Aging Behavior of x Pb(Fe 2/3 W 1/3 )O 3 · (1 – x )Pb(Fe 1/2 Nb 1/2 )O 3 Ceramic

Authors:

Abstract
The aging behavior of a series of lead perovskite dielectrics with the compositions x Pb(Fe 2/3 W 1/3 )O 3 ·(1 – x )Pb(Fe 1/2 ‐Nb 1/2 )O 3 , where 0 ≤ x ≤ 1, and the effect of dopants were studied. Below the Curie temperature ( T c ), the capacitance and the dissipation factor (tan δ) decrease approximately linearly with logarithmic time. The aging rate depends on the temperature difference, Δ T , between the aging temperature and T c , and on the dopant concentration, but is independent of the measurement frequency between 1 and 1000 kHz. The maximum aging rate is about 3% per decade of time for capacitance and 5% per decade for tan δ at 1 mol% dopant concentration, and increases to 6.3% for capacitance and 8.5% for tan δ at 0.7 mol% dopant concentration. These results are consistent with an aging mechanism caused by changing ferroelectric domain structure with time, as proposed for BaTiO 3 .