Linqing Liu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Linqing Liu has a total of 11 co-authors. Here are the top co-authors by number of shared publications:
- Changjun Han
South China University of Technology
1 shared publication - Di Wang
School of Mechanical and Automotive Engineering, South China University of Technology, Guangzhou 510641, China
1 shared publication - Hua Tan
State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi’an 710072, China
1 shared publication - Jingguang Du
School of Mechanical and Automotive Engineering, South China University of Technology, Guangzhou 510641, China
1 shared publication - Leilei Wang
College of Materials Science and Technology, Nanjing University of Aeronautics and Astronautics, Nanjing 211106, China
1 shared publication - Pengju Wang
School of Mechanical and Automotive Engineering, South China University of Technology, Guangzhou 510641, China
1 shared publication
Latest Publications
- Open Access
Effects of Scan Speed on Crack Elimination, Microstructural Evolution, and Mechanical Properties of IN738LC Alloy Processed by Laser Powder Bed Fusion
Cracking represents a critical issue in γ’-strengthened Ni-based superalloys processed via laser powder bed fusion. This study systematically investigated the influence of scan speed (800–1200 mm/s) on the crack elimination mechanism, microstructural evolution, and mechanical properties of LPBF-processed IN738LC alloy. Near-defect-free IN738LC parts were successfully produced with a relative density of 99.6% and a crack density of only 0.025%. The results indicate that as the scan speed increased from 800 mm/s to 1100 mm/s, a flatter melt pool (S4) was obtained, which reduced the proportion of high-angle grain boundaries. The cooling rate also increased from 13.68 K/μs to 15.96 K/μs, promoting grain refinement and the dispersion precipitation of MC carbides. The refined grains effectively suppressed stress concentration and inhibited crack propagation along grain boundaries. The optimized process (1100 mm/s) achieved optimal comprehensive mechanical properties. Compared to a scan speed of 800 mm/s, the ultimate tensile strength, yield strength, and elongation at room-temperature increased from 1075 MPa, 820 MPa, and 13.2% to 1179 MPa, 871 MPa, and 21.1%, respectively, while hardness increased from 365 HV1.0 to 387 HV1.0. This study demonstrated that the microstructure and mechanical properties of LPBF-processed IN738LC alloy can be tailored via controlling the thermal history of the melt pool, providing a foundation for processing high-crack-sensitivity alloys utilizing laser powder bed fusion.
Open AccessEffects of Scan Speed on Crack Elimination, Microstructural Evolution, and Mechanical Properties of IN738LC Alloy Processed by Laser Powder Bed Fusion
Cracking represents a critical issue in γ’-strengthened Ni-based superalloys processed via laser powder bed fusion. This study systematically investigated the influence of scan speed (800–1200 mm/s) on the crack elimination mechanism, microstructural evolution, and mechanical properties of LPBF-processed IN738LC alloy. Near-defect-free IN738LC parts were successfully produced with a relative density of 99.6% and a crack density of only 0.025%. The results indicate that as the scan speed increased from 800 mm/s to 1100 mm/s, a flatter melt pool (S4) was obtained, which reduced the proportion of high-angle grain boundaries. The cooling rate also increased from 13.68 K/μs to 15.96 K/μs, promoting grain refinement and the dispersion precipitation of MC carbides. The refined grains effectively suppressed stress concentration and inhibited crack propagation along grain boundaries. The optimized process (1100 mm/s) achieved optimal comprehensive mechanical properties. Compared to a scan speed of 800 mm/s, the ultimate tensile strength, yield strength, and elongation at room-temperature increased from 1075 MPa, 820 MPa, and 13.2% to 1179 MPa, 871 MPa, and 21.1%, respectively, while hardness increased from 365 HV1.0 to 387 HV1.0. This study demonstrated that the microstructure and mechanical properties of LPBF-processed IN738LC alloy can be tailored via controlling the thermal history of the melt pool, providing a foundation for processing high-crack-sensitivity alloys utilizing laser powder bed fusion.