Joining of SiO2f/SiO2 composite to Ti-6Al-4V using Ag-Cu-In-Ti brazing fillers, the joint strengths, and microstructures
Authors:
- 21 March 2017
- journal article
- research article
- Published by Springer Nature in Welding in the World
- Vol. 61 (4) , 833-837
Abstract
No abstract availableKeywords
Funding Information
- National Natural Science Foundation of China (5990522, 50475160)
This publication has 8 references indexed in Scilit:
- Joining of Cf/SiC Composite With Pd-Co-V Brazing FillerWelding in the World, 2012
- Influence of Ti on the Mechanical Properties of AgCuInTi Active Brazing FillersAdvanced Engineering Materials, 2009
- Vacuum brazing of SiO2 glass ceramic and Ti–6Al–4V alloy using AgCuTi filler foilMaterials Science and Engineering: A, 2008
- Processing and properties of unidirectional SiO2f/SiO2 compositesCeramics International, 2007
- Wettability of Co–V, and PdNi–Cr–V system alloys on SiC ceramic and interfacial reactionsScripta Materialia, 2007
- The Preparation and Characterization of 3D-Silica Fiber Reinforced Silica CompositesKey Engineering Materials, 2003
- Joining of AlN ceramic to metals using sputtered Al or Ti filmJournal of Materials Processing Technology, 2001
- Fundamentals of Residual Stresses in Joints Between Dissimilar MaterialsMRS Bulletin, 1995