Influence of heat treatments on microstructural and mechanical properties of Grade 5 titanium friction welds
Authors:
- K Sri Ram VikasKVK Sri Ram Vikas
- RahulRARahul
- 1 June 2022
- journal article
- research article
- Published by IOP Publishing in Engineering Research Express
- Vol. 4 (2) , 025053
Abstract
Titanium and its alloys are extensively used in automobile, aerospace and biomedical applications. There are many problems associated with the fusion welding of titanium. Thus, friction welding is an alternative technique for joining titanium without defects. In this study, Ti-6Al-4V (Grade 5 -Titanium alloy) rods were welded using a rotary friction process. Before welding, pre-heat treatments were carried in α - β and β conditions followed by stress relieving on Grade 5 -Titanium alloy rods and some rods were stress relieved after welding. After several trials, friction welding at rotational speed, 1500 rpm and 5 kN upset force obtained defect-free joints. α - β heat treatment enhanced ductility as compared with β heat treatment. α - β heat treatment lead formation of bimodal microstructure in the base metal and β heat treatment produced lamellar Coarse β grains with colonies of α within β grains. Among different heat treatment conditions, high hardness was observed in the α - β heat treatment condition with stress-relieving. Stress-relieving of the welds resulted in an improvement in the hardness because of β precipitates. Fracture morphology is brittle in β treated conditions and ductile in α - β conditions. All welded samples failed away from the weld region irrespective of heat treatments applied, this shows that the weld region is much stronger than the base region due to acicular α and β phases. Mechanical properties were correlated as evidenced by microstructural features.Keywords
This publication has 39 references indexed in Scilit:
- Microstructure and mechanical properties of friction- and electron-beam welded Ti–6Al–4V and Ti–6Al–2Sn–4Zr–6MoMaterials Science and Engineering: A, 2012
- Influence of Parent Metal Microstructure and Post‐Weld Heat Treatment on Microstructure and Mechanical Properties of Linear Friction Welded Ti‐6Al‐4V JointAdvanced Engineering Materials, 2012
- General relationship between strength and hardnessMaterials Science and Engineering: A, 2011
- Identification of Process Parameters for Friction Stir Welding Ti–6Al–4VJournal of Engineering Materials and Technology, 2010
- FEM simulation of the linear friction welding of titanium alloysComputational Materials Science, 2010
- Development of grain structure in β-phase field during friction stir welding of Ti–6Al–4V alloyScripta Materialia, 2008
- Microstructural characteristics and mechanical properties of Ti–6Al–4V friction stir weldsMaterials Science and Engineering: A, 2008
- Thermomechanical processing of alpha titanium alloys—an overviewMaterials Science and Engineering: A, 1999
- Thermomechanical processing of beta titanium alloys—an overviewMaterials Science and Engineering: A, 1998
- Influence of deformation on the β→α+β transformation kinetics of Ti-6wt.%Al-4wt.%V alloyJournal of the Less Common Metals, 1985