- 17 November 2026
- Published by Elsevier in Engineering Structures
- Vol. 371
Experimental and numerical investigation on the flexural performance of UHPC–NC beam-to-beam joints in steel–concrete composite girders
- 17 November 2026
- Published by Elsevier in Engineering Structures
- Vol. 371
Experimental and numerical investigation on the flexural performance of UHPC–NC beam-to-beam joints in steel–concrete composite girders
- Open Access
- 18 June 2026
- Published by Elsevier in SSRN Electronic Journal
Experimental and Numerical Investigation on the Flexural Performance of UHPC–NC Beam-to-beam Joints in Steel–concrete Composite Girders
A novel ultra-high performance concrete (UHPC) –normal concrete (NC) beam-to-beam joint with embedded steel girders and end plates with studs was proposed to ensure reliable force transfer between steel and concrete components. A full-scale double-cantilever flexural test, nonlinear finite element (FE) simulation, and theoretical analysis were conducted to investigate its flexural behavior. The test results showed that the specimen failed due to local buckling of the lower flange and web. Simplified load–reinforcement stress models were proposed and agreed well with test results. Model Code 2010 provided reasonable predictions for UHPC crack width, with an average calculated-to-measured ratio of 0.86 and a coefficient of variation (COV) of 0.16. Parametric analysis indicated that the lower flange thickness had the greatest influence on the initial stiffness K0 and cracking load Pcr, whereas the longitudinal reinforcement ratio was the most influential parameter for the ultimate load Pu. Increasing the UHPC layer thickness from 0 mm to 150 mm raised Pcr by 27.6%, while increasing the number of perfobond connectors from 0 to 22 increased Pcr by 9.4%–13.6% and the initial rotational stiffness S0 by 44.9%–55.9%. In addition, the cohesive zone model (CZM) reasonably simulated UHPC–NC interface behavior, and increasing the normal bond strength from 2.22 MPa to 5.18 MPa reduced the interfacial crack width by 9.0%–9.6%. The modified plastic method accurately predicted the flexural capacity, with a mean predicted-to-simulated ratio of 0.97 and a COV of 0.03. Overall, the proposed joint offers a practical solution for prefabricated composite girders.
- 18 June 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessExperimental and Numerical Investigation on the Flexural Performance of UHPC–NC Beam-to-beam Joints in Steel–concrete Composite Girders
A novel ultra-high performance concrete (UHPC) –normal concrete (NC) beam-to-beam joint with embedded steel girders and end plates with studs was proposed to ensure reliable force transfer between steel and concrete components. A full-scale double-cantilever flexural test, nonlinear finite element (FE) simulation, and theoretical analysis were conducted to investigate its flexural behavior. The test results showed that the specimen failed due to local buckling of the lower flange and web. Simplified load–reinforcement stress models were proposed and agreed well with test results. Model Code 2010 provided reasonable predictions for UHPC crack width, with an average calculated-to-measured ratio of 0.86 and a coefficient of variation (COV) of 0.16. Parametric analysis indicated that the lower flange thickness had the greatest influence on the initial stiffness K0 and cracking load Pcr, whereas the longitudinal reinforcement ratio was the most influential parameter for the ultimate load Pu. Increasing the UHPC layer thickness from 0 mm to 150 mm raised Pcr by 27.6%, while increasing the number of perfobond connectors from 0 to 22 increased Pcr by 9.4%–13.6% and the initial rotational stiffness S0 by 44.9%–55.9%. In addition, the cohesive zone model (CZM) reasonably simulated UHPC–NC interface behavior, and increasing the normal bond strength from 2.22 MPa to 5.18 MPa reduced the interfacial crack width by 9.0%–9.6%. The modified plastic method accurately predicted the flexural capacity, with a mean predicted-to-simulated ratio of 0.97 and a COV of 0.03. Overall, the proposed joint offers a practical solution for prefabricated composite girders.