Precipitation of crack tip hydrides in zirconium alloys
Authors:
- Young Suk KimYKYoung Suk Kim
- Yong Moo CheongYCYong Moo Cheong
- 1 February 2007
- journal article
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 429 (1-2) , 221-226
Abstract
No abstract availableKeywords
This publication has 14 references indexed in Scilit:
- Driving force for delayed Hydride cracking of zirconium alloysMetals and Materials International, 2005
- Delayed hydride cracking in Zr–2.5Nb tube with the cooling rate and the notch tip shapeJournal of Nuclear Materials, 2004
- Hydrogen concentration limit and critical temperatures for delayed hydride cracking in zirconium alloysJournal of Nuclear Materials, 1995
- Dependence of the threshold stress intensity factor on hydrogen concentration during delayed hydride cracking in zirconium alloysJournal of Nuclear Materials, 1995
- The thermal ratchetting of hydrogen in zirconium-niobium — An illustration using finite element modellingScripta Metallurgica et Materialia, 1993
- Effect of stress on hydride precipitation in zirconium-2.5% niobium and on delayed hydride crackingScripta Metallurgica, 1989
- Dilation of h.c.p. zirconium by interstitial deuteriumActa Metallurgica, 1985
- The effect of stress on hydride precipitationScripta Metallurgica, 1981
- Low temperature hydrogen embrittlement of niobium II—Microscopic observationsActa Metallurgica, 1977
- Hydride precipitation in Nb and some properties of NbHJournal of the Less Common Metals, 1976