Gengzhong Lin
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Gengzhong Lin has a total of 9 co-authors. Here are the top co-authors by number of shared publications:
- Benchi Li
Hubei Key Laboratory of Electrochemical Power Sources College of Chemistry & Molecular Sciences Wuhan University Wuhan Hubei China
1 shared publication - Guo Tang
Hubei Key Laboratory of Electrochemical Power Sources College of Chemistry & Molecular Sciences Wuhan University Wuhan Hubei China
1 shared publication - Hui Li
State Key Laboratory of New Textile Materials & Advanced Processing Wuhan Textile University Wuhan P. R. China
1 shared publication - Jiangfeng Qian
Hubei Key Laboratory of Electrochemical Power Sources, College of Chemistry and Molecular Sciences Wuhan University Wuhan Hubei China
1 shared publication - Kean Chen
Wuhan University
1 shared publication - Xinping Ai
Wuhan University
1 shared publication
Latest Publications
- Open Access
- 30 October 2026
- Published by Wiley in Advanced Energy Materials
- p. e71780
Constructing an Adaptive Flexible Interphase on Halide Electrolytes by Lewis‐Acid‐Induced Polymerization for High‐Voltage All‐Solid‐State Lithium Batteries
All‐solid‐state lithium batteries (ASSLBs) combining halide solid electrolytes (HSEs) with high‐nickel layered oxide cathodes offer great promise for high energy density, yet they suffer from severe interfacial issues such as oxidative decomposition, mechanical degradation, and chemical incompatibility with sulfide electrolytes. Herein, we report a Lewis‐acid‐induced surface‐softening strategy that constructs a nanoscale adaptive flexible interphase (AFI) via in situ polymerization of acrylonitrile (AN) on a representative halide electrolyte, Li 3 InCl 6 (LIC). The resulting AFI layer concurrently provides ionic conductivity, excellent oxidation stability (>4.8 V), and favorable viscoelasticity, thereby synergistically enhancing the electrochemical, chemical, and mechanical stability of the interface without compromising bulk ion transport. When paired with a single‐crystal ultrahigh‑nickel cathode LiNi 0.94 Co 0.05 Mn 0.01 O 2 (Ni94), the surface‑softened LIC (S‑LIC) enables ASSLBs delivering specific capacities of 223.8 and 209.5 mAh g −1 at 2 C and 4 C, respectively, retaining over 85% of the initial capacity after 2000 cycles at 2 C, and operate stably for more than 9000 cycles at 10 C. Even under an ultrahigh cutoff voltage of 4.8 V, a capacity retention of 81% is achieved after 800 cycles at 2 C. This work provides a broadly applicable and efficient interfacial engineering route for high‑voltage halide‑based ASSLBs.
- 30 October 2026
- Published by Wiley in Advanced Energy Materials
- p. e71780
Open AccessConstructing an Adaptive Flexible Interphase on Halide Electrolytes by Lewis‐Acid‐Induced Polymerization for High‐Voltage All‐Solid‐State Lithium Batteries
All‐solid‐state lithium batteries (ASSLBs) combining halide solid electrolytes (HSEs) with high‐nickel layered oxide cathodes offer great promise for high energy density, yet they suffer from severe interfacial issues such as oxidative decomposition, mechanical degradation, and chemical incompatibility with sulfide electrolytes. Herein, we report a Lewis‐acid‐induced surface‐softening strategy that constructs a nanoscale adaptive flexible interphase (AFI) via in situ polymerization of acrylonitrile (AN) on a representative halide electrolyte, Li 3 InCl 6 (LIC). The resulting AFI layer concurrently provides ionic conductivity, excellent oxidation stability (>4.8 V), and favorable viscoelasticity, thereby synergistically enhancing the electrochemical, chemical, and mechanical stability of the interface without compromising bulk ion transport. When paired with a single‐crystal ultrahigh‑nickel cathode LiNi 0.94 Co 0.05 Mn 0.01 O 2 (Ni94), the surface‑softened LIC (S‑LIC) enables ASSLBs delivering specific capacities of 223.8 and 209.5 mAh g −1 at 2 C and 4 C, respectively, retaining over 85% of the initial capacity after 2000 cycles at 2 C, and operate stably for more than 9000 cycles at 10 C. Even under an ultrahigh cutoff voltage of 4.8 V, a capacity retention of 81% is achieved after 800 cycles at 2 C. This work provides a broadly applicable and efficient interfacial engineering route for high‑voltage halide‑based ASSLBs.