Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Elshan Sefidgar Shahanaghi has a total of 17 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Yttrium Aluminium Garnet/Decanoic Acid Nanocomposite Phase Change Materials for Passive Thermal Management of an 18650 Li-ion Cell: From Measured Cycling Degradation to CFD Performance

    by Elshan Sefidgar Shahanaghi, Yasin Varol, Şafak Melih Şenocak, Ezgi Gürgenç, Coşkun Özalp, Naim Aslan, Asaf Varol, Turan Gürgenç

    Decanoic acid (DA) based nanocomposite phase change materials (PCMs) containing 0.5–2.0 wt% Y3Al5O12 nanoparticles dispersed with sodium dodecyl sulfate (SDS) were characterised fresh and after 1000 thermal cycles. FT-IR showed a mainly physical incorporation of Y3Al5O12 and an unchanged chemical structure of DA after cycling. Thermal conductivity increased with loading, by 14.2/12.5% (solid/liquid) at 2.0 wt%, and the specific heat was highest at 1.0 wt% (+23.6/27.7%). After 1000 cycles pure DA lost about 6% of its latent heat, whereas the nanocomposites retained 95.0–98.5% of their melting enthalpy. The measured fresh and aged properties were used in a computational fluid dynamics (CFD) model, validated against a fatty acid melting experiment, of an 18650 Li-ion cell wrapped in a 3 mm PCM shell and generating 2 W. Relative to the bare cell, the Al-cased PCM shell extended the time to 45 °C about 3.7-fold. At this point, fresh compositions differed only within the specific heat measurement uncertainty, whereas after 1000 cycles the PCMs with 0.5–1.5 wt% Y3Al5O12 kept this time 3.3–4.7% longer than pure DA, and the aged 1.0 wt% composite matched fresh pure DA (30.1 min). At a second operating point (4 W, 6 mm shell), where the PCM is only partly molten at 45 °C, thermal conductivity was as influential as specific heat and the gain grew with loading, in the fresh state and to +11.4–11.7% at 1.5–2.0 wt% after 1000 cycles. The best loading therefore depended on the operating point.

  • Open Access

    Microstructural Evolution, Densification, and Mechanical–Tribological Performance of AlSi12-Modified NiCrBSi Composites Fabricated by Spark Plasma Sintering

    by Ertuğrul Çelik, Yusuf Donat, Turan Gurgenc, Mehmet Erdi Korkmaz, Elshan Sefidgar Shahanaghi, Cevher Kürsat Macit, Tarık Selçuk Şeker, Asaf Varol

    The combined effects of low AlSi12 additions on densification, mechanical properties and load-dependent wear in bulk NiCrBSi consolidated by spark plasma sintering (SPS) remain insufficiently established. This study evaluates AlSi12 as a metallic modifier to improve hardness and wear resistance while identifying associated flexural-strength trade-offs. Compositions containing 0, 2, 4, 6 and 8 wt.% AlSi12 were processed at 950 °C under 38 MPa for 240 s in nitrogen. Phase constitution, microstructure, density, hardness, bending strength and dry-sliding wear at 50 and 100 N were examined. The Ni-rich matrix remained dominant, with local Al enrichment. Experimental density decreased from 8.01 to 6.97 g/cm3, whereas nominal relative density was highest, at approximately 98.7–98.9%, for 4–6 wt.% AlSi12. The highest reported mean hardness was 581 HV at 6 wt.%, while the unmodified alloy reached the highest maximum nominal flexural stress in the displayed bending records. The lowest specific wear rates were approximately 2.6 × 10−5 and 2.9 × 10−5 mm3/(N·m) for 6 wt.% at 50 N and 8 wt.% at 100 N, respectively. These findings support composition selection based on the required balance of hardness, flexural strength and load-specific wear resistance.

  • Open Access

    Refractory Nitride, Resilient PCM: Titanium Nitride/RT70 HC Nanocomposites for Medium-Temperature Thermal Energy Storage and Management

    by Elshan Sefidgar Shahanaghi, Yasin Varol, Ezgi Gürgenç, Şafak Melih Şenocak, Ayşe Biçer, Turan Gürgenç

    This study tailors titanium nitride (TiN)-reinforced RT70 HC nanocomposite phase change materials (PCMs) for medium-temperature thermal energy storage. TiN nanoparticles were incorporated into commercial RT70 HC at 0.1–2.0 wt.% by a two-stage method combining sodium dodecyl sulfate, magnetic stirring, and ultrasonication, and characterized by FT-IR, XRD, SEM-EDX, elemental mapping, DSC, thermal conductivity, Cp, TGA, and 1000-cycle tests. FT-IR and XRD confirmed the physical integration of TiN into RT70 HC without new chemical bonds or secondary phases, and SEM-EDX showed a concentration-dependent dispersion. The phase change temperatures were largely preserved. The latent heat varied non-monotonically with TiN content, increasing at low loadings (0.1–0.5 wt.%) and decreasing at higher loadings. Because each composition was prepared as a single batch and measured on small specimens, the low-loading latent-heat increase (up to about 9%) is indicative rather than statistically proven and may fall within the subsampling variance. The 0.5 wt.% sample reached the highest values of 306/296 J/g in the first cycle and 286/268 J/g after 1000 cycles. The thermal conductivity increased with TiN content, reaching a maximum enhancement of about 24.09% in the liquid phase (0.1785 to 0.2215 W/(m·K) at 80 °C) and 35.7% in the solid phase at 2.0 wt.%, whereas the specific heat capacity was lower at higher loadings, an indicative trade-off given the single-run measurement uncertainty. TGA showed degradation onset temperatures above 240 °C, a wide safety margin relative to the ~72 °C working range. Overall, the 0.1–0.5 wt.% formulations offered the most balanced thermal performance for medium-temperature applications.