Cun Liang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Cun Liang has a total of 10 co-authors. Here are the top co-authors by number of shared publications:
- Chengjun Zhu
1 Henan Flexible Manufacturing Engineering Research Center, Henan Polytechnic Institute, Nanyang, China
2 shared publications - Dachuan Zhu
College of Material Science and Engineering, Sichuan University, Chengdu 610065, China
2 shared publications - Deliang Zhang
School of Materials Science and Engineering, Northeastern University, Shenyang 110819, China
2 shared publications - Liang Zhao
School of Materials Electronics and Energy Storage, Zhongyuan University of Technology, Zhengzhou 451191, China
2 shared publications - Mingxing Ma
1 Henan Flexible Manufacturing Engineering Research Center, Henan Polytechnic Institute, Nanyang, China
2 shared publications - Ying Dong
School of Mechanical Engineering, Henan Polytechnic Institute, Nanyang 473000, China
2 shared publications
Latest Publications
- Open Access
Effect of cBN Addition on Phase Composition, Microstructure, Wear Resistance, and Corrosion Resistance of CoCuNiTi + x cBN (x = 0.0, 0.5, and 1.0 wt.%) High-Entropy Alloy Coatings
Although 45 steel is widely used in the manufacture of mechanical parts, its application in harsh working conditions is limited owing to its low hardness, poor wear resistance, and corrosion resistance. Laser cladding can enhance the performance of the working surface without sacrificing substrate toughness. CoCuNiTi HEACs with different cBN additions were successfully prepared on a 45-steel substrate. The phase structure, microstructure, elemental composition, wear, and corrosion behavior of CoCuNiTi + x cBN (x = 0.0, 0.5, and 1.0 wt.%) HEACs were investigated using XRD, OM, SEM, EDS, friction and wear tester, and electrochemical workstation, respectively. The results show that all three coatings exhibit a dual-phase structure composed of FCC and BCC phases. The addition of cBN transforms the alloy phase structure from the original FCC main phase to the BCC main phase. The incorporation of cBN significantly reduces the lattice constant and cell volume of the alloy phase. The change in the alloy phase density is negatively correlated with the cell volume. CoCuNiTi + x cBN (x = 0.0, 0.5, and 1.0 wt.%) alloys have a dendritic structure. No pores were observed in the cBN-containing sample. The content of Ti in the primary phase is the highest. Co is enriched in the dendrite region, and Cu is enriched in the interdendrite region. The significant reduction in the average segregation coefficient for cBN-containing samples is attributed to the heterogeneous nucleation of the alloy melt at lower undercooling levels and the significant increase in the diffusion rate. The friction coefficient of the alloy decreases significantly with increasing cBN content. The sample with 1.0 wt.% cBN shows the best wear resistance, mainly due to the combined effects of hard particle support, solid solution strengthening, phase interface reduction, and high thermal conductivity of cBN. The sample with 1.0 wt.% cBN has the largest capacitive arc radius and charge-transfer resistance, along with the lowest annual corrosion rate, indicating optimal corrosion resistance. This is primarily related to the reduction in pore defects caused by cBN addition, hindrance of uniform penetration of the corrosive medium by dispersed cBN particles, and increased complexity of the anodic dissolution process. CoCuNiTi HEACs reinforced by cBN can simultaneously improve the wear and corrosion resistance of the surface of the 45-steel substrate, providing a feasible strategy for the design of high-performance protective coatings.
Open AccessEffect of cBN Addition on Phase Composition, Microstructure, Wear Resistance, and Corrosion Resistance of CoCuNiTi + x cBN (x = 0.0, 0.5, and 1.0 wt.%) High-Entropy Alloy Coatings
Although 45 steel is widely used in the manufacture of mechanical parts, its application in harsh working conditions is limited owing to its low hardness, poor wear resistance, and corrosion resistance. Laser cladding can enhance the performance of the working surface without sacrificing substrate toughness. CoCuNiTi HEACs with different cBN additions were successfully prepared on a 45-steel substrate. The phase structure, microstructure, elemental composition, wear, and corrosion behavior of CoCuNiTi + x cBN (x = 0.0, 0.5, and 1.0 wt.%) HEACs were investigated using XRD, OM, SEM, EDS, friction and wear tester, and electrochemical workstation, respectively. The results show that all three coatings exhibit a dual-phase structure composed of FCC and BCC phases. The addition of cBN transforms the alloy phase structure from the original FCC main phase to the BCC main phase. The incorporation of cBN significantly reduces the lattice constant and cell volume of the alloy phase. The change in the alloy phase density is negatively correlated with the cell volume. CoCuNiTi + x cBN (x = 0.0, 0.5, and 1.0 wt.%) alloys have a dendritic structure. No pores were observed in the cBN-containing sample. The content of Ti in the primary phase is the highest. Co is enriched in the dendrite region, and Cu is enriched in the interdendrite region. The significant reduction in the average segregation coefficient for cBN-containing samples is attributed to the heterogeneous nucleation of the alloy melt at lower undercooling levels and the significant increase in the diffusion rate. The friction coefficient of the alloy decreases significantly with increasing cBN content. The sample with 1.0 wt.% cBN shows the best wear resistance, mainly due to the combined effects of hard particle support, solid solution strengthening, phase interface reduction, and high thermal conductivity of cBN. The sample with 1.0 wt.% cBN has the largest capacitive arc radius and charge-transfer resistance, along with the lowest annual corrosion rate, indicating optimal corrosion resistance. This is primarily related to the reduction in pore defects caused by cBN addition, hindrance of uniform penetration of the corrosive medium by dispersed cBN particles, and increased complexity of the anodic dissolution process. CoCuNiTi HEACs reinforced by cBN can simultaneously improve the wear and corrosion resistance of the surface of the 45-steel substrate, providing a feasible strategy for the design of high-performance protective coatings.
- Open Access
Effect of Diamond Content on Microstructure and Wear/Corrosion Resistance of CoCuNiTi + x Diamond (C) (x = 0, 0.5, and 1.0 wt.%) High-Entropy Alloy Coatings
CoCuNiTi HEACs reinforced by different diamond contents were prepared on the surface of 45 steel substrate by laser cladding. Their phase composition, microstructure, elemental composition, and wear/corrosion resistance were investigated using XRD, OM, SEM, EDS, a friction and wear testing machine, and an electrochemical workstation, respectively. The results show that after adding diamond, the phase composition of the sample transforms from the original dual-phase structure of the FCC main phase and BCC to the dual-phase structure of the BCC main phase and FCC. With an increase in the diamond content, the diffraction peak intensity of the alloy phases first increases and then decreases. This behavior is related to the significant enhancement of the alloy phase crystallinity with low diamond addition and the intensified crystal lattice distortion caused by excessive diamond addition. The CoCuNiTi + x Diamond (C) (x = 0, 0.5, and 1.0 wt.%) high-entropy alloys have a dendritic structure. After the addition of diamond, no hole defects were observed in the microstructure, and the dendritic structure was significantly refined. Ti and C are enriched in the primary phase, Cu is enriched in the interdendrite regions, and Co exhibits the highest concentration in the dendrite regions. The segregation coefficients of Ni in all three alloys are relatively small. As the diamond content increases, the friction coefficient of the samples decreases significantly. The 1 wt.% diamond sample exhibits the best wear resistance, primarily owing to the combined effects of superhard phase strengthening, solid solution strengthening, and fine grain strengthening resulting from diamond addition. The sample with 0.5 wt.% diamond addition has the lowest self-corrosion current density, highest polarization resistance, and lowest annual corrosion rate, indicating the best corrosion resistance. This performance is mainly attributed to the refinement of the microstructure, reduction in defects, and formation of a dense passivation film caused by the addition of a small amount of diamond.
Open AccessEffect of Diamond Content on Microstructure and Wear/Corrosion Resistance of CoCuNiTi + x Diamond (C) (x = 0, 0.5, and 1.0 wt.%) High-Entropy Alloy Coatings
CoCuNiTi HEACs reinforced by different diamond contents were prepared on the surface of 45 steel substrate by laser cladding. Their phase composition, microstructure, elemental composition, and wear/corrosion resistance were investigated using XRD, OM, SEM, EDS, a friction and wear testing machine, and an electrochemical workstation, respectively. The results show that after adding diamond, the phase composition of the sample transforms from the original dual-phase structure of the FCC main phase and BCC to the dual-phase structure of the BCC main phase and FCC. With an increase in the diamond content, the diffraction peak intensity of the alloy phases first increases and then decreases. This behavior is related to the significant enhancement of the alloy phase crystallinity with low diamond addition and the intensified crystal lattice distortion caused by excessive diamond addition. The CoCuNiTi + x Diamond (C) (x = 0, 0.5, and 1.0 wt.%) high-entropy alloys have a dendritic structure. After the addition of diamond, no hole defects were observed in the microstructure, and the dendritic structure was significantly refined. Ti and C are enriched in the primary phase, Cu is enriched in the interdendrite regions, and Co exhibits the highest concentration in the dendrite regions. The segregation coefficients of Ni in all three alloys are relatively small. As the diamond content increases, the friction coefficient of the samples decreases significantly. The 1 wt.% diamond sample exhibits the best wear resistance, primarily owing to the combined effects of superhard phase strengthening, solid solution strengthening, and fine grain strengthening resulting from diamond addition. The sample with 0.5 wt.% diamond addition has the lowest self-corrosion current density, highest polarization resistance, and lowest annual corrosion rate, indicating the best corrosion resistance. This performance is mainly attributed to the refinement of the microstructure, reduction in defects, and formation of a dense passivation film caused by the addition of a small amount of diamond.