Man F. Yan
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Man F. Yan has a total of 5 co-authors. Here are the top co-authors by number of shared publications:
Chen Wang
State Key Laboratory of Materials-Oriented Chemical Engineering Nanjing Tech University Nanjing China
1 shared publicationHung C. Ling
AT&T Bell Laboratories, Princeton, New Jersey 08540
1 shared publication- Min Deng
College of Materials Science and Engineering, Nanjing Tech University, Nanjing 211816, China
1 shared publication Warren W. Rhodes
AT&T Bell Laboratories, Murray Hill, New Jersey 07974
1 shared publicationZhiyang Chen
State Key Laboratory of Materials-Oriented Chemical Engineering Nanjing Tech University Nanjing China
1 shared publication
Latest Publications
- Open Access
- 1 January 2018
- Published by Wiley in Advances in Materials Science and Engineering
- Vol. 2018 (1)
Effect of Particle Size of Periclase on the Periclase Hydration and Expansion of Low‐Heat Portland Cement Pastes
In this paper, low‐heat Portland cement (LHC) clinkers were prepared by calcining raw materials at 1350°C for 2.0 hours, 1400°C for 1.0 hour, 1400°C for 1.5 hours, 1400°C for 2.0 hours, 1450°C for 1.0 hour, and 1450°C for 2.0 hours. The clinkers were ground with gypsum to produce LHC. The particle size of periclase was analysed by BSEM. Expansion of LHC pastes due to hydration of periclase was measured. The hydration degree of periclase in LHC pastes was quantitatively determined by XRD internal standard method and BSEM. The results showed that the particle size of periclase was larger when clinkers were calcined at higher temperatures or for longer time. Smaller periclase (2.60 μm) in LHC pastes tended to hydrate faster. As a result, expansion of LHC pastes develops relatively faster. Smaller particle of periclase in clinker tends to result in higher hydration degree of periclase in pastes cured at 20°C for 240 days, and there is a small amount of brucite appearing around periclase. The hydration rate of 4.00 μm periclase particle in cement paste cured at 80°C is obviously faster than that in paste cured at 20°C and 40°C. When cement paste was cured at 80°C for 7 days, the periclase was hydrated for 32.56%. The smaller size periclase (1–3 μm) had fully hydrated when the curing age was 240 days, and a large amount of brucite was produced around the larger periclase particle.
- 1 January 2018
- Published by Wiley in Advances in Materials Science and Engineering
- Vol. 2018 (1)
Open AccessEffect of Particle Size of Periclase on the Periclase Hydration and Expansion of Low‐Heat Portland Cement Pastes
In this paper, low‐heat Portland cement (LHC) clinkers were prepared by calcining raw materials at 1350°C for 2.0 hours, 1400°C for 1.0 hour, 1400°C for 1.5 hours, 1400°C for 2.0 hours, 1450°C for 1.0 hour, and 1450°C for 2.0 hours. The clinkers were ground with gypsum to produce LHC. The particle size of periclase was analysed by BSEM. Expansion of LHC pastes due to hydration of periclase was measured. The hydration degree of periclase in LHC pastes was quantitatively determined by XRD internal standard method and BSEM. The results showed that the particle size of periclase was larger when clinkers were calcined at higher temperatures or for longer time. Smaller periclase (2.60 μm) in LHC pastes tended to hydrate faster. As a result, expansion of LHC pastes develops relatively faster. Smaller particle of periclase in clinker tends to result in higher hydration degree of periclase in pastes cured at 20°C for 240 days, and there is a small amount of brucite appearing around periclase. The hydration rate of 4.00 μm periclase particle in cement paste cured at 80°C is obviously faster than that in paste cured at 20°C and 40°C. When cement paste was cured at 80°C for 7 days, the periclase was hydrated for 32.56%. The smaller size periclase (1–3 μm) had fully hydrated when the curing age was 240 days, and a large amount of brucite was produced around the larger periclase particle.
- 1 February 1991
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 74 (2) , 287-289
Aging Behavior of x Pb(Fe 2/3 W 1/3 )O 3 · (1 – x )Pb(Fe 1/2 Nb 1/2 )O 3 Ceramic
The aging behavior of a series of lead perovskite dielectrics with the compositions x Pb(Fe 2/3 W 1/3 )O 3 ·(1 – x )Pb(Fe 1/2 ‐Nb 1/2 )O 3 , where 0 ≤ x ≤ 1, and the effect of dopants were studied. Below the Curie temperature ( T c ), the capacitance and the dissipation factor (tan δ) decrease approximately linearly with logarithmic time. The aging rate depends on the temperature difference, Δ T , between the aging temperature and T c , and on the dopant concentration, but is independent of the measurement frequency between 1 and 1000 kHz. The maximum aging rate is about 3% per decade of time for capacitance and 5% per decade for tan δ at 1 mol% dopant concentration, and increases to 6.3% for capacitance and 8.5% for tan δ at 0.7 mol% dopant concentration. These results are consistent with an aging mechanism caused by changing ferroelectric domain structure with time, as proposed for BaTiO 3 .
- 1 February 1991
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 74 (2) , 287-289
Aging Behavior of x Pb(Fe 2/3 W 1/3 )O 3 · (1 – x )Pb(Fe 1/2 Nb 1/2 )O 3 Ceramic
The aging behavior of a series of lead perovskite dielectrics with the compositions x Pb(Fe 2/3 W 1/3 )O 3 ·(1 – x )Pb(Fe 1/2 ‐Nb 1/2 )O 3 , where 0 ≤ x ≤ 1, and the effect of dopants were studied. Below the Curie temperature ( T c ), the capacitance and the dissipation factor (tan δ) decrease approximately linearly with logarithmic time. The aging rate depends on the temperature difference, Δ T , between the aging temperature and T c , and on the dopant concentration, but is independent of the measurement frequency between 1 and 1000 kHz. The maximum aging rate is about 3% per decade of time for capacitance and 5% per decade for tan δ at 1 mol% dopant concentration, and increases to 6.3% for capacitance and 8.5% for tan δ at 0.7 mol% dopant concentration. These results are consistent with an aging mechanism caused by changing ferroelectric domain structure with time, as proposed for BaTiO 3 .