Manuel Vite Torres
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Manuel Vite Torres has a total of 5 co-authors. Here are the top co-authors by number of shared publications:
- César Sedano-De la Rosa
Universidad de Guadalajara
1 shared publication - Ezequiel Alberto Gallardo-Hernández
SEPI-Escuela Superior de Ingeniería Mecánica y Eléctrica, Instituto Politécnico Nacional, Unidad Zacatenco, Grupo de Tribología, Col. Lindavista, C.P. 07738, Ciudad de México, México
1 shared publication - Javier Alejandro Frias Flores
Universidad Veracruzana
1 shared publication - Jesús Gilberto Godinez Salcedo
Instituto Politécnico Nacional
1 shared publication Sergio Eduardo Vázquez-Mondragón
SEPI-Escuela Superior de Ingeniería Mecánica y Eléctrica, Instituto Politécnico Nacional, Unidad Zacatenco, Grupo de Tribología, Col. Lindavista, C.P. 07738, Ciudad de México, México
1 shared publication
Latest Publications
- 6 July 2026
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part J: Journal of Engineering Tribology
- Vol. 240 (11) , 2251-2266
Solid particle erosion of aluminium alloy of aircraft fuselage skin
Solid particle erosion (SPE) has been a significant problem since the beginning of modern aviation. SPE is caused by sand and volcanic ash particles, when an aircraft is taking off or landing, or passing through volcanic ash clouds even far from the crater. The current scope of knowledge on SPE studies affecting a fuselage skin material and some others turbine components caused by volcanic ash particles is still restricted. Volcanic ash particles can cause damage to the windscreens, fuselage surfaces, and compressor fan blades, among others. The aim of this work is to highlight the importance of erosion in aerospace vehicles related to the volcanic ash impacts on aluminium alloy used for aircraft fuselage skins at room temperature. Volcanic ash particles were collected and characterized with a hardness of 5 on the Mohs scale and an average size of 200 µm with angular morphology; additionally, chemical composition was determined. A series of tests were performed with a particle velocity of 55 m/s at three impact angles (30°, 60°, and 90°). The results show the wear rates for these three impact angles, revealing a low wear rate at high angles and higher wear rate at 30 °. Furthermore, wear profiles were taken from the wear scars, and microscopically some images were analysed to identify the wear mechanisms. The target material, when subjected to the impact of angular solid particles exhibited similar behaviour.
- 6 July 2026
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part J: Journal of Engineering Tribology
- Vol. 240 (11) , 2251-2266
Solid particle erosion of aluminium alloy of aircraft fuselage skin
Solid particle erosion (SPE) has been a significant problem since the beginning of modern aviation. SPE is caused by sand and volcanic ash particles, when an aircraft is taking off or landing, or passing through volcanic ash clouds even far from the crater. The current scope of knowledge on SPE studies affecting a fuselage skin material and some others turbine components caused by volcanic ash particles is still restricted. Volcanic ash particles can cause damage to the windscreens, fuselage surfaces, and compressor fan blades, among others. The aim of this work is to highlight the importance of erosion in aerospace vehicles related to the volcanic ash impacts on aluminium alloy used for aircraft fuselage skins at room temperature. Volcanic ash particles were collected and characterized with a hardness of 5 on the Mohs scale and an average size of 200 µm with angular morphology; additionally, chemical composition was determined. A series of tests were performed with a particle velocity of 55 m/s at three impact angles (30°, 60°, and 90°). The results show the wear rates for these three impact angles, revealing a low wear rate at high angles and higher wear rate at 30 °. Furthermore, wear profiles were taken from the wear scars, and microscopically some images were analysed to identify the wear mechanisms. The target material, when subjected to the impact of angular solid particles exhibited similar behaviour.
- 30 June 2026
- Published by Cientifica, Revista Mexicana de Ingenieria Electromecanica y de Sistemas, IPN
- Vol. 30 (1) , 1-12
Evaluation of corrosion behavior of a pipeline carbon steel (API 5L-X52) subjected to a short-term immersion test in a sour aqueous media
API carbon steels pipes are widely used in oil and gas industry for transporting products. They are constantly exposed to aggressive environments, most of them rich in CO2 and H2S concentrations, which increases wear by corrosion. This study investigated the corrosive behavior of API 5L-X52 carbon steel when immersed in a static solution simulating sour media for short periods of time, simulating conditions of initial contact between a sour media and API steels, which is of interest because oil production pipelines are affected by corrosion, causing embrittlement even after very short service times. Tests were performed according to ASTM G31 standard. The mass loss method was used to evaluate corrosion rates at each time point, and Scanning Electron Microscopy (SEM) with Energy Dispersive X Ray Spectroscopy (EDS) was used to characterize the microstructure and corrosion products of the samples. The results showed that the first few hours of contact with the sour media generate a peak in the corrosion rate; after this time, corrosion rate decreases and tends to stabilize. Furthermore, the presence of H2S in the media accelerates the formation of craters on the surface, causing pitting corrosion damage. Finally, the presence of Sb in the EDS analysis helps to identify corrosion products on the metal surface.
- 30 June 2026
- Published by Cientifica, Revista Mexicana de Ingenieria Electromecanica y de Sistemas, IPN
- Vol. 30 (1) , 1-12
Evaluation of corrosion behavior of a pipeline carbon steel (API 5L-X52) subjected to a short-term immersion test in a sour aqueous media
API carbon steels pipes are widely used in oil and gas industry for transporting products. They are constantly exposed to aggressive environments, most of them rich in CO2 and H2S concentrations, which increases wear by corrosion. This study investigated the corrosive behavior of API 5L-X52 carbon steel when immersed in a static solution simulating sour media for short periods of time, simulating conditions of initial contact between a sour media and API steels, which is of interest because oil production pipelines are affected by corrosion, causing embrittlement even after very short service times. Tests were performed according to ASTM G31 standard. The mass loss method was used to evaluate corrosion rates at each time point, and Scanning Electron Microscopy (SEM) with Energy Dispersive X Ray Spectroscopy (EDS) was used to characterize the microstructure and corrosion products of the samples. The results showed that the first few hours of contact with the sour media generate a peak in the corrosion rate; after this time, corrosion rate decreases and tends to stabilize. Furthermore, the presence of H2S in the media accelerates the formation of craters on the surface, causing pitting corrosion damage. Finally, the presence of Sb in the EDS analysis helps to identify corrosion products on the metal surface.