K. Sri Ram Vikas
Research Subjects
K. Sri Ram Vikas has a total of 26 co-authors. Here are the top co-authors by number of shared publications:
Rahul
Department of Mechanical Engineering, Chaitanya Bharathi Institute of Technology(A), Hyderabad, Telangana, India
4 shared publicationsV.S.N. Venkata Ramana
3 shared publicationsCh. Kishore Reddy
2 shared publicationsN. Raghu Ram
Department of Mechanical Engineering, PVP Siddhartha Institute of Technology, Vijayawada 520007, Andhra Pradesh, India
2 shared publicationsV S N Venkata Ramana
Department of Mechanical Engineering, GITAM (Deemed to be University), Visakhapatnam-530045, Andhra Pradesh, India
2 shared publicationsB. Sai Charan
Department of Metallurgical and Materials Engineering, Rajiv Gandhi University of Knowledge Technologies, Basar, Telangana 504107, India
1 shared publication
Latest Publications
- 4 August 2026
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part L: Journal of Materials: Design and Applications
Influence of profile-edge geometry on Yttria-Stabilized Zirconia reinforced AA6061 friction stir welds
In the current study, the effects of edge profile configuration and reinforcement with Yttria-Stabilized Zirconia (YSZ) particles on the microstructure, crystallographic texture, and mechanical properties of friction stir welded AA6061-T651 aluminum alloy joints are investigated. A novel profile-edge joint configuration is employed to improve material flow and particle dispersion in friction stir welding, and is compared with a conventional straight-edge joint configuration. Electron Backscattered Diffraction (EBSD) analysis showed that the profile-edge configuration results in better microstructural refinement of the joint, with an average grain size of 6.6 μm compared with 8.4 μm for the straight-edge joint. Moreover, the amount of high-angle grain boundaries increases from 40.1% to 46.3% due to improved recrystallization. Texture analysis has shown that shear texture components are more pronounced in the profile-edge joint, where the maximum texture intensity is 13.6 times that of a random distribution. Microanalysis of the profile-edge joint using Scanning Electron Microscope (SEM) and Energy Dispersive Spectroscopy (EDX) showed that yttria-stabilized zirconia particles were successfully incorporated into the stir zone with a relatively uniform distribution. Phases α-Al, Mg 2 Si, Al 5 FeSi, zirconia, and yttria-stabilized zirconia have been identified by X-Ray Diffraction (XRD) analysis. The profile-edge configuration resulted in an improved hardness of up to 105 HV, compared with 101 HV for the straight-edge configuration. The mechanical properties are considerably improved in the profile-edge joint, with an ultimate tensile strength of 348 ± 12.9 MPa, a yield strength of 311 ± 10.4 MPa, and an elongation of 12.8 ± 2.5%, resulting in a joint efficiency of 92–95%. Fractographic analysis indicates a ductile fracture with evenly distributed dimples.
- 4 August 2026
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part L: Journal of Materials: Design and Applications
Influence of profile-edge geometry on Yttria-Stabilized Zirconia reinforced AA6061 friction stir welds
In the current study, the effects of edge profile configuration and reinforcement with Yttria-Stabilized Zirconia (YSZ) particles on the microstructure, crystallographic texture, and mechanical properties of friction stir welded AA6061-T651 aluminum alloy joints are investigated. A novel profile-edge joint configuration is employed to improve material flow and particle dispersion in friction stir welding, and is compared with a conventional straight-edge joint configuration. Electron Backscattered Diffraction (EBSD) analysis showed that the profile-edge configuration results in better microstructural refinement of the joint, with an average grain size of 6.6 μm compared with 8.4 μm for the straight-edge joint. Moreover, the amount of high-angle grain boundaries increases from 40.1% to 46.3% due to improved recrystallization. Texture analysis has shown that shear texture components are more pronounced in the profile-edge joint, where the maximum texture intensity is 13.6 times that of a random distribution. Microanalysis of the profile-edge joint using Scanning Electron Microscope (SEM) and Energy Dispersive Spectroscopy (EDX) showed that yttria-stabilized zirconia particles were successfully incorporated into the stir zone with a relatively uniform distribution. Phases α-Al, Mg 2 Si, Al 5 FeSi, zirconia, and yttria-stabilized zirconia have been identified by X-Ray Diffraction (XRD) analysis. The profile-edge configuration resulted in an improved hardness of up to 105 HV, compared with 101 HV for the straight-edge configuration. The mechanical properties are considerably improved in the profile-edge joint, with an ultimate tensile strength of 348 ± 12.9 MPa, a yield strength of 311 ± 10.4 MPa, and an elongation of 12.8 ± 2.5%, resulting in a joint efficiency of 92–95%. Fractographic analysis indicates a ductile fracture with evenly distributed dimples.
- 20 September 2023
- Published by Springer Nature in Journal of The Institution of Engineers (India): Series D
- Vol. 105 (2) , 929-947
Effect of Heat Treatments on Tensile Fracture Behaviour of Ti-6Al-4V Alloy Friction Welds
- 20 September 2023
- Published by Springer Nature in Journal of The Institution of Engineers (India): Series D
- Vol. 105 (2) , 929-947
Effect of Heat Treatments on Tensile Fracture Behaviour of Ti-6Al-4V Alloy Friction Welds
- 9 September 2022
- Published by Elsevier in Chemical Data Collections
- Vol. 42
Influence of heat treatments on corrosion behavior of Ti64 friction welds
- 9 September 2022
- Published by Elsevier in Chemical Data Collections
- Vol. 42
Influence of heat treatments on corrosion behavior of Ti64 friction welds
- 1 June 2022
- Published by IOP Publishing in Engineering Research Express
- Vol. 4 (2) , 025053
Influence of heat treatments on microstructural and mechanical properties of Grade 5 titanium friction welds
Titanium and its alloys are extensively used in automobile, aerospace and biomedical applications. There are many problems associated with the fusion welding of titanium. Thus, friction welding is an alternative technique for joining titanium without defects. In this study, Ti-6Al-4V (Grade 5 -Titanium alloy) rods were welded using a rotary friction process. Before welding, pre-heat treatments were carried in α - β and β conditions followed by stress relieving on Grade 5 -Titanium alloy rods and some rods were stress relieved after welding. After several trials, friction welding at rotational speed, 1500 rpm and 5 kN upset force obtained defect-free joints. α - β heat treatment enhanced ductility as compared with β heat treatment. α - β heat treatment lead formation of bimodal microstructure in the base metal and β heat treatment produced lamellar Coarse β grains with colonies of α within β grains. Among different heat treatment conditions, high hardness was observed in the α - β heat treatment condition with stress-relieving. Stress-relieving of the welds resulted in an improvement in the hardness because of β precipitates. Fracture morphology is brittle in β treated conditions and ductile in α - β conditions. All welded samples failed away from the weld region irrespective of heat treatments applied, this shows that the weld region is much stronger than the base region due to acicular α and β phases. Mechanical properties were correlated as evidenced by microstructural features.
- 1 June 2022
- Published by IOP Publishing in Engineering Research Express
- Vol. 4 (2) , 025053
Influence of heat treatments on microstructural and mechanical properties of Grade 5 titanium friction welds
Titanium and its alloys are extensively used in automobile, aerospace and biomedical applications. There are many problems associated with the fusion welding of titanium. Thus, friction welding is an alternative technique for joining titanium without defects. In this study, Ti-6Al-4V (Grade 5 -Titanium alloy) rods were welded using a rotary friction process. Before welding, pre-heat treatments were carried in α - β and β conditions followed by stress relieving on Grade 5 -Titanium alloy rods and some rods were stress relieved after welding. After several trials, friction welding at rotational speed, 1500 rpm and 5 kN upset force obtained defect-free joints. α - β heat treatment enhanced ductility as compared with β heat treatment. α - β heat treatment lead formation of bimodal microstructure in the base metal and β heat treatment produced lamellar Coarse β grains with colonies of α within β grains. Among different heat treatment conditions, high hardness was observed in the α - β heat treatment condition with stress-relieving. Stress-relieving of the welds resulted in an improvement in the hardness because of β precipitates. Fracture morphology is brittle in β treated conditions and ductile in α - β conditions. All welded samples failed away from the weld region irrespective of heat treatments applied, this shows that the weld region is much stronger than the base region due to acicular α and β phases. Mechanical properties were correlated as evidenced by microstructural features.
- 14 April 2022
- Published by IOP Publishing in Engineering Research Express
- Vol. 4 (2) , 025010
Effect of nano ZrB2 particles on physical, mechanical and corrosion properties of Al6061 metal-matrix nano composites through stir casting route
The present study investigated the microstructure, mechanical and corrosion behaviour of Al6061 alloy reinforced with nano zirconium diboride (ZrB2) particles. The stir casting route is carried out to fabricate the Al6061 metal matrix nanocomposites (AMMNCs) by varying 0 to 2 Wt% of ZrB2 nanoparticles. X-ray Diffraction (XRD)was used to study the crystalline size and phase distribution of AMMNCs. Scanning electron microscope (SEM) analysis reveals the uniform dispersion of ZrB2 nano particulates in AMMNCs. Ultimate tensile strength and yield strength, hardness of the AMMNCs were increased by 33.58%, 27.54%, and 40.57%, respectively, with the addition of ZrB2 nano particulates, while the elongation decreased to 46.03%. with the increase in ZrB2 Wt%. The corrosion rate of AMMNCs (2 Wt% ZrB2) decreased by 86% compared to Al6061 alloy. Fracture analysis of the samples showed that the fracture behaviour of Al6061 matrix alloy changed from ductile intergranular fracture to cleavage. The results show that the developed nanocomposite enhances mechanical properties and corrosion resistance with an increase in Wt% of reinforcement.
- 14 April 2022
- Published by IOP Publishing in Engineering Research Express
- Vol. 4 (2) , 025010
Effect of nano ZrB2 particles on physical, mechanical and corrosion properties of Al6061 metal-matrix nano composites through stir casting route
The present study investigated the microstructure, mechanical and corrosion behaviour of Al6061 alloy reinforced with nano zirconium diboride (ZrB2) particles. The stir casting route is carried out to fabricate the Al6061 metal matrix nanocomposites (AMMNCs) by varying 0 to 2 Wt% of ZrB2 nanoparticles. X-ray Diffraction (XRD)was used to study the crystalline size and phase distribution of AMMNCs. Scanning electron microscope (SEM) analysis reveals the uniform dispersion of ZrB2 nano particulates in AMMNCs. Ultimate tensile strength and yield strength, hardness of the AMMNCs were increased by 33.58%, 27.54%, and 40.57%, respectively, with the addition of ZrB2 nano particulates, while the elongation decreased to 46.03%. with the increase in ZrB2 Wt%. The corrosion rate of AMMNCs (2 Wt% ZrB2) decreased by 86% compared to Al6061 alloy. Fracture analysis of the samples showed that the fracture behaviour of Al6061 matrix alloy changed from ductile intergranular fracture to cleavage. The results show that the developed nanocomposite enhances mechanical properties and corrosion resistance with an increase in Wt% of reinforcement.
- 1 January 2022
- Published by Elsevier in Materials Today: Proceedings
- Vol. 52, 1615-1621
Comparison of microstructure and corrosion behaviour of AA2014 electron beam and friction stir welds
- 1 January 2022
- Published by Elsevier in Materials Today: Proceedings
- Vol. 52, 1615-1621
Comparison of microstructure and corrosion behaviour of AA2014 electron beam and friction stir welds
- 1 January 2022
- Published by Elsevier in Materials Today: Proceedings
- Vol. 52, 1515-1520
Wear and corrosion behavior of AA6061 metal matrix composites with ilmenite as reinforcement
- 1 January 2022
- Published by Elsevier in Materials Today: Proceedings
- Vol. 52, 1515-1520
Wear and corrosion behavior of AA6061 metal matrix composites with ilmenite as reinforcement
- 9 July 2020
- Published by Elsevier in Materials Today: Proceedings
- Vol. 41, 1001-1007
Hot pressing of copper and copper-based composites: Microstructure and suitability as electrodes for electric discharge machining
- 9 July 2020
- Published by Elsevier in Materials Today: Proceedings
- Vol. 41, 1001-1007
Hot pressing of copper and copper-based composites: Microstructure and suitability as electrodes for electric discharge machining
- 1 November 2015
- Published by Diva Enterprises Private Limited in International Journal of Scientific Engineering and Technology
- Vol. 4 (11) , 505-510
Process Parameters and Foaming Agents Used in Manufacturing of Aluminium metallic foams: A Review
- 1 November 2015
- Published by Diva Enterprises Private Limited in International Journal of Scientific Engineering and Technology
- Vol. 4 (11) , 505-510
Process Parameters and Foaming Agents Used in Manufacturing of Aluminium metallic foams: A Review