Atomic layer deposition of scandium‐based oxides

Authors:

Abstract
GdxSc2−xO3 and AlxSc2−xO3 have been investigated as potential high‐k intergate dielectric (IGD) in planar NAND flash technology, such as hybrid floating gate (HFG). We have examined the atomic layer deposition (ALD) of Sc2O3, GdxSc2−xO3, and AlxSc2−xO3 on Si using Sc(MeCp)3, Gd(iPrCp)3, TMA, and H2O as precursors. The composition of GdxSc2−xO3 and AlxSc2−xO3 ranged from 4% to 76% Gd and from 7% to 66% Al, respectively. All compositions show linear growth behavior. While pure Sc2O3 is crystalline as‐deposited, the layer becomes amorphous once ∼20% of Al is added. The (222) reflection of the cubic phase is also seen for GdxSc2−xO3 with less than 9% Gd. The bandgap of as‐deposited GdxSc2−xO3 decreases with increasing Gd content while the opposite trend is observed for AlxSc2−xO3. A k‐value of ∼21 can be obtained for GdxSc2−xO3 with approximately 26–52% Gd, irrespective of the Gd content. For AlxSc2−xO3 on the other hand, a maximum k‐value of ∼19 is achieved with ∼48% Al. Although the k‐value of AlxSc2−xO3 is lower than that of GdxSc2−xO3, its large breakdown field makes this material more suitable for HFG flash applications.

This publication has 28 references indexed in Scilit: