Shaoqing Wang
Research Subjects
Shaoqing Wang has a total of 17 co-authors. Here are the top co-authors by number of shared publications:
Rihong Han
3 shared publicationsQingxuan Ran
2 shared publications- Qingxuan Ran2 shared publications
Shan Liu
2 shared publicationsShuaiwei Chen
2 shared publicationsXiaojun Jiang
2 shared publications
Latest Publications
- Open Access
- 10 March 2026
- Published by Elsevier in SSRN Electronic Journal
亚稳态经济型TRIP辅助19Cr双面不锈钢的异质晶粒微观结构形成及诱导非均匀变形开裂行为
Deformation-induced martensite phase (α') undergoes reverse transformation recrystallization to austenite phase (γ) of α'→γ in the cold-rolled TRIP-aided 19Cr economical duplex stainless steel (EDSS) plate during tempering recrystallization process at 950 °C, which takes precedence over the recrystallization of dislocation-type ferrite (α) and retained dislocation dominated austenite (γ). The difference in sequential order of recrystallization among multiple phases (induced α' phase, dislocation dominated α and retained γ phase to recrystallized α and γ phase) and grain growth rates of recrystallized α and γ phase result in the heterogeneous grains size distribution characteristic in the material during tempering recrystallization process. Recrystallized ferrite undergoes plastic deformation preferentially over the recrystallized austenitein the recrystallized 19Cr EDSS during tensile deformation at room temperature. Nevertheless, the equivalent strain of the recrystallized austenite is larger than that of the ferrite phase during tensile deformation process. Initial cracks preferentially form in the austenite phase and then propagate to phase interface as strain incompatibility effect of recrystallized α/γ phase leading to the final cracking.
- 10 March 2026
- Published by Elsevier in SSRN Electronic Journal
Open Access亚稳态经济型TRIP辅助19Cr双面不锈钢的异质晶粒微观结构形成及诱导非均匀变形开裂行为
Deformation-induced martensite phase (α') undergoes reverse transformation recrystallization to austenite phase (γ) of α'→γ in the cold-rolled TRIP-aided 19Cr economical duplex stainless steel (EDSS) plate during tempering recrystallization process at 950 °C, which takes precedence over the recrystallization of dislocation-type ferrite (α) and retained dislocation dominated austenite (γ). The difference in sequential order of recrystallization among multiple phases (induced α' phase, dislocation dominated α and retained γ phase to recrystallized α and γ phase) and grain growth rates of recrystallized α and γ phase result in the heterogeneous grains size distribution characteristic in the material during tempering recrystallization process. Recrystallized ferrite undergoes plastic deformation preferentially over the recrystallized austenitein the recrystallized 19Cr EDSS during tensile deformation at room temperature. Nevertheless, the equivalent strain of the recrystallized austenite is larger than that of the ferrite phase during tensile deformation process. Initial cracks preferentially form in the austenite phase and then propagate to phase interface as strain incompatibility effect of recrystallized α/γ phase leading to the final cracking.
- Open Access
- 10 February 2026
- Published by Elsevier in SSRN Electronic Journal
A Study on the Microstructure and Corrosion Properties of Laser-Clad FeCoCrNiMo x High-Entropy Alloy Coatings
High-entropy alloys (HEAs) exhibit broad application prospects in the field of surface engineering due to their excellent mechanical properties and corrosion resistance. In this study, FeCoCrNiMox (x = 0.0, 0.2, 0.4, 0.6, 0.8) HEA coatings were prepared on 45# steel substrates using laser cladding technology. The effects of Mo content on the phase composition, microstructure, microhardness, and corrosion resistance of the coatings were systematically investigated. The results indicate that when the Mo content x ≤ 0.4, the coatings exhibit a single face-centered cubic (FCC) structure with an equiaxed grain morphology. When x ≥ 0.6, σ phase precipitates in the coatings, resulting in a dendritic structure. Microhardness tests show that as the Mo content increases, the hardness of the coatings significantly improves from 220 HV (x = 0.0) to 400 HV (x = 0.8), primarily attributed to solid solution strengthening induced by Mo and second-phase strengthening due to σ phase precipitation. Electrochemical test results demonstrate that the FeCoCrNiMo0.6 coating exhibits the optimal corrosion resistance in both 0.5 mol/L H2SO4 and 3.5 wt.% NaCl environments. Specifically, in the acidic environment, it achieves the lowest corrosion current density (0.79 μA/cm2), which is attributed to the formation of a stable and dense passive film promoted by Mo, significantly enhancing the protective capability of the coating. When the Mo content increases to x = 0.8, the corrosion resistance declines in both environments, though through different mechanisms: in the H2SO4 environment, the precipitation of the σ phase compromises the stability of the passive film; whereas in the NaCl environment, the deterioration is primarily caused by Cl−-induced galvanic corrosion between the σ phase and the matrix.
- 10 February 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessA Study on the Microstructure and Corrosion Properties of Laser-Clad FeCoCrNiMo x High-Entropy Alloy Coatings
High-entropy alloys (HEAs) exhibit broad application prospects in the field of surface engineering due to their excellent mechanical properties and corrosion resistance. In this study, FeCoCrNiMox (x = 0.0, 0.2, 0.4, 0.6, 0.8) HEA coatings were prepared on 45# steel substrates using laser cladding technology. The effects of Mo content on the phase composition, microstructure, microhardness, and corrosion resistance of the coatings were systematically investigated. The results indicate that when the Mo content x ≤ 0.4, the coatings exhibit a single face-centered cubic (FCC) structure with an equiaxed grain morphology. When x ≥ 0.6, σ phase precipitates in the coatings, resulting in a dendritic structure. Microhardness tests show that as the Mo content increases, the hardness of the coatings significantly improves from 220 HV (x = 0.0) to 400 HV (x = 0.8), primarily attributed to solid solution strengthening induced by Mo and second-phase strengthening due to σ phase precipitation. Electrochemical test results demonstrate that the FeCoCrNiMo0.6 coating exhibits the optimal corrosion resistance in both 0.5 mol/L H2SO4 and 3.5 wt.% NaCl environments. Specifically, in the acidic environment, it achieves the lowest corrosion current density (0.79 μA/cm2), which is attributed to the formation of a stable and dense passive film promoted by Mo, significantly enhancing the protective capability of the coating. When the Mo content increases to x = 0.8, the corrosion resistance declines in both environments, though through different mechanisms: in the H2SO4 environment, the precipitation of the σ phase compromises the stability of the passive film; whereas in the NaCl environment, the deterioration is primarily caused by Cl−-induced galvanic corrosion between the σ phase and the matrix.