Temperature Increase Beneath Etched Dentin Discs During Composite Polymerization
- 1 January 2011
- journal article
- research article
- Published by SAGE Publications in Photomedicine and Laser Surgery
- Vol. 29 (1) , 47-52
Abstract
Objective: The purpose of this in vitro study was to measure the temperature increase during the polymerization of a composite resin beneath acid-etched or laser-etched dentin discs. Background Data: The irradiation of dentin with an Er:YAG laser may have a positive effect on the thermal conductivity of dentin. This technique has not been studied extensively. Materials and Methods: Forty dentin discs (5 mm in diameter and 0.5 or 1 mm in height) were prepared from extracted permanent third molars. These dentin discs were etched with 20% orthophosphoric acid or an Er:YAG laser, and were then placed on an apparatus developed to measure temperature increases. The composite resin was polymerized with a high-intensity quartz tungsten halogen (HQTH) or light-emitting diode unit (LED). The temperature increase was measured under the dentin disc with a J-type thermocouple wire that was connected to a data logger. Five measurements were made for each dentin disc, curing unit, and etching system combination. Differences between the initial and the highest temperature readings were taken, and the five calculated temperature changes were averaged to determine the value of the temperature increase. Statistical analysis was performed with a three-way ANOVA and Tukey HSD tests at a 0.05 level of significance. Further SEM examinations were performed. Results: The temperature increase values varied significantly, depending on etching systems ( p < 0.05), dentin thicknesses ( p < 0.05), and curing units ( p < 0.05). Temperature increases measured beneath laser-etched discs were significantly higher than those for acid-etched dentin discs ( p < 0.05). The HQTH unit induced significantly higher temperature increases than the LED unit ( p < 0.05). The LED unit induced the lowest temperature change (5.2°C) in the 1-mm, acid-etched dentin group. The HQTH unit induced the highest temperature change (10.4°C) for the 0.5-mm, laser-etched dentin group. Conclusion: The risk of heat-induced pulpal damage should be taken into consideration during the polymerization of composite resin after laser etching when the dentin thickness is less than 0.5 mm.Keywords
This publication has 28 references indexed in Scilit:
- Influence of heat from light curing units and dental composite polymerization on cells in vitroJournal of Dentistry, 2006
- Mechanisms of Pulsed Laser Ablation of Biological TissuesChemical Reviews, 2003
- Pulpal Heat Changes With Newly Developed Resin Photopolymerisation SystemsAustralian Endodontic Journal, 2002
- Shear Strength of Composite Bonded to Er:YAG Laser-prepared DentinJournal of Dental Research, 1996
- Thermographic measurement of temperature change during resin composite polymerization in vivoJournal of Dentistry, 1995
- Measurement of temperature generated by visible-light-cure lamps in an in vitro modelDental Materials, 1989
- Experimental studies of the application of the Er:YAG laser on dental hard substances: I. Measurement of the ablation rateLasers in Surgery and Medicine, 1989
- Temperature rises produced by light sources and composites during curingDental Materials, 1986
- The promotion of adhesion by the infiltration of monomers into tooth substratesJournal of Biomedical Materials Research, 1982
- A Simple Method of Increasing the Adhesion of Acrylic Filling Materials to Enamel SurfacesJournal of Dental Research, 1955