Tuğçe Gültan
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Tuğçe Gültan has a total of 9 co-authors. Here are the top co-authors by number of shared publications:
- Menemşe Gümüşderelioğlu
Bioengineering Division, Graduate School of Science and Engineering, Hacettepe University, Ankara 06800, Turkey
3 shared publications - Elvan Konuk Tokak
Department of Chemical Engineering, Faculty of Engineering, Hacettepe University, Ankara 06800, Turkey
2 shared publications Menemşe Gümüşderelioğlu
2 shared publications- Damla Çetin Altındal
HACETTEPE UNIVERSITY, INSTITUTE OF SCIENCE, DEPARTMENT OF BIOENGINEERING (INTERDISCIPLINARY), BIOENGINEERING (DR)
1 shared publication - Efkan Çatıker
Ordu University
1 shared publication M. Gümüşderelioğlu
Inst. of Graduate Studies in Science, Hacettepe University, Ankara, Turkey
1 shared publication
Latest Publications
- Open Access
- 23 June 2026
- Published by MDPI AG in Journal of Functional Biomaterials
- Vol. 17 (7) , 310
Thickness-Tunable Bilayer PBAT Nanofibrous Scaffolds for Enhancing r-AdMSCs’ Tenogenic Commitment in Supraspinatus Tendon Regeneration
Acute or chronic rotator cuff tears are major causes of shoulder dysfunction, motivating the development of scaffolds with tailored thickness and mechanics for supraspinatus tendon regeneration. This study aimed to investigate the effect of bilayer poly(butylene adipate-co-terephthalate) (PBAT) scaffold thickness on the tenogenic differentiation of rat adipose mesenchymal stem cells (r-AdMSCs) and supraspinatus tendon regeneration. Aligned fibers with a diameter of approximately 476 nm were deposited onto randomly oriented layers at different times (4 h; 4S, 6 h; 6S, 8 h; 8S), and scaffolds with increasing thicknesses from 441 µm (4S) to 1132 µm (8S) were produced. Mechanical testing showed comparable tensile strength for 4S and 6S (≈1.9–2.0 MPa) and modulus (5.5–7.3 MPa), while 8S exhibited markedly reduced stiffness (0.5 MPa) and hyper elastic deformation. Mechanical performance across degradation conditions remained strongly thickness-dependent: thinner scaffolds retained integrity and strengthened, with modulus increases during hydrolytic and enzymatic degradation, whereas thicker matrices showed limited remodeling and instability. Rat-AdMSCs’ were cultured on the scaffolds for 21 days. Cell-free and cell-laden mechanical responses further reflected thickness effects: cell-free samples stiffened due to media-induced passive matrix tightening, whereas cell-laden scaffolds showed extracellular matrix (ECM)-driven reinforcement, most prominently in 4S, which reached 2.1 MPa tensile strength with improved elasticity and balanced deformation. The 4S scaffold exhibited the highest tensile strength and significantly increased collagen-1 (col1), tenomodulin (tnmd) and scleraxis (scx) expression compared with the other groups. In conclusion, among all groups, 4S scaffolds demonstrated the most favorable mechanical and biological performance, suggesting that scaffold thickness plays a critical role in regulating tendon regeneration and will become even more suitable when matured in bioreactors.
- 23 June 2026
- Published by MDPI AG in Journal of Functional Biomaterials
- Vol. 17 (7) , 310
Open AccessThickness-Tunable Bilayer PBAT Nanofibrous Scaffolds for Enhancing r-AdMSCs’ Tenogenic Commitment in Supraspinatus Tendon Regeneration
Acute or chronic rotator cuff tears are major causes of shoulder dysfunction, motivating the development of scaffolds with tailored thickness and mechanics for supraspinatus tendon regeneration. This study aimed to investigate the effect of bilayer poly(butylene adipate-co-terephthalate) (PBAT) scaffold thickness on the tenogenic differentiation of rat adipose mesenchymal stem cells (r-AdMSCs) and supraspinatus tendon regeneration. Aligned fibers with a diameter of approximately 476 nm were deposited onto randomly oriented layers at different times (4 h; 4S, 6 h; 6S, 8 h; 8S), and scaffolds with increasing thicknesses from 441 µm (4S) to 1132 µm (8S) were produced. Mechanical testing showed comparable tensile strength for 4S and 6S (≈1.9–2.0 MPa) and modulus (5.5–7.3 MPa), while 8S exhibited markedly reduced stiffness (0.5 MPa) and hyper elastic deformation. Mechanical performance across degradation conditions remained strongly thickness-dependent: thinner scaffolds retained integrity and strengthened, with modulus increases during hydrolytic and enzymatic degradation, whereas thicker matrices showed limited remodeling and instability. Rat-AdMSCs’ were cultured on the scaffolds for 21 days. Cell-free and cell-laden mechanical responses further reflected thickness effects: cell-free samples stiffened due to media-induced passive matrix tightening, whereas cell-laden scaffolds showed extracellular matrix (ECM)-driven reinforcement, most prominently in 4S, which reached 2.1 MPa tensile strength with improved elasticity and balanced deformation. The 4S scaffold exhibited the highest tensile strength and significantly increased collagen-1 (col1), tenomodulin (tnmd) and scleraxis (scx) expression compared with the other groups. In conclusion, among all groups, 4S scaffolds demonstrated the most favorable mechanical and biological performance, suggesting that scaffold thickness plays a critical role in regulating tendon regeneration and will become even more suitable when matured in bioreactors.
- 2 December 2025
- Published by Elsevier in Journal of Photochemistry and Photobiology B: Biology
- Vol. 274, 113331
Photobiomodulation-driven cardiomyogenic differentiation and endothelial vascularization: A dual approach with Aloe Vera
- 2 December 2025
- Published by Elsevier in Journal of Photochemistry and Photobiology B: Biology
- Vol. 274, 113331
Photobiomodulation-driven cardiomyogenic differentiation and endothelial vascularization: A dual approach with Aloe Vera
- 30 April 2020
- Published by IOP Publishing in Biomedical Materials
- Vol. 15 (3) , 035019
NaOH-etched/boron-doped nanohydroxyapatite-coated PEEK implants enhance the proliferation and differentiation of osteogenic cells
The aim of the present study is to eliminate the bioinertness of polyetheretherketone (PEEK) material and to increase its osteogenic activity by applying a number of surface modifications in order to discover the most effective method. First, the surface of the bare PEEK (B-PEEK) was mechanically modified by sandblasting (S-PEEK). As a second method, physical modification was provided by etching of B-PEEK in 10 M sodium hydroxide (NaOH) solution at 60 °C for 48 h (N-PEEK). Following the sandblasting, S-PEEK samples were also etched with NaOH to obtain SN-PEEK samples. In order to increase osteogenic activity of the mechanically and/or physically modified PEEK samples, they were coated with boron-doped nanohydroxyapatite (B-nHAp) in the presence of microwave energy. Thus, B-PEEK/B-nHAp, S-PEEK/B-nHAp, N-PEEK/B-nHAp and SN-PEEK/B-nHAp samples were obtained. While water contact angles and surface roughness of the B-PEEK samples increased after modification, hydrophilicity increased with B-nHAp coating. Cell culture results demonstrated that high proliferation and differentiation capacities of MC3T3-E1 cells were obtained on the B-nHAP-coated surfaces compared to uncoated specimens. However, channeled texture of both the N-PEEK and N-PEEK/B-nHAp samples enhanced Col1a1 mRNA expression and collagen secretion in addition to increased alkaline phosphatase (ALP) activity when compared to other groups. As a result, it was determined that the bioactivity increased on the modified PEEK surfaces, but the most effective osteogenic activity was provided with B-nHAp coatings. The synergetic effect of NaOH etching and B-nHAp coatings might be used as a promising surface modification method to use PEEK material in orthopedic and dental applications with increased osteogenic activity.
- 30 April 2020
- Published by IOP Publishing in Biomedical Materials
- Vol. 15 (3) , 035019
NaOH-etched/boron-doped nanohydroxyapatite-coated PEEK implants enhance the proliferation and differentiation of osteogenic cells
The aim of the present study is to eliminate the bioinertness of polyetheretherketone (PEEK) material and to increase its osteogenic activity by applying a number of surface modifications in order to discover the most effective method. First, the surface of the bare PEEK (B-PEEK) was mechanically modified by sandblasting (S-PEEK). As a second method, physical modification was provided by etching of B-PEEK in 10 M sodium hydroxide (NaOH) solution at 60 °C for 48 h (N-PEEK). Following the sandblasting, S-PEEK samples were also etched with NaOH to obtain SN-PEEK samples. In order to increase osteogenic activity of the mechanically and/or physically modified PEEK samples, they were coated with boron-doped nanohydroxyapatite (B-nHAp) in the presence of microwave energy. Thus, B-PEEK/B-nHAp, S-PEEK/B-nHAp, N-PEEK/B-nHAp and SN-PEEK/B-nHAp samples were obtained. While water contact angles and surface roughness of the B-PEEK samples increased after modification, hydrophilicity increased with B-nHAp coating. Cell culture results demonstrated that high proliferation and differentiation capacities of MC3T3-E1 cells were obtained on the B-nHAP-coated surfaces compared to uncoated specimens. However, channeled texture of both the N-PEEK and N-PEEK/B-nHAp samples enhanced Col1a1 mRNA expression and collagen secretion in addition to increased alkaline phosphatase (ALP) activity when compared to other groups. As a result, it was determined that the bioactivity increased on the modified PEEK surfaces, but the most effective osteogenic activity was provided with B-nHAp coatings. The synergetic effect of NaOH etching and B-nHAp coatings might be used as a promising surface modification method to use PEEK material in orthopedic and dental applications with increased osteogenic activity.
- 13 February 2020
- Published by Taylor & Francis in International Journal of Polymeric Materials and Polymeric Biomaterials
- Vol. 70 (6) , 371-382
Synergistic effect of fabrication and stabilization methods on physicochemical and biological properties of chitosan scaffolds
In this study, the aim was to investigate the changes in the physical, chemical and biological properties of chitosan scaffolds obtained by freeze-drying and microwave-assisted gas foaming methods. Also, it was aimed to determine the most suitable one when scaffolds are subjected to different stabilization processes. To prevent the solubility of chitosan scaffolds, stabilization processes were carried out by treatment with ethanol (EtOH), sodium hydroxide (NaOH), or sodium bicarbonate (Na2CO3). The chemical and physical changes in the chitosan structure induced by different stabilization methods were investigated by characterization studies carried out comparatively with two-dimensional chitosan films. The results showed that, particularly, NaOH stabilization improved the physical, thermal, and mechanical properties of the bulk material. The wettability and surface roughness of the chitosan films were enhanced for cellular adhesion after stabilization. Cell culture studies revealed that variations in both fabrication and stabilization methods significantly affected in vitro cellular responses such as cell attachment, proliferation and viability. In conclusion, chitosan scaffolds fabricated by microwave-assisted gas foaming and stabilized by NaOH solution were found as the best structure due to their higher cellular activities.
- 13 February 2020
- Published by Taylor & Francis in International Journal of Polymeric Materials and Polymeric Biomaterials
- Vol. 70 (6) , 371-382
Synergistic effect of fabrication and stabilization methods on physicochemical and biological properties of chitosan scaffolds
In this study, the aim was to investigate the changes in the physical, chemical and biological properties of chitosan scaffolds obtained by freeze-drying and microwave-assisted gas foaming methods. Also, it was aimed to determine the most suitable one when scaffolds are subjected to different stabilization processes. To prevent the solubility of chitosan scaffolds, stabilization processes were carried out by treatment with ethanol (EtOH), sodium hydroxide (NaOH), or sodium bicarbonate (Na2CO3). The chemical and physical changes in the chitosan structure induced by different stabilization methods were investigated by characterization studies carried out comparatively with two-dimensional chitosan films. The results showed that, particularly, NaOH stabilization improved the physical, thermal, and mechanical properties of the bulk material. The wettability and surface roughness of the chitosan films were enhanced for cellular adhesion after stabilization. Cell culture studies revealed that variations in both fabrication and stabilization methods significantly affected in vitro cellular responses such as cell attachment, proliferation and viability. In conclusion, chitosan scaffolds fabricated by microwave-assisted gas foaming and stabilized by NaOH solution were found as the best structure due to their higher cellular activities.
- 21 January 2019
- Published by Taylor & Francis in International Journal of Polymeric Materials and Polymeric Biomaterials
- Vol. 68 (6) , 338-349
Enhancement of scaffolding properties for poly(3-hydroxybutyrate): blending with poly-β-alanine and wet electrospinning
Poly-β-alanine (PBA), and its derivatives poly(α-methyl-β-alanine) and poly[N-(3-methoxypropyl-β-alanine) were synthesized by hydrogen transfer polymerization (HTP). Porous 3 D matrices of poly(3-hydroxybutyrate) (P3HB) reinforced with PBA/its derivatives were obtained via lyophilization and wet electrospinning. However, mechanical properties of the porous matrices prepared by wet electrospinning were found to present superior performance for tissue engineering applications. Cell culture study was performed by using wet electrospun P3HB matrices doped with 10% (w/w) PBA which show better manipulation ability, chemical and mechanical properties. Scaffolds of P3HB-PBA (10% w/w) blend was determined to demonstrate better cell attachment and proliferation compared to the scaffolds of pure P3HB.
- 21 January 2019
- Published by Taylor & Francis in International Journal of Polymeric Materials and Polymeric Biomaterials
- Vol. 68 (6) , 338-349
Enhancement of scaffolding properties for poly(3-hydroxybutyrate): blending with poly-β-alanine and wet electrospinning
Poly-β-alanine (PBA), and its derivatives poly(α-methyl-β-alanine) and poly[N-(3-methoxypropyl-β-alanine) were synthesized by hydrogen transfer polymerization (HTP). Porous 3 D matrices of poly(3-hydroxybutyrate) (P3HB) reinforced with PBA/its derivatives were obtained via lyophilization and wet electrospinning. However, mechanical properties of the porous matrices prepared by wet electrospinning were found to present superior performance for tissue engineering applications. Cell culture study was performed by using wet electrospun P3HB matrices doped with 10% (w/w) PBA which show better manipulation ability, chemical and mechanical properties. Scaffolds of P3HB-PBA (10% w/w) blend was determined to demonstrate better cell attachment and proliferation compared to the scaffolds of pure P3HB.