, yet this benefit is ultimately offset by displacement loss from compression set (8.0 mm to 6.1 mm), yielding a net pressure reduction of 0.006 MPa. Critically, even under the most severe coupled condition (56 days aging with compression set), the predicted CPRESS remains above the 0.1 MPa leak-tightness criterion across the entire cryogenic service envelope. This framework provides deterministic boundaries for temperature, aging duration, and allowable preload relaxation, enabling risk-informed maintenance and replacement scheduling for safety-critical phenyl-silicone seals.