Viacheslav Stolbovyi
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Viacheslav Stolbovyi has a total of 10 co-authors. Here are the top co-authors by number of shared publications:
- Alexander Timoshenko
Institute of Plasma Physics, Kharkiv Institute of Physics and Technology, Kharkiv, Ukraine, Ukraine
1 shared publication - Andrey Manokhin
Bakul Institute for Superhard Materials, National Academy of Sciences of Ukraine, Kyiv, Ukraine
1 shared publication - Anton Taran
Kharkov Inst Phys & Technol, Inst Plasma Phys NSC, Kharkiv, Ukraine
1 shared publication - Bohdan N. Mordyuk
G.V. Kurdyumov Institute for Metal Physics of the NAS of Ukraine, 36 Academician Vernadsky Boulevard, 03142 Kyiv, Ukraine
1 shared publication - Igor Garkusha
Institute of Plasma Physics, Kharkiv Institute of Physics and Technology, Kharkiv, Ukraine, Ukraine
1 shared publication - Islam M. Zakiev
State University "Kyiv Aviation Institute", Kyiv, Ukraine, Ukraine
1 shared publication
Latest Publications
- Open Access
- 25 November 2026
- Published by MDPI AG in Preprints.org
Microstructure–Property Relationships for Zirconia and Titania PVD Coatings on AISI 430 Steel: A Comparative Study of Microtribological Behaviour
Oxide coatings, including titanium dioxide and zirconium dioxide, are widely used to protect metals and polymers in industrial, architectural, environmental, aerospace, and biomedical applications. This study compares the surface topography, microstructure, and phase composition of reactive PVD ZrO₂ and TiO₂ coatings and correlates these with their microtribological properties. Hardness and wear/friction behaviour were analysed using nanoindentation, scratch tests, and dry microtribological sliding tests on an indentation tester equipped with a precision rotational stage. X-ray diffraction (XRD) analysis, white light interferometry (WLI), scanning electron microscopy (SEM), and energy-dispersive spectroscopy (EDS) show the peculiarities in the microstructure and phase composition of both nanocrystalline coatings (with grain sizes of ~26 nm and ~11 nm for ZrO₂ and TiO2, respectively). Despite the slightly lower hardness of ZrO₂ (12.57 GPa) in comparison with that of TiO2 (13.88 GPa), the volumetric wear rate is on the order of magnitude lower for the zirconia coating (1.5×105 μm3/m) than that of the titanium dioxide coating (2.2×106 μm3/m). This finding correlates well with the wear track morphology observed by interference profilometry and SEM. Wear mechanisms are discussed in relation to the phase compositions of the studied coatings. As observed, both coatings underwent stress-induced tetragonal to monoclinic phase transformations due to a high enough Hertzian contact pressure (6.6–6.7 GPa) applied at indentation and wear tests. However, the TRIP effect related to the phase transformation in the ZrO2 coating seems to be beneficial for wear resistance enhancement owing to acquired localised ductility and clamping down on crack propagation, while the increased phase misfit and microstresses accumulated in the TiO2 coating resulted in its early brittle fracture and further abrasive wear.
- 25 November 2026
- Published by MDPI AG in Preprints.org
Open AccessMicrostructure–Property Relationships for Zirconia and Titania PVD Coatings on AISI 430 Steel: A Comparative Study of Microtribological Behaviour
Oxide coatings, including titanium dioxide and zirconium dioxide, are widely used to protect metals and polymers in industrial, architectural, environmental, aerospace, and biomedical applications. This study compares the surface topography, microstructure, and phase composition of reactive PVD ZrO₂ and TiO₂ coatings and correlates these with their microtribological properties. Hardness and wear/friction behaviour were analysed using nanoindentation, scratch tests, and dry microtribological sliding tests on an indentation tester equipped with a precision rotational stage. X-ray diffraction (XRD) analysis, white light interferometry (WLI), scanning electron microscopy (SEM), and energy-dispersive spectroscopy (EDS) show the peculiarities in the microstructure and phase composition of both nanocrystalline coatings (with grain sizes of ~26 nm and ~11 nm for ZrO₂ and TiO2, respectively). Despite the slightly lower hardness of ZrO₂ (12.57 GPa) in comparison with that of TiO2 (13.88 GPa), the volumetric wear rate is on the order of magnitude lower for the zirconia coating (1.5×105 μm3/m) than that of the titanium dioxide coating (2.2×106 μm3/m). This finding correlates well with the wear track morphology observed by interference profilometry and SEM. Wear mechanisms are discussed in relation to the phase compositions of the studied coatings. As observed, both coatings underwent stress-induced tetragonal to monoclinic phase transformations due to a high enough Hertzian contact pressure (6.6–6.7 GPa) applied at indentation and wear tests. However, the TRIP effect related to the phase transformation in the ZrO2 coating seems to be beneficial for wear resistance enhancement owing to acquired localised ductility and clamping down on crack propagation, while the increased phase misfit and microstresses accumulated in the TiO2 coating resulted in its early brittle fracture and further abrasive wear.