Abstract
In the common spent fuels, actinides and fission products are generally in the form of oxide, so direct dealing with oxide will be the most convenient way for spent fuel reprocessing. In this work, the electrolytic reduction of Gd 2 O 3 has been studied in LiCl-KCl-Li 2 O (1 wt%) melts at different conditions, and the effect of sintering temperature on the porosity of Gd 2 O 3 powder and the electrochemical behavior of Li 2 O in LiCl-KCl molten salt were investigated, too. The diffusion coefficient of O 2− was calculated to be 2.0 × 10 −5 cm 2 ·s −1 in LiCl-KCl melts on the Mo electrode at 923 K by cyclic voltammetry (CV). The electrode process of Gd 2 O 3 powder was also analyzed in LiCl-KCl-Li 2 O (1 wt%) melts, and the formation process of composite oxide LiGdO 2 was determined. By the analysis of XRD and oxygen content characterization, it was suggested that after 74 h electrolysis (923 K, 3.40 V), the oxygen content of Gd 2 O 3 cathode decreased from 12.25 wt% to 1.41 wt%, indicating 88.5% Gd 2 O 3 was reduced to metal.

This publication has 39 references indexed in Scilit: