Warneri Warneri
Research Subjects
Warneri Warneri has a total of 9 co-authors. Here are the top co-authors by number of shared publications:
- Agus Paul Setiawan Kaban
Universitas Indonesia
2 shared publications - Johny Wahyuadi Soedarsono
University of Indonesia
2 shared publications - Sidhi Aribowo
Universitas Indonesia
2 shared publications - Sopar Mangarapot Simanullang
Pertamina Drilling Services Indonesia
2 shared publications - Ario Oktora
Pertamina Drilling Services Indonesia
1 shared publication - Raajwa Ayudhia Kamila
Universitas Indonesia
1 shared publication
Latest Publications
- Open Access
- 30 June 2026
- Published by Private Company Technology Center in Eastern-European Journal of Enterprise Technologies
- Vol. 3 (1 (141)) , 53-63
The identification of hydrogen embrittlement and the role of intergranular brittle fracture of API 5DP G105 drill pipe failure on onshore drilling activity
The object of this study is high-strength steel of API 5DP Gr 105 that has been used during well completion in a corrosive environment. This work emphasizes key factors affecting material damage caused by slip marks, tensile load, and hydrogen content in contaminated brine and completion fluid, which were not addressed in previous studies. Several tests, including chemical, mechanical, and surface characterization, were conducted. The chemical composition test of the fluid shows that the brine has been contaminated by H2S gas and sulfur, with inevitable traces of chloride, bicarbonate, carbonate, bisulfide, and sulfide, providing active sites for hydrogen atom diffusion at the slip marks. The material composition test confirms that the failed material is API 5DP Gr 105. A noticeable amount of phosphorus increases grain boundary segregation and weakens the cohesive metallic bond. A hardness at 28 Rockwell C is inevitable and increases the material’s vulnerability to embrittlement, despite the Charpy energy test showing a manageable level, confirming local brittleness. The high tensile strength of 914 MPa is evidence of embrittlement, even though the material remains ductile, with a noticeable elongation of 20%. An intergranular crack was observed in the microstructure, and slip marks serve as stress concentrators for the crack. Thus, it can be concluded that the combination of tensile load, hydrogen gas content, local slip marks, and completion fluid in the well weakened the grain boundaries and served as an initial crack with a high hydrogen-atom concentration. This work models the root-cause analysis of high-strength steel during well-completion operations in an onshore facility
- 30 June 2026
- Published by Private Company Technology Center in Eastern-European Journal of Enterprise Technologies
- Vol. 3 (1 (141)) , 53-63
Open AccessThe identification of hydrogen embrittlement and the role of intergranular brittle fracture of API 5DP G105 drill pipe failure on onshore drilling activity
The object of this study is high-strength steel of API 5DP Gr 105 that has been used during well completion in a corrosive environment. This work emphasizes key factors affecting material damage caused by slip marks, tensile load, and hydrogen content in contaminated brine and completion fluid, which were not addressed in previous studies. Several tests, including chemical, mechanical, and surface characterization, were conducted. The chemical composition test of the fluid shows that the brine has been contaminated by H2S gas and sulfur, with inevitable traces of chloride, bicarbonate, carbonate, bisulfide, and sulfide, providing active sites for hydrogen atom diffusion at the slip marks. The material composition test confirms that the failed material is API 5DP Gr 105. A noticeable amount of phosphorus increases grain boundary segregation and weakens the cohesive metallic bond. A hardness at 28 Rockwell C is inevitable and increases the material’s vulnerability to embrittlement, despite the Charpy energy test showing a manageable level, confirming local brittleness. The high tensile strength of 914 MPa is evidence of embrittlement, even though the material remains ductile, with a noticeable elongation of 20%. An intergranular crack was observed in the microstructure, and slip marks serve as stress concentrators for the crack. Thus, it can be concluded that the combination of tensile load, hydrogen gas content, local slip marks, and completion fluid in the well weakened the grain boundaries and served as an initial crack with a high hydrogen-atom concentration. This work models the root-cause analysis of high-strength steel during well-completion operations in an onshore facility
- Open Access
- 27 February 2026
- Published by Private Company Technology Center in Eastern-European Journal of Enterprise Technologies
- Vol. 1 (1 (139)) , 59-69
Unveiling the root cause failure 3-1/2" parted drill in onshore environment
The object of this study is HSS API 5DP Gr 105 which has been used as drill pipe and was found leak during drilling activity, causing a delay in the delivery of drilling products. The interaction among the high partial pressure of H2S, a high-hardness material, and the injection of high-density completion fluid (HDCF) remains poorly understood, leading to sulfide stress cracking. Despite offering substantial benefits, the detected trace amounts of hydrogen and sulfur indicate a localized corrosion, which can lead to unprecedented drilling shutdowns and consequently impose greater operational costs. Recently, the API 5DP 3-1/2’’ drill pipe experienced failure with a significant hardness value of 26 HRC, exceeding the standard specified by NACE MR 0175. The material was in service in rich H2S gas well, where HDCF was injected to maintain hydrostatic pressure and serve as a control fluid. Multiple field and laboratory investigations have been undertaken to identify the root cause of this failure, including visual inspections, macrophotography, chemical composition analysis, completion fluid testing, tensile testing, metallography, and SEM-EDX analysis. The shear-slip and step-like markings on the failed material clearly indicate a brittle nature, correlating with a noticeable tensile strength of 907.80 MPa and an elongation limit of 18.18%. The increase in hardness beyond 22 HRC indicates susceptibility to sulfide stress cracking (SSC) where the hydrogen permeation increases with the increasing H2S partial pressure. These facts align with water chemistry analysis results to show S2– and HS–levels exceeding one ppm. Additionally, metallography reveals intergranular cracking in the tempered martensite, likely initiated at a local stress concentrator before propagating and confirmed by scanning electron microscope (SEM) images
- 27 February 2026
- Published by Private Company Technology Center in Eastern-European Journal of Enterprise Technologies
- Vol. 1 (1 (139)) , 59-69
Open AccessUnveiling the root cause failure 3-1/2" parted drill in onshore environment
The object of this study is HSS API 5DP Gr 105 which has been used as drill pipe and was found leak during drilling activity, causing a delay in the delivery of drilling products. The interaction among the high partial pressure of H2S, a high-hardness material, and the injection of high-density completion fluid (HDCF) remains poorly understood, leading to sulfide stress cracking. Despite offering substantial benefits, the detected trace amounts of hydrogen and sulfur indicate a localized corrosion, which can lead to unprecedented drilling shutdowns and consequently impose greater operational costs. Recently, the API 5DP 3-1/2’’ drill pipe experienced failure with a significant hardness value of 26 HRC, exceeding the standard specified by NACE MR 0175. The material was in service in rich H2S gas well, where HDCF was injected to maintain hydrostatic pressure and serve as a control fluid. Multiple field and laboratory investigations have been undertaken to identify the root cause of this failure, including visual inspections, macrophotography, chemical composition analysis, completion fluid testing, tensile testing, metallography, and SEM-EDX analysis. The shear-slip and step-like markings on the failed material clearly indicate a brittle nature, correlating with a noticeable tensile strength of 907.80 MPa and an elongation limit of 18.18%. The increase in hardness beyond 22 HRC indicates susceptibility to sulfide stress cracking (SSC) where the hydrogen permeation increases with the increasing H2S partial pressure. These facts align with water chemistry analysis results to show S2– and HS–levels exceeding one ppm. Additionally, metallography reveals intergranular cracking in the tempered martensite, likely initiated at a local stress concentrator before propagating and confirmed by scanning electron microscope (SEM) images