John A Olsen
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
John A Olsen has a total of 10 co-authors. Here are the top co-authors by number of shared publications:
- Aleksei V. Solomonov
Weizmann Institute of Science
1 shared publication - Alfons Schulte
Department of Physics, University of Central Florida 1 , Orlando, Florida 32816
1 shared publication - Arie Ruzin
School of Electrical Engineering, Tel Aviv University 5 , Tel Aviv 69978
1 shared publication - Chao-Ching Chiang
University of Florida
1 shared publication - Fan Ren
Department of Chemical Engineering, University of Florida 3 , Gainesville, Florida 32611
1 shared publication - Gabriel Marciaga
Department of Physics, University of Central Florida 1 , Orlando, Florida 32816
1 shared publication
Latest Publications
- Open Access
- 1 July 2026
- Published by The Electrochemical Society in ECS Journal of Solid State Science and Technology
- Vol. 15 (7) , 075004
Electron Beam Irradiation-Induced Transport and Recombination in P-type Diamond Diodes
This study investigates minority carrier diffusion length ( L ) and defect-mediated recombination phenomena in boron-doped p-type diamond epitaxial layers. Utilizing temperature-dependent electron beam-induced current (EBIC) and cathodoluminescence (CL), the influence of temperature and sustained electron beam irradiation was characterized. The diamond sample demonstrates a pronounced thermal enhancement to the minority carrier diffusion length. This temperature enhancement for L has an activation energy of 177 meV. Furthermore, sustained electron injection induces a near-linear elongation of the diffusion length through passivation of deep-level defects. From the EBIC injection data, an activation energy of 151 meV was extracted from fitting. Temperature-resolved CL reveals the quenching of the characteristic A-band emission at 100 °C. Additionally, a thermal activation energy of 112 meV was extracted via a decay fit of the temperature dependent CL intensity data. While sustained electron beam irradiation reveals dose-dependent quenching of the A-band emission with thermally activated decay rates. This yields activation energies of 110 meV and 11 meV associated with distinct defect generation mechanisms at high and low temperatures, respectively. This provides a complementary assessment of the defect landscape governing minority carrier lifetimes in these boron-doped diamond diodes.
- 1 July 2026
- Published by The Electrochemical Society in ECS Journal of Solid State Science and Technology
- Vol. 15 (7) , 075004
Open AccessElectron Beam Irradiation-Induced Transport and Recombination in P-type Diamond Diodes
This study investigates minority carrier diffusion length ( L ) and defect-mediated recombination phenomena in boron-doped p-type diamond epitaxial layers. Utilizing temperature-dependent electron beam-induced current (EBIC) and cathodoluminescence (CL), the influence of temperature and sustained electron beam irradiation was characterized. The diamond sample demonstrates a pronounced thermal enhancement to the minority carrier diffusion length. This temperature enhancement for L has an activation energy of 177 meV. Furthermore, sustained electron injection induces a near-linear elongation of the diffusion length through passivation of deep-level defects. From the EBIC injection data, an activation energy of 151 meV was extracted from fitting. Temperature-resolved CL reveals the quenching of the characteristic A-band emission at 100 °C. Additionally, a thermal activation energy of 112 meV was extracted via a decay fit of the temperature dependent CL intensity data. While sustained electron beam irradiation reveals dose-dependent quenching of the A-band emission with thermally activated decay rates. This yields activation energies of 110 meV and 11 meV associated with distinct defect generation mechanisms at high and low temperatures, respectively. This provides a complementary assessment of the defect landscape governing minority carrier lifetimes in these boron-doped diamond diodes.