Nonmetallic Inclusions in Fe–26Mn–10Al–1.2Si–3Cr–3Ni–1.4C–0.1V Induction‐Melted Steel and their Influence on Fracture Under Hot Plastic Deformation
- 27 October 2025
- journal article
- Published by Wiley in Steel Research International
- Vol. 97 (5) , 2421-2428
Abstract
The work represents study of the nonmetallic inclusions formation and their influence on the fracture of induction‐melted Fe–26Mn–10Al–1.2Si–3Cr–3Ni–1.4C–0.1V steel in as‐cast state and under conditions of hot plastic deformation. The microstructure of steel in initial state is investigated, as well as cold and hot fractures. It is shown that the investigated steel has several types of noticeable defects after casting. The first one is represented by small Mn‐rich oxides and eutectic‐like areas, while the other one seems to be Al 2 O 3 films, which leads to microcrack formation. The reason for low deformability is also in a rough columnar grain structure, which points to slow crystallization and impurity movement to the grain boundaries. After 90 min annealing with further rolling from 1050 °C, steel remains prone to hot crack formation. It is mainly caused by initial structure, inclusions, and formation of carbides at the grain boundary, especially in near eutectic areas that contain S and P. XRD investigations show that hot crack surface contains N and C‐rich austenite, iron nitride, as well as Mn and Al oxides with complex Fe–Mn oxides.Keywords
This publication has 23 references indexed in Scilit:
- Implications of the microstructure on strength-ductility synergy in a novel B2-strengthened medium manganese advanced high strength steelMaterials Science and Engineering: A, 2025
- Internal oxidation behavior and its effect on the surface crack formation in a Fe-Mn-Al-C high Mn steelEngineering Failure Analysis, 2024
- Uncovering Microstructure–Property Relationship in Ni-Alloyed Fe–Mn–Al–C Low-Density Steel Treated by Hot-Rolling and Air-Cooling ProcessActa Metallurgica Sinica (English Letters), 2024
- Effects of Mn Content on the Formation of Inclusions in High Aluminum SteelMetallurgical and Materials Transactions B, 2023
- Precipitation behavior of κ-carbides and its relationship with mechanical properties of Fe–Mn–Al–C lightweight austenitic steelJournal of Materials Research and Technology, 2023
- B2-ordered NiAl content on microstructure, mechanical and oxidation properties of FeAl intermetallic compoundsJournal of Materials Research and Technology, 2022
- Microstructural and Fracture Behavior of Phosphorus-Containing Fe-30Mn-9Al-1Si-0.9C-0.5Mo Alloy SteelMetallurgical and Materials Transactions A, 2015
- High Manganese and Aluminum Steels for the Military and Transportation IndustryJOM, 2014
- Alloy Design, Combinatorial Synthesis, and Microstructure–Property Relations for Low-Density Fe-Mn-Al-C Austenitic SteelsJOM, 2014
- State of the art in the control of inclusions during steel ingot castingMetallurgical and Materials Transactions B, 2006