Mikhail M. Motkov
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Mikhail M. Motkov has a total of 29 co-authors. Here are the top co-authors by number of shared publications:
- Andrey Evgenievich Medvedev
Laboratory of Metals and Alloys Under Extreme Impacts, Ufa University of Science and Technology, Ufa, Russia
3 shared publications - Maxim Yurievich Murashkin
Ufa University of Science and Technology, Ufa, Russia
3 shared publications - Olga O. Zhukova
Ufa University of Science and Technology, Ufa, Russia
3 shared publications - A. F. Shaikhulova
Ufa University of Science and Technology, Ufa, Russia
2 shared publications - Nikolay A. Belov
National University of Science and Technology MISiS
2 shared publications - Виктор Николаевич Тимофеев
Department of Electrical Engineering, Siberian Federal University, 79 Svobodnyy Prospekt, 660041 Krasnoyarsk, Russia
2 shared publications
Latest Publications
- 1 February 2026
- Published by Pleiades Publishing Ltd in Russian Journal of Non-Ferrous Metals
- Vol. 67 (1) , 1-12
The Influence of Production Technology and Subsequent Deformation Treatment on the Microstructure and Properties of the Al–0.5Fe Alloy
Two alloys with similar chemical composition—Al–0.5 wt % Fe were produced via two different production technology being casting into electromagnetic mold (EMC) and continuous casting and rolling (CCR), respectively. Production methods provided different cooling rates resulting in different structure formation and sets of properties, such as mechanical strength, elongation to failure and electrical conductivity. Samples of the alloys were subjected to the combination of the equal-channel angular pressing by the “Conform” scheme and cold drawing (ECAP-С + CD), as well as cold drawing (CD) only. It was demonstrated that the difference in production process provided distinct structural states, mainly different in size and distribution of the intermetallic particles. Differences in the morphology of the intermetallic particles notably affected the physical and mechanical properties of the alloys, mainly electrical conductivity. Thermal stability of the alloys, measured according to the international standard for thermal-resistant aluminium alloy wire for overhead line conductor, differs as well, depending on the particle morphology—EMC alloy retains 94–98% of its ultimate tensile strength after annealing, while CCR alloy only 60–83%.
- 1 February 2026
- Published by Pleiades Publishing Ltd in Russian Journal of Non-Ferrous Metals
- Vol. 67 (1) , 1-12
The Influence of Production Technology and Subsequent Deformation Treatment on the Microstructure and Properties of the Al–0.5Fe Alloy
Two alloys with similar chemical composition—Al–0.5 wt % Fe were produced via two different production technology being casting into electromagnetic mold (EMC) and continuous casting and rolling (CCR), respectively. Production methods provided different cooling rates resulting in different structure formation and sets of properties, such as mechanical strength, elongation to failure and electrical conductivity. Samples of the alloys were subjected to the combination of the equal-channel angular pressing by the “Conform” scheme and cold drawing (ECAP-С + CD), as well as cold drawing (CD) only. It was demonstrated that the difference in production process provided distinct structural states, mainly different in size and distribution of the intermetallic particles. Differences in the morphology of the intermetallic particles notably affected the physical and mechanical properties of the alloys, mainly electrical conductivity. Thermal stability of the alloys, measured according to the international standard for thermal-resistant aluminium alloy wire for overhead line conductor, differs as well, depending on the particle morphology—EMC alloy retains 94–98% of its ultimate tensile strength after annealing, while CCR alloy only 60–83%.
- 1 December 2025
- Published by Pleiades Publishing Ltd in Russian Journal of Non-Ferrous Metals
- Vol. 66 (6) , 381-392
Improving the Complex of Properties of Copper-Clad Aluminum Wire by Using Electromagnetically Cast Al–Fe Alloys
This work is dedicated to the analysis of the influence of the core material on the complex of physical and mechanical properties of copper-clad aluminum wires (CCAW) in hard (hard-drawn) and soft (annealed) states. Low-alloyed aluminium alloys of the Al–Fe system were chosen as research material as an alternative to the conventionally used technically pure aluminium in terms of thermal stability, mechanical strength and ductility. Such alloys, while still retaining low cost and high electrical conductivity, are characterized by the improved relative to technically pure Al mechanical strength and thermal stability. Alloys used in this study were produced by casting into electromagnetic mold to further improve their mechanical properties. Three different alloy compositions Al–0.5 wt % Fe, Al–0.5 wt % Fe–0.3 wt % Cu and Al–1.7 wt % Fe were used. To achieve a hard-drawn state, the copper-clad wire was cold-drawn to a reduction degree of 90%, and the soft state was achieved by annealing at 300 and 325°C for 1 h. To compare CCAW with the core materials produced by electromagnetic casting, samples with similar copper content were produced based on commercial alloy 8176, produced by a traditional combined casting and rolling method. Based on the experimental data obtained and the results of the optimization performed (from the combined tensile strength, ductility and electrical conductivity point of view) using the linear convolution target function, the most suitable alloy of the Al–Fe system as the core material for the CCAW was proposed.
- 1 December 2025
- Published by Pleiades Publishing Ltd in Russian Journal of Non-Ferrous Metals
- Vol. 66 (6) , 381-392
Improving the Complex of Properties of Copper-Clad Aluminum Wire by Using Electromagnetically Cast Al–Fe Alloys
This work is dedicated to the analysis of the influence of the core material on the complex of physical and mechanical properties of copper-clad aluminum wires (CCAW) in hard (hard-drawn) and soft (annealed) states. Low-alloyed aluminium alloys of the Al–Fe system were chosen as research material as an alternative to the conventionally used technically pure aluminium in terms of thermal stability, mechanical strength and ductility. Such alloys, while still retaining low cost and high electrical conductivity, are characterized by the improved relative to technically pure Al mechanical strength and thermal stability. Alloys used in this study were produced by casting into electromagnetic mold to further improve their mechanical properties. Three different alloy compositions Al–0.5 wt % Fe, Al–0.5 wt % Fe–0.3 wt % Cu and Al–1.7 wt % Fe were used. To achieve a hard-drawn state, the copper-clad wire was cold-drawn to a reduction degree of 90%, and the soft state was achieved by annealing at 300 and 325°C for 1 h. To compare CCAW with the core materials produced by electromagnetic casting, samples with similar copper content were produced based on commercial alloy 8176, produced by a traditional combined casting and rolling method. Based on the experimental data obtained and the results of the optimization performed (from the combined tensile strength, ductility and electrical conductivity point of view) using the linear convolution target function, the most suitable alloy of the Al–Fe system as the core material for the CCAW was proposed.
- Open Access
- 7 March 2025
- Published by University of Chemical Technology and Metallurgy in Journal of Chemical Technology and Metallurgy
- Vol. 60 (2) , 327-336
ELECTRICAL WIRE PRODUCTION FROM Al - Ce - La ALLOY RODS AFTER ELECTROMAGNETIC MOLD AND COMBINED ROLLING ‑ EXTRUSION
The paper presents the results of the power parameters when producing rods and wires with Ø 2 mm from them and the mechanical and electrical properties of the resulting semi - finished products from an alloy of the Al - Ce - La system with a rare earth metal content of 1 %. The wire is produced using the method of combined rolling-extrusion (CRE) from the billet Ø 12 mm after electromagnetic mold (EMM), and further drawing. The results of experimental studies of the process of producing longish deformed semi-finished products from the Al - 1 % REM alloy using the CRE-200 combined processing unit are presented. Data were obtained on the mechanical properties of hot - extruded rods Ø 5 mm and Ø 9 mm, as well as wire Ø 2 mm obtained from these rods after implementing the combined processes of rolling - extrusion. It was found that the proposed processing modes make it possible to obtain rods with Ø 9 mm and Ø 5 mm using a combined rolling - extrusion method from workpieces after EMM with diameter 12 mm. The forces on the rolls and die were measured during the implementation of the investigated combined processes. The plasticity of the resulting rods Ø 5 and 9 mm after the CRE method was quite high (elongation to failure reached 14 - 26 %). When drawing wire up to Ø 2 mm, no intermediate annealing was required. The values of electrical resistance do not exceed 0.0271 Ω mm2 m-1 for rods and from 0.0301 Ω mm2 m-1 for wire with a diameter of 2 mm, depending on the processing modes. At all stages of the experimental studies, the structure of the metal was studied and the patterns of change in physical and mechanical properties depending on the processing modes were established.
- 7 March 2025
- Published by University of Chemical Technology and Metallurgy in Journal of Chemical Technology and Metallurgy
- Vol. 60 (2) , 327-336
Open AccessELECTRICAL WIRE PRODUCTION FROM Al - Ce - La ALLOY RODS AFTER ELECTROMAGNETIC MOLD AND COMBINED ROLLING ‑ EXTRUSION
The paper presents the results of the power parameters when producing rods and wires with Ø 2 mm from them and the mechanical and electrical properties of the resulting semi - finished products from an alloy of the Al - Ce - La system with a rare earth metal content of 1 %. The wire is produced using the method of combined rolling-extrusion (CRE) from the billet Ø 12 mm after electromagnetic mold (EMM), and further drawing. The results of experimental studies of the process of producing longish deformed semi-finished products from the Al - 1 % REM alloy using the CRE-200 combined processing unit are presented. Data were obtained on the mechanical properties of hot - extruded rods Ø 5 mm and Ø 9 mm, as well as wire Ø 2 mm obtained from these rods after implementing the combined processes of rolling - extrusion. It was found that the proposed processing modes make it possible to obtain rods with Ø 9 mm and Ø 5 mm using a combined rolling - extrusion method from workpieces after EMM with diameter 12 mm. The forces on the rolls and die were measured during the implementation of the investigated combined processes. The plasticity of the resulting rods Ø 5 and 9 mm after the CRE method was quite high (elongation to failure reached 14 - 26 %). When drawing wire up to Ø 2 mm, no intermediate annealing was required. The values of electrical resistance do not exceed 0.0271 Ω mm2 m-1 for rods and from 0.0301 Ω mm2 m-1 for wire with a diameter of 2 mm, depending on the processing modes. At all stages of the experimental studies, the structure of the metal was studied and the patterns of change in physical and mechanical properties depending on the processing modes were established.
- Open Access
- 1 January 2025
- Published by Togliatti State University in Frontier materials & technologies
- No. 2,p. 29-38
Ductility, bending and wrapping ability relationship in wires made of electromagnetically cast ultrafine grained Al–0.5Fe and Al–0.5Fe–0.3Cu alloys
The research status on such functional properties, as bending capability, wrapping capability and ductility of conductive Al–Fe and Al–Fe–Cu alloys wires is uncertain. Bending and wrapping capability is determined by the industrial standards while no attempts were made to study the relation between them and ductility of the Al alloys wires, paying even less attention to the ultrafine-grained Al-based wires, produced by electromagnetic casting and equal-channel angular pressing. In this study alloys with two different chemical compositions (Al–0.5 wt. % Fe and Al–0.5 wt. % Fe–0.3 wt. % Cu) and two different casting methods (casting into electromagnetic mold and continuous casting and rolling) were used. Part of the wires for the study was prepared by cold drawing (CD), the other part – by the combination of the equal-channel angular pressing by the Conform scheme and cold drawing (ECAP-C+CD) to obtain coarse grained (CG) and ultrafine grained (UFG) structures, respectively. Annealing at 230 °C for 1 h was carried out to evaluate the thermal stability of the wires. It was shown that the correlation between ductility (elongation to failure), number of wraps and number of bends (both before the first crack and before complete failure of the specimen) may differ depending on the deformation value, deformation scheme, and amount of alloying elements of the alloy wire, as well as ability to form solid solutions.
- 1 January 2025
- Published by Togliatti State University in Frontier materials & technologies
- No. 2,p. 29-38
Open AccessDuctility, bending and wrapping ability relationship in wires made of electromagnetically cast ultrafine grained Al–0.5Fe and Al–0.5Fe–0.3Cu alloys
The research status on such functional properties, as bending capability, wrapping capability and ductility of conductive Al–Fe and Al–Fe–Cu alloys wires is uncertain. Bending and wrapping capability is determined by the industrial standards while no attempts were made to study the relation between them and ductility of the Al alloys wires, paying even less attention to the ultrafine-grained Al-based wires, produced by electromagnetic casting and equal-channel angular pressing. In this study alloys with two different chemical compositions (Al–0.5 wt. % Fe and Al–0.5 wt. % Fe–0.3 wt. % Cu) and two different casting methods (casting into electromagnetic mold and continuous casting and rolling) were used. Part of the wires for the study was prepared by cold drawing (CD), the other part – by the combination of the equal-channel angular pressing by the Conform scheme and cold drawing (ECAP-C+CD) to obtain coarse grained (CG) and ultrafine grained (UFG) structures, respectively. Annealing at 230 °C for 1 h was carried out to evaluate the thermal stability of the wires. It was shown that the correlation between ductility (elongation to failure), number of wraps and number of bends (both before the first crack and before complete failure of the specimen) may differ depending on the deformation value, deformation scheme, and amount of alloying elements of the alloy wire, as well as ability to form solid solutions.
- 22 July 2023
- Published by Springer Nature in Metallurgist
- Vol. 67 (3-4) , 362-379
Multi-Disciplinary Numerical Analysis of Aluminum Ingot Electromagnetic Casting
- 22 July 2023
- Published by Springer Nature in Metallurgist
- Vol. 67 (3-4) , 362-379
Multi-Disciplinary Numerical Analysis of Aluminum Ingot Electromagnetic Casting
- Open Access
Effect of Radial-Shear Rolling on the Structure and Hardening of an Al–8%Zn–3.3%Mg–0.8%Ca–1.1%Fe Alloy Manufactured by Electromagnetic Casting
Aluminum alloys are one of the most common structural materials. To improve the mechanical properties, an alloy of the Al–Zn–Mg–Ca–Fe system was proposed. In this alloy, when Fe and Ca are added, compact particles of the Al10CaFe2 compound are formed, which significantly reduces the negative effect of Fe on the mechanical properties. Because of the high solidification rate (about 600 K/s) during cylindrical ingot (~33 mm) production, the electromagnetic casting method (ECM) makes it possible to obtain a highly dispersed structure in the cast state. The size of the dendritic cell is ~7 μm, while the entire amount of Fe is bound into eutectic inclusions of the Al10CaFe2 phase with an average size of less than 3 μm. In this study, the effect of radial shear rolling (RSR) on the formation of the structure and hardening of the Al–8%Zn–3.3%Mg–0.8%Ca–1.1%Fe alloy obtained by EMC was studied. Computer simulation of the RSR process made it possible to analyze the temperature and stress–strain state of the alloy and to select the optimal rolling modes. It was shown that the flow features during RSR and the severe shear strains near the surface of the rod (10 mm) provided a refining and decrease in the size of the initial Fe-containing particles.
Open AccessEffect of Radial-Shear Rolling on the Structure and Hardening of an Al–8%Zn–3.3%Mg–0.8%Ca–1.1%Fe Alloy Manufactured by Electromagnetic Casting
Aluminum alloys are one of the most common structural materials. To improve the mechanical properties, an alloy of the Al–Zn–Mg–Ca–Fe system was proposed. In this alloy, when Fe and Ca are added, compact particles of the Al10CaFe2 compound are formed, which significantly reduces the negative effect of Fe on the mechanical properties. Because of the high solidification rate (about 600 K/s) during cylindrical ingot (~33 mm) production, the electromagnetic casting method (ECM) makes it possible to obtain a highly dispersed structure in the cast state. The size of the dendritic cell is ~7 μm, while the entire amount of Fe is bound into eutectic inclusions of the Al10CaFe2 phase with an average size of less than 3 μm. In this study, the effect of radial shear rolling (RSR) on the formation of the structure and hardening of the Al–8%Zn–3.3%Mg–0.8%Ca–1.1%Fe alloy obtained by EMC was studied. Computer simulation of the RSR process made it possible to analyze the temperature and stress–strain state of the alloy and to select the optimal rolling modes. It was shown that the flow features during RSR and the severe shear strains near the surface of the rod (10 mm) provided a refining and decrease in the size of the initial Fe-containing particles.