Zuyong Wei
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Zuyong Wei has a total of 4 co-authors. Here are the top co-authors by number of shared publications:
Ge Jin
Shanghai Electric Nuclear Power Equipment Co. Ltd. Shanghai China
1 shared publicationGuiqing Zhang
School of Materials Science and Engineering Shenyang University of Technology Shenyang China
1 shared publication- Jiaqing You
School of Materials Science and Engineering Shenyang University of Technology Shenyang China
1 shared publication - Yunhai Su
School of Materials Science and Engineering Shenyang University of Technology Shenyang China
1 shared publication
Latest Publications
- 30 May 2026
- Published by Wiley in Advanced Engineering Materials
- Vol. 28 (15)
Effect of Transverse Auxiliary Magnetic Field Strength on the Microstructure, Mechanical Properties, and Ductility‐Dip Cracking Susceptibility of ERNiCrFe‐7A GTAW Overlays
ERNiCrFe‐7A is widely used for welding critical nuclear‐island components because of its excellent corrosion resistance and high‐temperature performance. However, it remains susceptible to ductility‐dip cracking (DDC) during thick‐section welding. In this study, transverse magnetic‐field‐assisted gas tungsten arc welding was utilized to fabricate ERNiCrFe‐7A overlays. The effects of magnetic field strength on weld microstructure and mechanical properties were systematically investigated. Applying the magnetic field transformed coarse, elongated (Nb and Ti)C precipitates into fine, dispersed particles and converted Cr 23 C 6 precipitates at grain‐boundary triple junctions from thick, continuous lamellae to discontinuous granular particles. With increasing magnetic field strength, grain size and kernel average misorientation first decreased and then increased, whereas the fractions of low‐angle grain boundaries (LAGBs) and low‐Σ coincidence‐site lattice (CSL) boundaries first increased and then decreased. At 10 mT, the overlay exhibited the highest hardness of 188.7 HV and the best tensile properties, with tensile and yield strengths of 567.5 and 387.6 MPa, respectively, at 350°C. The critical strain for crack initiation at 950°C also increased and then decreased with increasing magnetic field. The critical strain for crack initiation increased to about 6% at 10 mT. The improved strength–ductility balance and reduced DDC susceptibility are attributed to mechanical interlocking induced by grain‐boundary serration, enhanced precipitate dispersion, Cr 23 C 6 granulation, and increased fractions of LAGBs and low‐Σ CSL boundaries.
- 30 May 2026
- Published by Wiley in Advanced Engineering Materials
- Vol. 28 (15)
Effect of Transverse Auxiliary Magnetic Field Strength on the Microstructure, Mechanical Properties, and Ductility‐Dip Cracking Susceptibility of ERNiCrFe‐7A GTAW Overlays
ERNiCrFe‐7A is widely used for welding critical nuclear‐island components because of its excellent corrosion resistance and high‐temperature performance. However, it remains susceptible to ductility‐dip cracking (DDC) during thick‐section welding. In this study, transverse magnetic‐field‐assisted gas tungsten arc welding was utilized to fabricate ERNiCrFe‐7A overlays. The effects of magnetic field strength on weld microstructure and mechanical properties were systematically investigated. Applying the magnetic field transformed coarse, elongated (Nb and Ti)C precipitates into fine, dispersed particles and converted Cr 23 C 6 precipitates at grain‐boundary triple junctions from thick, continuous lamellae to discontinuous granular particles. With increasing magnetic field strength, grain size and kernel average misorientation first decreased and then increased, whereas the fractions of low‐angle grain boundaries (LAGBs) and low‐Σ coincidence‐site lattice (CSL) boundaries first increased and then decreased. At 10 mT, the overlay exhibited the highest hardness of 188.7 HV and the best tensile properties, with tensile and yield strengths of 567.5 and 387.6 MPa, respectively, at 350°C. The critical strain for crack initiation at 950°C also increased and then decreased with increasing magnetic field. The critical strain for crack initiation increased to about 6% at 10 mT. The improved strength–ductility balance and reduced DDC susceptibility are attributed to mechanical interlocking induced by grain‐boundary serration, enhanced precipitate dispersion, Cr 23 C 6 granulation, and increased fractions of LAGBs and low‐Σ CSL boundaries.