Effects of Oxidized Metal Powders on Pore Defects in Powder-Fed Direct Energy Deposition
Open Access
- 6 February 2024
- journal article
- research article
- Published by MDPI AG in Micromachines
- Vol. 15 (2) , 243
Abstract
Laser-based additive manufacturing processes, particularly direct energy deposition (DED), have gained prominence for fabricating complex, functionally graded, or customized parts. DED employs a high-powered heat source to melt metallic powder or wire, enabling precise control of grain structures and the production of high-strength objects. However, common defects, such as a lack of fusion and pores between layers or beads, can compromise the mechanical properties of the printed components. This study focuses on investigating the recurrent causes of pore defects in the powder-fed DED process, with a specific emphasis on the influence of oxidized metal powders. This research explores the impact of intentionally oxidizing metal powders of hot work tool steel H13 by exposing them to regulated humidity and temperature conditions. Scanning electron microscopy images and energy-dispersive X-ray spectroscopy results demonstrate the clumping of powders and the deposition of iron oxides in the oxidized powders at elevated temperatures (70 °C for 72 h). Multi-layered depositions of the oxidized H13 powders on STD61 substrate do not show significant differences in cross sections among specimens, suggesting that oxidation does not visibly form large pores. However, fine pores, detected through CT scanning, are observed in depositions of oxidized powders at higher temperatures. These fine pores, typically less than 250 µm in diameter, are irregularly distributed throughout the deposition, indicating a potential degradation in mechanical properties. The findings highlight the need for careful consideration of oxidation effects in optimizing process parameters for enhanced additive manufacturing quality.Keywords
Funding Information
- Korea Evaluation Institute of Industrial Technology (K-G012000875302, KITECH JA-24-0001)
- Korea Institute of Industrial Technology (K-G012000875302, KITECH JA-24-0001)
This publication has 27 references indexed in Scilit:
- In-situ crack and keyhole pore detection in laser directed energy deposition through acoustic signal and deep learningAdditive Manufacturing, 2023
- Investigation of pore formation mechanisms induced by spherical-powder delivery in directed energy deposition using in situ high-speed X-ray imagingAdditive Manufacturing Letters, 2022
- A fatigue life prediction approach for laser-directed energy deposition titanium alloys by using support vector regression based on pore-induced failuresInternational Journal of Fatigue, 2022
- Investigation of surface modifications for combating the molten aluminum corrosion of AISI H13 steelCorrosion Science, 2020
- The effect of powder oxidation on defect formation in laser additive manufacturingActa Materialia, 2019
- An overview of Direct Laser Deposition for additive manufacturing; Part II: Mechanical behavior, process parameter optimization and controlAdditive Manufacturing, 2015
- An overview of Direct Laser Deposition for additive manufacturing; Part I: Transport phenomena, modeling and diagnosticsAdditive Manufacturing, 2015
- Mitigation of pores generation at overlapping zone during laser claddingJournal of Materials Processing Technology, 2015
- Repairing of sintered tools using laser cladding by wireJournal of Materials Processing Technology, 2005
- Characteristics of laser aided direct metal/material deposition process for tool steelInternational Journal of Machine Tools and Manufacture, 2005