ELECTRICAL WIRE PRODUCTION FROM Al - Ce - La ALLOY RODS AFTER ELECTROMAGNETIC MOLD AND COMBINED ROLLING ‑ EXTRUSION
Authors:
- Denis VoroshilovDVDenis Voroshilov
- Sergey SidelnikovSSSergey Sidelnikov
- Dorzhizhab DarmazhapovDDDorzhizhab Darmazhapov
- Vadim BespalovVBVadim Bespalov
- Alexander DurnopyanovADAlexander Durnopyanov
- Viktor BerngardtVBViktor Berngardt
- Sergey LezhnevSLSergey Lezhnev
- Mikhail MotkovMMMikhail Motkov
- Marina VoroshilovaMVMarina Voroshilova
Open Access
- 7 March 2025
- journal article
- Published by University of Chemical Technology and Metallurgy in Journal of Chemical Technology and Metallurgy
- Vol. 60 (2) , 327-336
Abstract
The paper presents the results of the power parameters when producing rods and wires with Ø 2 mm from them and the mechanical and electrical properties of the resulting semi - finished products from an alloy of the Al - Ce - La system with a rare earth metal content of 1 %. The wire is produced using the method of combined rolling-extrusion (CRE) from the billet Ø 12 mm after electromagnetic mold (EMM), and further drawing. The results of experimental studies of the process of producing longish deformed semi-finished products from the Al - 1 % REM alloy using the CRE-200 combined processing unit are presented. Data were obtained on the mechanical properties of hot - extruded rods Ø 5 mm and Ø 9 mm, as well as wire Ø 2 mm obtained from these rods after implementing the combined processes of rolling - extrusion. It was found that the proposed processing modes make it possible to obtain rods with Ø 9 mm and Ø 5 mm using a combined rolling - extrusion method from workpieces after EMM with diameter 12 mm. The forces on the rolls and die were measured during the implementation of the investigated combined processes. The plasticity of the resulting rods Ø 5 and 9 mm after the CRE method was quite high (elongation to failure reached 14 - 26 %). When drawing wire up to Ø 2 mm, no intermediate annealing was required. The values of electrical resistance do not exceed 0.0271 Ω mm2 m-1 for rods and from 0.0301 Ω mm2 m-1 for wire with a diameter of 2 mm, depending on the processing modes. At all stages of the experimental studies, the structure of the metal was studied and the patterns of change in physical and mechanical properties depending on the processing modes were established.Keywords
This publication has 18 references indexed in Scilit:
- Combined rolling-extrusion of various billets from the Al–Ce–La alloy for electrical wire productionThe International Journal of Advanced Manufacturing Technology, 2024
- Cerium in aluminum alloysJournal of Materials Science, 2019
- Effect of Ce addition on the microstructure and properties of Al-Cu-Mn-Mg-Fe lithium battery shell alloyMaterials Characterization, 2018
- The Effect of Addition of Ce and Sr on the Solidification Path of Al–8Si–2Cu AlloyTransactions of the Indian Institute of Metals, 2015
- Effects of La addition on the microstructure and tensile properties of Al-Si-Cu-Mg casting alloysInternational Journal of Minerals, Metallurgy and Materials, 2015
- The improved effects by the combinative addition of lanthanum and samarium on the microstructures and the tensile properties of high-pressure die-cast Mg–4Al-based alloyMaterials Science and Engineering: A, 2015
- Effects of rare earth elements addition on microstructures, tensile properties and fractography of A357 alloyMaterials Science and Engineering: A, 2014
- Effect of trace La addition on the microstructure and mechanical property of as-cast ADC12 Al-AlloyJournal of Wuhan University of Technology-Mater. Sci. Ed., 2013
- Effects of La addition on the elevated temperature properties of the casting Al–Cu alloyMaterials Science and Engineering: A, 2011
- Effect of trace La addition on the microstructures and mechanical properties of A356 (Al–7Si–0.35Mg) aluminum alloysJournal of Alloys and Compounds, 2009