Effect of steel substrate type on the thermal stability and phase transformations of amorphous quasi-high-entropy (Fe0.25Co0.25Ni0.25Cr0.125V0.125)80B20 coatings obtained by vacuum electrospark deposition

Authors:

Abstract
Most studies on high-entropy and quasi-high-entropy Me–B alloys have been conducted on ribbons or bulk specimens; however, data on the crystallization, phase transformations, and thermal stability of these amorphous materials remain extremely limited. Coatings allow the advantages of amorphous and nanocrystalline states to be realized in a thin surface layer, but the substrate material has an additional effect. Local remelting and interdiffusion incorporate some of the substrate elements into the coating, altering its average chemical composition and creating local concentration gradients through its thickness. This study aimed to establish the effect of steel substrate type on the thermal stability, crystallization kinetics, and phase transformations of amorphous quasi-high-entropy (Fe 0.25 Co 0.25 Ni 0.25 Cr 0.125 V 0.125 ) 80 B 20 coatings produced by vacuum electrospark deposition on 30KhGSA and AISI 430 steels. Differential scanning calorimetry, X -ray diffraction (XRD), and electron microscopy were used, together with microhardness measurements in the as-deposited and annealed states. Crystallization of the (Fe 0.25 Co 0.25 Ni 0.25 Cr 0.125 V 0.125 ) 80 B 20 alloy coating on 30KhGSA steel proceeded through a metastable two-phase stage involving competition between BCC and FCC phases, whereas the coating on AISI 430 followed a direct pathway to FCC phase formation. However, after annealing at 820 °C, the coatings reached similar structure states, confirming the thermodynamic stability of the combination of an FCC solid solution and Me₃B₂ borides in the FeCoNiCrV–20B system, regardless of steel substrate type. The coating on 30KhGSA steel had a high as-deposited hardness of 12.4 GPa, which was retained after annealing at 600 °C (12.3 GPa) and increased slightly after annealing at 700 °C (13.0 GPa). Annealing at 820 °C caused a sharp decrease in hardness to 6.6 GPa. The coating on AISI 430 steel showed similar behavior: its as-deposited hardness was 12.6 GPa, decreasing to 11.3–11.6 GPa after annealing at 600–700 °C and falling sharply to 6.6 GPa after annealing at 820 °C.

This publication has 35 references indexed in Scilit: