High‐cycle fatigue and fracture behaviours of Cu‐Be alloy with a wide strength range
- 15 July 2012
- journal article
- Published by Wiley in Fatigue & Fracture of Engineering Materials & Structures
- Vol. 36 (2) , 168-176
Abstract
The high‐cycle fatigue and fracture behaviours of Cu‐Be alloy with tensile strength ranging from 500 to 1300 MPa acquired by different treatments were studied. Fatigue crack initiation, fracture surface morphologies, S‐N curves and fatigue strength show obvious differences due to the change of microstructure. At relatively low‐strength level, some fatigue cracks originated from defects; while at high‐strength level, all the fatigue cracks initiated from cleavage facets. It was found that the fatigue ratio increases linearly and fatigue strength changes quadratically with increasing tensile strength, only considering one strengthening mechanism. Finally, the fatigue strengths of various Cu‐Be alloys were summarized.Keywords
This publication has 25 references indexed in Scilit:
- Fatigue strengths of Cu–Be alloy with high tensile strengthsScripta Materialia, 2010
- Cyclic deformation and fatigue properties of very fine-grained metals and alloysInternational Journal of Fatigue, 2010
- Mechanisms of strain localization, crack initiation and fracture of polycrystalline copper in the VHCF regimeInternational Journal of Fatigue, 2010
- Fatigue damage in copper polycrystals subjected to ultrahigh-cycle fatigue below the PSB thresholdInternational Journal of Fatigue, 2010
- Mechanical Behavior of Materials2008
- Fatigue strength and formation behavior of surface damage in ultrafine grained copper with different non-equilibrium microstructuresInternational Journal of Fatigue, 2008
- Fatigue of Materials1998
- Fatigue and corrosion fatigue of beryllium-copper spring materialsInternational Journal of Fatigue, 1994
- THE ENGINEERING FATIGUE PROPERTIES OF WROUGHT COPPER*†Fatigue & Fracture of Engineering Materials & Structures, 1981
- High resolution electron microscope observations on G.P. zones in an aged Cu-1.97wt.% Be crystalActa Metallurgica, 1973