Effect of a polymerization inhibitor on the chemomechanical properties and consistency of experimental resin composites
Authors:
- Caio Vinícius Signorelli GrohmannCGCaio Vinícius Signorelli Grohmann
- Mário Alexandre Coelho SinhoretiMSMário Alexandre Coelho Sinhoreti
- Eveline Freitas SoaresESEveline Freitas Soares
- Robson Ferraz de OliveiraRORobson Ferraz de Oliveira
- Eduardo José de Carvalho Souza-JúniorESEduardo José de Carvalho Souza-Júnior
- Saulo GeraldeliSGSaulo Geraldeli
Open Access
- 29 June 2022
- journal article
- research article
- Published by FapUNIFESP (SciELO) in Brazilian Dental Journal
- Vol. 33 (3) , 92-98
Abstract
This study investigated the effect of butylated hydroxytoluene (BHT) inhibitor on degree of conversion (DC), flexural strength (FS), flexural modulus (FM), Knoop microhardness (KH), microhardness reduction (HR), and consistency of experimental resin composites at different BHT concentrations: C0 (control-0%); C0.01 (0.01%); C0.025 (0.025%); C0.05 (0.05%); C0.1 (0.1%); and C0.5 (0.5%). For the consistency, the composites were tested immediately after being exposed to a dental chair headlight (0, 20, 40 and 60 s). Data concerning DC, FS, FM, KH, and HR were submitted to one-way ANOVA, while the consistency data was submitted to 2-way ANOVA; mean values were then compared (Tukey’s test; α=0.05). The KH, FS and FM analyses showed no significant difference among the composites tested. For DC, C0 showed the highest mean value (74.2%) and differed only from C0.5 (67.2%). For HR, C0.5 showed the lowest mean (13.09%) value and differed from C0 (26.4%) and C0.01 (24.87). The consistency analysis showed no difference among C0.05, C0.1 and C0.5, considering 0 and 20 s of light exposure, while C0 (14.07 mm), C0.01 (13.97 mm), and C0.025 (14.18 mm) showed higher mean values at 0 s when compared to 20 s (12.67, 12.77 and 13.05 mm, respectivelly). Polymerization occurred within 40 s of light exposure for C0, C0.01, C0.025, and C0.05 and within 60 s for C0.1. In conclusion, the BHT concentrations had no significant influence on FS, FM and KH. The higher the BHT concentration, the longer was its handling time under light, with a significant improvement in the HR, but a decrease in DC. Therefore, BHT at 0.1% showed the best outcomes concerning all the BHT concentrations tested.Keywords
This publication has 24 references indexed in Scilit:
- Optimizing light-cured composite through variations in camphorquinone and butylhydroxytoluene concentrationsBrazilian Oral Research, 2016
- Mapping camphorquinone consumption, conversion and mechanical properties in methacrylates with systematically varied CQ/amine compositionsDental Materials, 2014
- Controlling the kinetic chain length of the crosslinks in photo-polymerized biodegradable networksJournal of Materials Science: Materials in Medicine, 2013
- The Effect of Inhibitor Concentrations on the Chemical and Mechanical Properties of Bis-GMA-Based Resin Dental CompositesJournal of Materials Science Research, 2013
- Competitive light absorbers in photoactive dental resin-based materialsDental Materials, 2012
- Effect of different photo-activation methods on push out force, hardness and cross-link density of resin composite restorationsDental Materials, 2008
- Cross-link density evaluation through softening tests: Effect of ethanol concentrationDental Materials, 2008
- Contraction stress related to degree of conversion and reaction kinetics.2002
- Primary cyclization in the polymerization of bis-GMA and TEGDMA: a modeling approach to understanding the cure of dental resinsDental Materials, 2001
- The effect of resin formulation on the degree of conversion and mechanical properties of dental restorative resinsJournal of Biomedical Materials Research, 1986