Maxim Vadimovich Matanov
Research Subjects
Maxim Vadimovich Matanov has a total of 10 co-authors. Here are the top co-authors by number of shared publications:
- Alexander Pavlovich Demirov
Department of Functional Nanosystems and High-Temperature Materials, University of Science and Technology MISIS, Leninskiy Prospekt 4, 119049 Moscow, Russia
2 shared publications - Dmitry Sergeevich Belov
Department of Functional Nanosystems and High-Temperature Materials, University of Science and Technology MISIS, Leninskiy Prospekt 4, 119049 Moscow, Russia
2 shared publications - Igor Victorovich Blinkov
National University of Science and Technology MISiS
2 shared publications - Roman Antonovich Bykov
National University of Science and Technology MISiS
1 shared publication - Sergei Eremin
A.A. Baikov Institute of Metallurgy and Materials Science, Russian Academy of Science, Moscow, Russia
1 shared publication А. П. Демиров
Университет науки и технологий МИСИС
1 shared publication
Latest Publications
- Open Access
- 14 October 2026
- Published by National University of Science and Technology MISiS in Powder Metallurgy аnd Functional Coatings
Effect of Cr and CrN interlayers on the structure and mechanical properties of multilayer Ti–Al–Mo–N coatings
This study investigated the effects of metallic chromium (Cr) and chromium nitride (CrN) underlayers on the structure and mechanical properties of TiN/Mo₂N multilayer coatings deposited on 13KhFA steel. The coatings were produced by vacuum arc deposition, alternating coating growth with heating by ion bombardment. The coatings were approximately 750 nm thick, and the Cr and CrN underlayers were 300 and 700 nm thick, respectively. Silicon from the steel substrate was detected in the coating deposited on the Cr underlayer, which also exhibited more pronounced intermixing between sublayers. In contrast, no silicon was detected in the coating deposited on the CrN underlayer using the analytical method employed. This coating exhibited sharper compositional transitions and a more distinct alternating arrangement of nanolayers approximately 10 nm thick. These differences in coating structure and composition led to marked differences in physical and mechanical properties. The coatings with Cr and CrN underlayers had hardness values of 26 ± 2.6 and 20 ± 2.1 GPa and elastic moduli of 257 ± 23 and 246 ± 23 GPa, respectively. The higher hardness of the coating with the Cr underlayer is attributed to solid-solution strengthening. Although the loads required to initiate the first crack were similar, complete wear-through to the substrate occurred at 4.71 N for the coating with Cr underlayer and at 5.86 N for the coating with the CrN underlayers. The results demonstrate that, under the conditions studied, the CrN underlayer better preserves the multilayer structure and allows the coating to withstand a higher load before complete wear-through, whereas the Cr underlayer yields a harder coating
- 14 October 2026
- Published by National University of Science and Technology MISiS in Powder Metallurgy аnd Functional Coatings
Open AccessEffect of Cr and CrN interlayers on the structure and mechanical properties of multilayer Ti–Al–Mo–N coatings
This study investigated the effects of metallic chromium (Cr) and chromium nitride (CrN) underlayers on the structure and mechanical properties of TiN/Mo₂N multilayer coatings deposited on 13KhFA steel. The coatings were produced by vacuum arc deposition, alternating coating growth with heating by ion bombardment. The coatings were approximately 750 nm thick, and the Cr and CrN underlayers were 300 and 700 nm thick, respectively. Silicon from the steel substrate was detected in the coating deposited on the Cr underlayer, which also exhibited more pronounced intermixing between sublayers. In contrast, no silicon was detected in the coating deposited on the CrN underlayer using the analytical method employed. This coating exhibited sharper compositional transitions and a more distinct alternating arrangement of nanolayers approximately 10 nm thick. These differences in coating structure and composition led to marked differences in physical and mechanical properties. The coatings with Cr and CrN underlayers had hardness values of 26 ± 2.6 and 20 ± 2.1 GPa and elastic moduli of 257 ± 23 and 246 ± 23 GPa, respectively. The higher hardness of the coating with the Cr underlayer is attributed to solid-solution strengthening. Although the loads required to initiate the first crack were similar, complete wear-through to the substrate occurred at 4.71 N for the coating with Cr underlayer and at 5.86 N for the coating with the CrN underlayers. The results demonstrate that, under the conditions studied, the CrN underlayer better preserves the multilayer structure and allows the coating to withstand a higher load before complete wear-through, whereas the Cr underlayer yields a harder coating
- Open Access
- 3 April 2026
- Published by Elsevier in SSRN Electronic Journal
Structure and composition of arc-PVD coatings deposited in Ar and N2 residual atmospheres via Zr/(ZrB2-SiC) combined cathode evaporation
Deposition of coatings based on the Zr-B-Si-C system was carried out by vacuum arc evaporation using combined cathodes, which consist of a sintered ZrB₂–SiC ceramic insert embedded in a bulk zirconium cathode. The coatings have an amorphous structure with pronounced structural heterogeneity, manifesting as layers ranging from 1 to 15 nm in size. These layers have varying contents of the elements present in the cathode and are separated by boundaries. The observed multi-layered nature of the structure is related to the architectural design of the combined cathodes used and their evaporation within the cathode spots of the vacuum electric arc. The constant movement of cathode spots across the cathode surface, facilitated by a system of magnetic coils, results in a stochastic probability of evaporation for its different components from various areas. Consequently, the generated plasma flux, enriched with various components, interacts with the substrate to form the structural and phase heterogeneity of the coating. By determining the binding energies of photoelectrons C1s, N1s, Zr3d + B1s, Si2p, the composition of the formed coatings and the influence of the energy of the sputtered ions on it were established.
- 3 April 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessStructure and composition of arc-PVD coatings deposited in Ar and N2 residual atmospheres via Zr/(ZrB2-SiC) combined cathode evaporation
Deposition of coatings based on the Zr-B-Si-C system was carried out by vacuum arc evaporation using combined cathodes, which consist of a sintered ZrB₂–SiC ceramic insert embedded in a bulk zirconium cathode. The coatings have an amorphous structure with pronounced structural heterogeneity, manifesting as layers ranging from 1 to 15 nm in size. These layers have varying contents of the elements present in the cathode and are separated by boundaries. The observed multi-layered nature of the structure is related to the architectural design of the combined cathodes used and their evaporation within the cathode spots of the vacuum electric arc. The constant movement of cathode spots across the cathode surface, facilitated by a system of magnetic coils, results in a stochastic probability of evaporation for its different components from various areas. Consequently, the generated plasma flux, enriched with various components, interacts with the substrate to form the structural and phase heterogeneity of the coating. By determining the binding energies of photoelectrons C1s, N1s, Zr3d + B1s, Si2p, the composition of the formed coatings and the influence of the energy of the sputtered ions on it were established.