Ria Zulfiati
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Ria Zulfiati has a total of 4 co-authors. Here are the top co-authors by number of shared publications:
- Aaroon Joshua Das
Department of Civil Engineering, Capital University of Science and Technology, Islamabad 45750, Pakistan
1 shared publication Saloma
1 shared publication- Wari Dony
Faculty of Civil Engineering, University of Batanghari, Jambi, Indonesia
1 shared publication Yakni Idris
1 shared publication
Latest Publications
- Open Access
- 1 January 2023
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 2677 (1) , 040006
Compressive strength geopolymer mortar with fine aggregate soaked in NaOH solution
Geopolymer mortar is a mortar based on fly ash derived from coal combustion waste as a substitute for whole cement or mortar without cement which provides an environmentally friendly and efficient effect in terms of energy utilization. In contrast to cement which undergoes a hydration reaction with water to produce a binder, fly ash which is rich in silicon (Si) and alumina (Al) elements will react when mixed with an alkaline activator solution. The alkaline activator solution used is Na2SiO3 and NaOH with a mixing ratio of 1,5 where the variation of NaOH concentration used is 9 and 13 molar. The fine aggregate used was taken from the Batanghari River which was soaked with NaOH solution. Based on the research, the average flow value is 112,3% and the compressive strength of geopolymer mortar 9 and 13 Molar respectively for the age of 7 days = 26,03 and 34,02 MPa, 14 days = 32,01 and 43,01 MPa, 28 days = 35,36 and 48,40 MPa. The compressive strength of the geopolymer mortar with a concentration of NaOH 13 Molar is closer to the value of a cement mortar compared to a concentration of 9 Molar.
- 1 January 2023
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 2677 (1) , 040006
Open AccessCompressive strength geopolymer mortar with fine aggregate soaked in NaOH solution
Geopolymer mortar is a mortar based on fly ash derived from coal combustion waste as a substitute for whole cement or mortar without cement which provides an environmentally friendly and efficient effect in terms of energy utilization. In contrast to cement which undergoes a hydration reaction with water to produce a binder, fly ash which is rich in silicon (Si) and alumina (Al) elements will react when mixed with an alkaline activator solution. The alkaline activator solution used is Na2SiO3 and NaOH with a mixing ratio of 1,5 where the variation of NaOH concentration used is 9 and 13 molar. The fine aggregate used was taken from the Batanghari River which was soaked with NaOH solution. Based on the research, the average flow value is 112,3% and the compressive strength of geopolymer mortar 9 and 13 Molar respectively for the age of 7 days = 26,03 and 34,02 MPa, 14 days = 32,01 and 43,01 MPa, 28 days = 35,36 and 48,40 MPa. The compressive strength of the geopolymer mortar with a concentration of NaOH 13 Molar is closer to the value of a cement mortar compared to a concentration of 9 Molar.
- Open Access
- 1 March 2020
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 807 (1)
The Nature of Coconut Fibre Fly Ash-Based Mechanical Geopolymer
In order to reduce carbon emissions in the atmosphere, one of the steps is to use environmentally friendly concrete. Environmentally friendly concrete uses industrial waste as a substitute for cement, such as rice husk ash, palm burning ash, coal burning ash or fly ash. Today, the development of the use of fly ash as a substitute for cement has been widely used, especially in geopolymer concrete. This study uses natural fibres such as coconut fibre. Coconut fibre is also an alternative material in the use of natural fibres as geopolymer mortar composites. This research carried out compressive strength and flexural strength test by doing several variations such as the length of coconut fibres 10 mm, 20 mm, and 30 mm and the percentage of fibre used was 0, 0.25% and 0.50% of the weight of the mortar. Geopolymer mortar made from 100% fly ash. The concentration of NaOH solution used was 14 M and 16 M. The results of this study indicate that the fibre length of 30 mm with a percentage of 0.50% fibre at a concentration of 16 M NaOH solution gives a compressive strength of 40.016 MPa and the greatest flexural strength of 8.799 MPa at 28 days mortar age.
- 1 March 2020
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 807 (1)
Open AccessThe Nature of Coconut Fibre Fly Ash-Based Mechanical Geopolymer
In order to reduce carbon emissions in the atmosphere, one of the steps is to use environmentally friendly concrete. Environmentally friendly concrete uses industrial waste as a substitute for cement, such as rice husk ash, palm burning ash, coal burning ash or fly ash. Today, the development of the use of fly ash as a substitute for cement has been widely used, especially in geopolymer concrete. This study uses natural fibres such as coconut fibre. Coconut fibre is also an alternative material in the use of natural fibres as geopolymer mortar composites. This research carried out compressive strength and flexural strength test by doing several variations such as the length of coconut fibres 10 mm, 20 mm, and 30 mm and the percentage of fibre used was 0, 0.25% and 0.50% of the weight of the mortar. Geopolymer mortar made from 100% fly ash. The concentration of NaOH solution used was 14 M and 16 M. The results of this study indicate that the fibre length of 30 mm with a percentage of 0.50% fibre at a concentration of 16 M NaOH solution gives a compressive strength of 40.016 MPa and the greatest flexural strength of 8.799 MPa at 28 days mortar age.