Effect of Pyrolysis Temperature on the Piezoresistivity of Polymer‐Derived Ceramics
Authors:
- 10 January 2011
- journal article
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 94 (2) , 359-362
Abstract
Amorphous silicon carbonitride (SiCN) ceramics were synthesized by pyrolyzing a polysilazane at different temperatures between 900° and 1400°C. The microstructures and compositions of the materials obtained were analyzed using X‐ray diffraction, elemental analysis, and Raman spectroscopy. To study their piezoresistive behavior, the resistivity of the resultant materials were measured as a function of applied stress. We found that the piezoresistive behavior of all materials can fit the tunneling‐percolation model. The piezoresistive stress coefficient of the materials obtained at temperatures below 1200°C showed both reverse and logarithmical dependences on applied stress, but that of the materials obtained at higher temperatures showed only logarithmical dependence. We believe that the pyrolysis temperature induces a change in the free carbon structure thus, causing this effect on the piezoresistivity.Keywords
This publication has 16 references indexed in Scilit:
- Giant piezoresistivity of polymer-derived ceramics at high temperaturesJournal of the European Ceramic Society, 2010
- A Silicon Carbonitride Ceramic with Anomalously High PiezoresistivityJournal of the American Ceramic Society, 2008
- Polymer-derived SiAlCN ceramics resist oxidation at 1400°CScripta Materialia, 2006
- Silicoaluminum carbonitride ceramic resist to oxidation/corrosion in water vaporJournal of Materials Research, 2006
- Carbon‐Nanotube‐Reinforced Polymer‐Derived Ceramic CompositesAdvanced Materials, 2004
- Application of microforging to SiCN MEMS fabricationSensors and Actuators A: Physical, 2002
- Polymer Derived Engineering CeramicsAdvanced Engineering Materials, 2000
- Amorphous Silicoboron Carbonitride Ceramic with Very High Viscosity at Temperatures above 1500°CJournal of the American Ceramic Society, 1998
- A silicoboron carbonitride ceramic stable to 2,000°CNature, 1996
- Development of high tensile strength silicon carbide fibre using an organosilicon polymer precursorNature, 1978