Compressive strength geopolymer mortar with fine aggregate soaked in NaOH solution
Open Access
- 1 January 2023
- conference paper
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 2677 (1) , 040006
Abstract
Geopolymer mortar is a mortar based on fly ash derived from coal combustion waste as a substitute for whole cement or mortar without cement which provides an environmentally friendly and efficient effect in terms of energy utilization. In contrast to cement which undergoes a hydration reaction with water to produce a binder, fly ash which is rich in silicon (Si) and alumina (Al) elements will react when mixed with an alkaline activator solution. The alkaline activator solution used is Na2SiO3 and NaOH with a mixing ratio of 1,5 where the variation of NaOH concentration used is 9 and 13 molar. The fine aggregate used was taken from the Batanghari River which was soaked with NaOH solution. Based on the research, the average flow value is 112,3% and the compressive strength of geopolymer mortar 9 and 13 Molar respectively for the age of 7 days = 26,03 and 34,02 MPa, 14 days = 32,01 and 43,01 MPa, 28 days = 35,36 and 48,40 MPa. The compressive strength of the geopolymer mortar with a concentration of NaOH 13 Molar is closer to the value of a cement mortar compared to a concentration of 9 Molar.Keywords
This publication has 5 references indexed in Scilit:
- The Nature of Coconut Fibre Fly Ash-Based Mechanical GeopolymerIOP Conference Series: Materials Science and Engineering, 2020
- Mechanical Properties of Fly Ash-Based Geopolymer with Natural FiberJournal of Physics: Conference Series, 2019
- Oil palm ash-based geopolymer mortar with variation Na2SiO3/NaOH ratioAIP Conference Proceedings, 2018
- Strength and Setting Times of Low Calcium Fly Ash-based Geopolymer MortarModern Applied Science, 2008
- Alkali–aggregate reaction in activated fly ash systemsCement and Concrete Research, 2007