Linan An
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Linan An has a total of 27 co-authors. Here are the top co-authors by number of shared publications:
Kewei Wang
Science and Technology on Thermostuctural Composite Materials Laboratory, Northwestern Polytechnical University , Xi'an, Shaanxi 710072, People's Republic of China
4 shared publicationsYiguang Wang
National Key Laboratory of Thermostructure Composite Northwestern Polytechnical University Xi'an Shaanxi 710072 China
4 shared publications- Yiguang Wang
Science and Technology on Thermostructural Composite Materials Laboratory Northwestern Polytechnical University Xi'an Shaanxi China
4 shared publications - Baisheng Ma
State Key Laboratory of Solidification Processing Northwestern Polytechnical University Xi'an Shaanxi 710072 China
3 shared publications - Chengying Xu
Department of Mechanical and Aerospace Engineering, North Carolina State University, Raleigh, USA
2 shared publications Xuqin Li
Science and Technology on Thermostuctural Composite Materials Laboratory, Northwestern Polytechnical University, Xi’an, Shaanxi 710072, People’s Republic of China
2 shared publications
Latest Publications
- 1 May 2017
- Published by American Scientific Publishers in Journal of Nanoscience and Nanotechnology
- Vol. 17 (5) , 3233-3237
Synthesis and Photoluminescence Properties of Tb3+ Doped ZrO2 Hollow Spheres
ZrO2:Tb3+ hollow spheres were successfully fabricated with the resin microspheres as the template. The sample characterizations were carried out by means of X-ray diffraction (XRD), scanning electron microscope (SEM) and photoluminescence (PL) spectra. XRD results revealed Tb3+ doped samples were pure t-ZrO2 phase after being calcined at 873 K. SEM results exhibited these Tb3+ doped ZrO2 was hollow spheres, the diameter and thickness of which were about 450 nm and 50 nm, respectively. The PL spectra indicate that the 5D4 → 7F5 (545 nm) electric dipole transition is the most intensive when excited at 235 nm. It is shown that the 2.0 mol% of doping concentration of Tb3+ ions in t-ZrO2:Tb3+ is optimum. According to Dexter’s theory, the critical distance between Tb3+ ions for energy transfer was determined to be 15 Å. It is found that the decay curves follow the single-exponential decay. The convenient synthetic procedure, excellent reproducibility, clean reactions, high yield, and fine quality of products in the work make the present route attractive and significant.
- 1 May 2017
- Published by American Scientific Publishers in Journal of Nanoscience and Nanotechnology
- Vol. 17 (5) , 3233-3237
Synthesis and Photoluminescence Properties of Tb3+ Doped ZrO2 Hollow Spheres
ZrO2:Tb3+ hollow spheres were successfully fabricated with the resin microspheres as the template. The sample characterizations were carried out by means of X-ray diffraction (XRD), scanning electron microscope (SEM) and photoluminescence (PL) spectra. XRD results revealed Tb3+ doped samples were pure t-ZrO2 phase after being calcined at 873 K. SEM results exhibited these Tb3+ doped ZrO2 was hollow spheres, the diameter and thickness of which were about 450 nm and 50 nm, respectively. The PL spectra indicate that the 5D4 → 7F5 (545 nm) electric dipole transition is the most intensive when excited at 235 nm. It is shown that the 2.0 mol% of doping concentration of Tb3+ ions in t-ZrO2:Tb3+ is optimum. According to Dexter’s theory, the critical distance between Tb3+ ions for energy transfer was determined to be 15 Å. It is found that the decay curves follow the single-exponential decay. The convenient synthetic procedure, excellent reproducibility, clean reactions, high yield, and fine quality of products in the work make the present route attractive and significant.
- 20 January 2015
- Published by American Chemical Society (ACS) in The Journal of Physical Chemistry A
- Vol. 119 (4) , 552-558
Structural Evolutions in Polymer-Derived Carbon-Rich Amorphous Silicon Carbide
The detailed structural evolutions in polycarbosilane-derived carbon-rich amorphous SiC were investigated semiquantitatively by combining experimental and analytical methods. It is revealed that the material is comprised of a Si-containing matrix phase and a free-carbon phase. The matrix phase is amorphous, comprised of SiC4 tetrahedra, SiCxOx–4 tetrahedra, and Si–C–C–Si/Si–C–H defects. With increasing pyrolysis temperature, the amorphous matrix becomes more ordered, accompanied by a transition from SiC2O2 to SiCO3. The transition was completed at 1250 °C, where the matrix phase started to crystallize by forming a small amount of β-SiC. The free-carbon phase was comprised of carbon nanoclusters and C-dangling bonds. Increasing pyrolysis temperature led to the transition of the free carbon from amorphous carbon to nanocrystalline graphite. The size of the carbon clusters decreased first and then increased, while the C-dangling bond content decreased continuously. The growth of carbon clusters was attributed to Ostwald ripening and described using a two-dimensional grain growth model. The calculated activation energy suggested that the decrease in C-dangling bonds is directly related to the lateral growth of the carbon clusters.
- 20 January 2015
- Published by American Chemical Society (ACS) in The Journal of Physical Chemistry A
- Vol. 119 (4) , 552-558
Structural Evolutions in Polymer-Derived Carbon-Rich Amorphous Silicon Carbide
The detailed structural evolutions in polycarbosilane-derived carbon-rich amorphous SiC were investigated semiquantitatively by combining experimental and analytical methods. It is revealed that the material is comprised of a Si-containing matrix phase and a free-carbon phase. The matrix phase is amorphous, comprised of SiC4 tetrahedra, SiCxOx–4 tetrahedra, and Si–C–C–Si/Si–C–H defects. With increasing pyrolysis temperature, the amorphous matrix becomes more ordered, accompanied by a transition from SiC2O2 to SiCO3. The transition was completed at 1250 °C, where the matrix phase started to crystallize by forming a small amount of β-SiC. The free-carbon phase was comprised of carbon nanoclusters and C-dangling bonds. Increasing pyrolysis temperature led to the transition of the free carbon from amorphous carbon to nanocrystalline graphite. The size of the carbon clusters decreased first and then increased, while the C-dangling bond content decreased continuously. The growth of carbon clusters was attributed to Ostwald ripening and described using a two-dimensional grain growth model. The calculated activation energy suggested that the decrease in C-dangling bonds is directly related to the lateral growth of the carbon clusters.
- 10 April 2014
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 97 (7) , 2135-2138
Effect of Pyrolysis Temperature on the Structure and Conduction of Polymer‐Derived SiC
We studied the electric conductivity and structure of polymer‐derived carbon‐rich amorphous SiC pyrolyzed at different temperatures. The conductivity of the material increased drastically with pyrolysis temperature followed an Arrhenius relationship with the activation energy of ~3.4 eV. Raman and X‐ray photoelectron spectroscopy analysis revealed that the order of free carbon phase increased with pyrolysis temperature, accompanied by sp3→sp2 transition. The activation energy for such a structure change was 3.1–3.8 eV, which is close to that for the conductivity change. We thus believe that the increase in the conductivity was mainly due to the increase in conductivity of the free carbon phase.
- 10 April 2014
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 97 (7) , 2135-2138
Effect of Pyrolysis Temperature on the Structure and Conduction of Polymer‐Derived SiC
We studied the electric conductivity and structure of polymer‐derived carbon‐rich amorphous SiC pyrolyzed at different temperatures. The conductivity of the material increased drastically with pyrolysis temperature followed an Arrhenius relationship with the activation energy of ~3.4 eV. Raman and X‐ray photoelectron spectroscopy analysis revealed that the order of free carbon phase increased with pyrolysis temperature, accompanied by sp3→sp2 transition. The activation energy for such a structure change was 3.1–3.8 eV, which is close to that for the conductivity change. We thus believe that the increase in the conductivity was mainly due to the increase in conductivity of the free carbon phase.
- 19 April 2013
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 96 (5) , 1363-1365
Complex Impedance Spectra of Polymer‐Derived Silicon Oxycarbides
The complex impedance spectra of polymer‐derived amorphous silicon oxycarbides synthesized at different temperatures are reported. Analysis of the spectra using equivalent circuit models showed that the conduction of current is dominantly through the matrix and free carbon in series, instead of through the matrix or free carbon only. We found that the conductivity of both matrix and free‐carbon phase increases with increasing synthesis temperature, whereas the relaxation time of the matrix is much shorter than that of the free carbon. The results are correlated with the structures of the materials.
- 19 April 2013
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 96 (5) , 1363-1365
Complex Impedance Spectra of Polymer‐Derived Silicon Oxycarbides
The complex impedance spectra of polymer‐derived amorphous silicon oxycarbides synthesized at different temperatures are reported. Analysis of the spectra using equivalent circuit models showed that the conduction of current is dominantly through the matrix and free carbon in series, instead of through the matrix or free carbon only. We found that the conductivity of both matrix and free‐carbon phase increases with increasing synthesis temperature, whereas the relaxation time of the matrix is much shorter than that of the free carbon. The results are correlated with the structures of the materials.
- 15 November 2011
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 95 (1) , 374-378
Oxidation Behavior of ZrB 2 –SiC–TaC Ceramics
ZrB 2 –SiC–TaC ceramics with different content of TaC were prepared by hot‐pressing at 1800°C in vacuum environment. The oxidation behavior of these ceramics was studied in the temperature range of 1200°C–1500°C in air. It was found that low concentration of TaC (10 vol%) deteriorated the oxidation resistance of ZrB 2 – SiC , while high concentration of TaC (30 vol%) significantly improved the oxidation resistance of the ceramics. Reoxidation experiments indicated that the metallic species (tantalum and/or silicon) diffusing out of the materials into the oxides was initially involved in the controlling process.
- 15 November 2011
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 95 (1) , 374-378
Oxidation Behavior of ZrB 2 –SiC–TaC Ceramics
ZrB 2 –SiC–TaC ceramics with different content of TaC were prepared by hot‐pressing at 1800°C in vacuum environment. The oxidation behavior of these ceramics was studied in the temperature range of 1200°C–1500°C in air. It was found that low concentration of TaC (10 vol%) deteriorated the oxidation resistance of ZrB 2 – SiC , while high concentration of TaC (30 vol%) significantly improved the oxidation resistance of the ceramics. Reoxidation experiments indicated that the metallic species (tantalum and/or silicon) diffusing out of the materials into the oxides was initially involved in the controlling process.
- 19 October 2011
- Published by Royal Society of Chemistry (RSC) in Journal of Materials Chemistry
- Vol. 21 (45) , 18186-18190
Self-assembled carbon–silicon carbonitride nanocomposites: high-performance anode materials for lithium-ion batteries
A new class of nanocomposites comprising an amorphous silicon carbonitride matrix and carbon nanoclusters was synthesized by decomposing polymeric precursors with thermally induced phase separation. Electrochemical measurements show that the nanocomposite with 30% of carbon nanoclusters exhibits a specific capacity of 480 mA h g−1 and excellent cycling performance. The high capacity of the nanocomposites is attributed to the formation of a novel structure around the SiCN–C interface. The excellent electrochemical properties, together with the simple, low-cost processing, make the nanocomposites very promising for Li-ion battery applications.
- 19 October 2011
- Published by Royal Society of Chemistry (RSC) in Journal of Materials Chemistry
- Vol. 21 (45) , 18186-18190
Self-assembled carbon–silicon carbonitride nanocomposites: high-performance anode materials for lithium-ion batteries
A new class of nanocomposites comprising an amorphous silicon carbonitride matrix and carbon nanoclusters was synthesized by decomposing polymeric precursors with thermally induced phase separation. Electrochemical measurements show that the nanocomposite with 30% of carbon nanoclusters exhibits a specific capacity of 480 mA h g−1 and excellent cycling performance. The high capacity of the nanocomposites is attributed to the formation of a novel structure around the SiCN–C interface. The excellent electrochemical properties, together with the simple, low-cost processing, make the nanocomposites very promising for Li-ion battery applications.
- 15 July 2011
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 94 (9) , 2779-2782
Synthesis of Spherical Non‐Oxide Silicon Carbonitride Ceramic Particles
In this article, we report a simple technique for synthesizing spherical non‐oxide silicon carbonitride ceramic particles from a polysilazane precursor. In this technique, the spherical particles of the polysilazane precursor were synthesized first via a precipitation polymerization process and then converted to ceramic particles by pyrolysis. The resultant ceramic particles exhibited a close‐to‐perfect spherical shape and a narrow size distribution around 430 nm. The precipitation and pyrolysis processes were characterized using SEM , TEM , FTIR , and XRD to illustrate the formation mechanisms of the ceramic particles.
- 15 July 2011
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 94 (9) , 2779-2782
Synthesis of Spherical Non‐Oxide Silicon Carbonitride Ceramic Particles
In this article, we report a simple technique for synthesizing spherical non‐oxide silicon carbonitride ceramic particles from a polysilazane precursor. In this technique, the spherical particles of the polysilazane precursor were synthesized first via a precipitation polymerization process and then converted to ceramic particles by pyrolysis. The resultant ceramic particles exhibited a close‐to‐perfect spherical shape and a narrow size distribution around 430 nm. The precipitation and pyrolysis processes were characterized using SEM , TEM , FTIR , and XRD to illustrate the formation mechanisms of the ceramic particles.
- 27 June 2011
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 94 (10) , 3359-3363
Structure and Optical Property of Polymer‐Derived Amorphous Silicon Oxycarbides Obtained at Different Temperatures
Amorphous silicon carbides are prepared by pyrolysis of a polycarbosilane precursor at different temperatures between 1000° and 1400°C. The structures of the resultant materials are analyzed using X‐ray diffraction, electron paramagnetic resonance, and Raman spectroscopy. The optical properties of the SiC ceramics are investigated by measuring their absorption spectra. It is found that there is a critical temperature range, at which the structural and optical behavior varied in different ways as a function of pyrolysis temperature. The evolution in structures is discussed and the optical behavior is explained in terms of the structural evolution during pyrolysis at different temperatures.
- 27 June 2011
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 94 (10) , 3359-3363
Structure and Optical Property of Polymer‐Derived Amorphous Silicon Oxycarbides Obtained at Different Temperatures
Amorphous silicon carbides are prepared by pyrolysis of a polycarbosilane precursor at different temperatures between 1000° and 1400°C. The structures of the resultant materials are analyzed using X‐ray diffraction, electron paramagnetic resonance, and Raman spectroscopy. The optical properties of the SiC ceramics are investigated by measuring their absorption spectra. It is found that there is a critical temperature range, at which the structural and optical behavior varied in different ways as a function of pyrolysis temperature. The evolution in structures is discussed and the optical behavior is explained in terms of the structural evolution during pyrolysis at different temperatures.
- 10 January 2011
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 94 (2) , 359-362
Effect of Pyrolysis Temperature on the Piezoresistivity of Polymer‐Derived Ceramics
Amorphous silicon carbonitride (SiCN) ceramics were synthesized by pyrolyzing a polysilazane at different temperatures between 900° and 1400°C. The microstructures and compositions of the materials obtained were analyzed using X‐ray diffraction, elemental analysis, and Raman spectroscopy. To study their piezoresistive behavior, the resistivity of the resultant materials were measured as a function of applied stress. We found that the piezoresistive behavior of all materials can fit the tunneling‐percolation model. The piezoresistive stress coefficient of the materials obtained at temperatures below 1200°C showed both reverse and logarithmical dependences on applied stress, but that of the materials obtained at higher temperatures showed only logarithmical dependence. We believe that the pyrolysis temperature induces a change in the free carbon structure thus, causing this effect on the piezoresistivity.
- 10 January 2011
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 94 (2) , 359-362
Effect of Pyrolysis Temperature on the Piezoresistivity of Polymer‐Derived Ceramics
Amorphous silicon carbonitride (SiCN) ceramics were synthesized by pyrolyzing a polysilazane at different temperatures between 900° and 1400°C. The microstructures and compositions of the materials obtained were analyzed using X‐ray diffraction, elemental analysis, and Raman spectroscopy. To study their piezoresistive behavior, the resistivity of the resultant materials were measured as a function of applied stress. We found that the piezoresistive behavior of all materials can fit the tunneling‐percolation model. The piezoresistive stress coefficient of the materials obtained at temperatures below 1200°C showed both reverse and logarithmical dependences on applied stress, but that of the materials obtained at higher temperatures showed only logarithmical dependence. We believe that the pyrolysis temperature induces a change in the free carbon structure thus, causing this effect on the piezoresistivity.