Huihua Zhang
Huihua Zhang has a total of 22 co-authors. Here are the top co-authors by number of shared publications:
- Guonan Ma
Ningbo Branch of Chinese Academy of Ordnance Science, Ningbo 315103, China
3 shared publications - Pengwei Yang
Ningbo Branch of Chinese Academy of Ordnance Science, Ningbo 315103, China
3 shared publications - Shuming Zhao
Ningbo Branch of Chinese Academy of Ordnance Science, Ningbo 315103, China
3 shared publications - Yangping Dong
Ningbo Branch of Chinese Academy of Ordnance Science, Ningbo 315103, China
3 shared publications - Jinyu Zhu
Ningbo Branch of Chinese Academy of Ordnance Science, Ningbo 315103, China
2 shared publications - Liang Zhong
Ningbo Branch of Chinese Academy of Ordnance Science, Ningbo 315103, China
2 shared publications
Latest Publications
- Open Access
Grain Morphology Evolution of TiAl Alloy During Electron Beam Powder Bed Fusion
Electron beam powder bed fusion (PBF-EB) of TiAl alloys exhibits different grain morphologies: equiaxed grains and columnar grains. However, the rule for controlling grain morphologies has not been found. In addition, the grain morphology is closely related to thermal gradient and growth velocity during PBF-EB. Here, thermal gradient and growth velocity are controlled by preheating temperature, beam current, and scanning speed. Based on the numerical simulation, the relationship between solidification parameters (thermal gradient and growth velocity) and process parameters (preheating temperature, beam current, and scanning speed) has been revealed. Meanwhile, the grain morphology of the topmost region of the PBF-EB-built Ti-48Al-2Cr-2Nb alloy can be controlled. In addition, the columnar-to-equiaxed transition is found in the PBF-EB-built Ti-48Al-2Cr-2Nb alloy. This is attributed to the PBF-EB technology belonging to the layer-by-layer stacking process, and the stacked layer reduces the thermal gradient and increases growth velocity in the remelting region. These findings will contribute to understanding the grain morphology evolution of TiAl alloys during PBF-EB, providing the principle for controlling the grain morphology of PBF-EB-built TiAl alloys.
Open AccessGrain Morphology Evolution of TiAl Alloy During Electron Beam Powder Bed Fusion
Electron beam powder bed fusion (PBF-EB) of TiAl alloys exhibits different grain morphologies: equiaxed grains and columnar grains. However, the rule for controlling grain morphologies has not been found. In addition, the grain morphology is closely related to thermal gradient and growth velocity during PBF-EB. Here, thermal gradient and growth velocity are controlled by preheating temperature, beam current, and scanning speed. Based on the numerical simulation, the relationship between solidification parameters (thermal gradient and growth velocity) and process parameters (preheating temperature, beam current, and scanning speed) has been revealed. Meanwhile, the grain morphology of the topmost region of the PBF-EB-built Ti-48Al-2Cr-2Nb alloy can be controlled. In addition, the columnar-to-equiaxed transition is found in the PBF-EB-built Ti-48Al-2Cr-2Nb alloy. This is attributed to the PBF-EB technology belonging to the layer-by-layer stacking process, and the stacked layer reduces the thermal gradient and increases growth velocity in the remelting region. These findings will contribute to understanding the grain morphology evolution of TiAl alloys during PBF-EB, providing the principle for controlling the grain morphology of PBF-EB-built TiAl alloys.
- Open Access
Microstructural and Mechanical Properties of Y2O3 Modified Ti6Al4V Alloy Fabricated by Laser Powder Bed Fusion
A Ti6Al4V alloy fabrication via laser powder bed fusion (L-PBF) leads to the formation of coarse columnar β grains that give rise to anisotropic mechanical properties and inadequate strength. Incorporating the rare-earth oxide, yttrium oxide (Y2O3), has proven an effective strategy in enhancing the mechanical performance of Ti6Al4V alloys. Nevertheless, the critical Y2O3 content required to achieve an optimal strength–ductility balance in L-PBF Ti6Al4V has not been systematically determined. To address these critical gaps, this study, for the first time, systematically investigates the effect of various Y2O3 contents on the microstructural evolution and mechanical properties of Ti6Al4V alloys fabricated via L-PBF. The results demonstrate that a Y2O3 addition of 0.2 wt.% produces β grains and α phases with average sizes of 61.6 and 7.6 μm, respectively. Transmission electron microscopy observations reveal that Y2O3 nanoparticles, together with elemental Y nanoparticles formed by reduction, are distributed both within the α-Ti matrix and along phase boundaries. This distribution effectively reinforces grain boundaries and promotes heterogeneous nucleation, thereby refining the microstructure. Mechanical property tests indicate that the alloy strength significantly improves as the Y2O3 content increases. Specifically, the alloy with 0.2 wt.%Y2O3 exhibits a tensile strength of 1106 MPa, a yield strength of 1074 MPa, and an elongation of 10.7%. This study proposes an innovative rare-earth strengthening method for refining the microstructure of L-PBF-fabricated titanium alloys and comprehensively enhancing their mechanical properties.
Open AccessMicrostructural and Mechanical Properties of Y2O3 Modified Ti6Al4V Alloy Fabricated by Laser Powder Bed Fusion
A Ti6Al4V alloy fabrication via laser powder bed fusion (L-PBF) leads to the formation of coarse columnar β grains that give rise to anisotropic mechanical properties and inadequate strength. Incorporating the rare-earth oxide, yttrium oxide (Y2O3), has proven an effective strategy in enhancing the mechanical performance of Ti6Al4V alloys. Nevertheless, the critical Y2O3 content required to achieve an optimal strength–ductility balance in L-PBF Ti6Al4V has not been systematically determined. To address these critical gaps, this study, for the first time, systematically investigates the effect of various Y2O3 contents on the microstructural evolution and mechanical properties of Ti6Al4V alloys fabricated via L-PBF. The results demonstrate that a Y2O3 addition of 0.2 wt.% produces β grains and α phases with average sizes of 61.6 and 7.6 μm, respectively. Transmission electron microscopy observations reveal that Y2O3 nanoparticles, together with elemental Y nanoparticles formed by reduction, are distributed both within the α-Ti matrix and along phase boundaries. This distribution effectively reinforces grain boundaries and promotes heterogeneous nucleation, thereby refining the microstructure. Mechanical property tests indicate that the alloy strength significantly improves as the Y2O3 content increases. Specifically, the alloy with 0.2 wt.%Y2O3 exhibits a tensile strength of 1106 MPa, a yield strength of 1074 MPa, and an elongation of 10.7%. This study proposes an innovative rare-earth strengthening method for refining the microstructure of L-PBF-fabricated titanium alloys and comprehensively enhancing their mechanical properties.
- Open Access
- 30 January 2026
- Published by MDPI AG in Preprints.org
Microstructural and Mechanical Properties of Y₂O₃ Modified Ti6Al4V Alloy Fabricated by Laser Powder Bed Fusion
A Ti6Al4V alloy fabrication via laser powder bed fusion (L-PBF) leads to the formation of coarse columnar β grains that give rise to anisotropic mechanical properties and inadequate strength. Incorporating the rare earth oxide, yttrium oxide (Y₂O₃), has proven an effective strategy in enhancing the mechanical performance of Ti6Al4V al-loys. This study systematically investigates the effects of various Y₂O₃ contents on the microstructure and mechanical properties of Ti6Al4V alloys fabricated via L-PBF. The results demonstrate that a Y₂O₃ addition of 0.2 wt.% produces β grains and α phases with average sizes of 61.6 and 7.6 μm, respectively. Transmission electron microscopy observations reveal that Y₂O₃ nanoparticles, together with elemental Y nanoparticles formed by reduction, are distributed both within the α-Ti matrix and along phase boundaries. This distribution effectively reinforces grain boundaries and promotes heterogeneous nucleation, thereby refining the microstructure. Mechanical property tests indicate that the alloy strength significantly improves as the Y₂O₃ content in-creases. Specifically, the alloy with 0.2 wt.%Y₂O₃ exhibits a tensile strength of 1106 MPa, a yield strength of 1074 MPa, and an elongation of 10.0%. This study proposes an in-novative rare earth strengthening method for refining the microstructure of L-PBF-fabricated titanium alloys and comprehensively enhancing their mechanical properties.
- 30 January 2026
- Published by MDPI AG in Preprints.org
Open AccessMicrostructural and Mechanical Properties of Y₂O₃ Modified Ti6Al4V Alloy Fabricated by Laser Powder Bed Fusion
A Ti6Al4V alloy fabrication via laser powder bed fusion (L-PBF) leads to the formation of coarse columnar β grains that give rise to anisotropic mechanical properties and inadequate strength. Incorporating the rare earth oxide, yttrium oxide (Y₂O₃), has proven an effective strategy in enhancing the mechanical performance of Ti6Al4V al-loys. This study systematically investigates the effects of various Y₂O₃ contents on the microstructure and mechanical properties of Ti6Al4V alloys fabricated via L-PBF. The results demonstrate that a Y₂O₃ addition of 0.2 wt.% produces β grains and α phases with average sizes of 61.6 and 7.6 μm, respectively. Transmission electron microscopy observations reveal that Y₂O₃ nanoparticles, together with elemental Y nanoparticles formed by reduction, are distributed both within the α-Ti matrix and along phase boundaries. This distribution effectively reinforces grain boundaries and promotes heterogeneous nucleation, thereby refining the microstructure. Mechanical property tests indicate that the alloy strength significantly improves as the Y₂O₃ content in-creases. Specifically, the alloy with 0.2 wt.%Y₂O₃ exhibits a tensile strength of 1106 MPa, a yield strength of 1074 MPa, and an elongation of 10.0%. This study proposes an in-novative rare earth strengthening method for refining the microstructure of L-PBF-fabricated titanium alloys and comprehensively enhancing their mechanical properties.