Konstantin A. Kuptsov
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Konstantin A. Kuptsov has a total of 87 co-authors. Here are the top co-authors by number of shared publications:
- Dmitry V. Shtansky
National University of Science and Technology “MISIS” Moscow Russian Federation
22 shared publications - Philipp Vladimirovich Kiryukhantsev-Korneev
National University of Science and Technology “MISIS
13 shared publications A.N. Sheveyko
9 shared publications- Alexander Nikolaevich Sheveyko
Scientific-Educational Center of SHS, National University of Science and Technology “MISiS”, 119049 Moscow, Russia
7 shared publications - Mariya N. Antonyuk
National University of Science and Technology “MISIS
4 shared publications - Alexander N. Sheveyko
National University of Science and Technology MISiS
3 shared publications
Latest Publications
- Open Access
- 24 October 2026
- Published by National University of Science and Technology MISiS in Powder Metallurgy аnd Functional Coatings
Effect of steel substrate type on the thermal stability and phase transformations of amorphous quasi-high-entropy (Fe0.25Co0.25Ni0.25Cr0.125V0.125)80B20 coatings obtained by vacuum electrospark deposition
Most studies on high-entropy and quasi-high-entropy Me–B alloys have been conducted on ribbons or bulk specimens; however, data on the crystallization, phase transformations, and thermal stability of these amorphous materials remain extremely limited. Coatings allow the advantages of amorphous and nanocrystalline states to be realized in a thin surface layer, but the substrate material has an additional effect. Local remelting and interdiffusion incorporate some of the substrate elements into the coating, altering its average chemical composition and creating local concentration gradients through its thickness. This study aimed to establish the effect of steel substrate type on the thermal stability, crystallization kinetics, and phase transformations of amorphous quasi-high-entropy (Fe 0.25 Co 0.25 Ni 0.25 Cr 0.125 V 0.125 ) 80 B 20 coatings produced by vacuum electrospark deposition on 30KhGSA and AISI 430 steels. Differential scanning calorimetry, X -ray diffraction (XRD), and electron microscopy were used, together with microhardness measurements in the as-deposited and annealed states. Crystallization of the (Fe 0.25 Co 0.25 Ni 0.25 Cr 0.125 V 0.125 ) 80 B 20 alloy coating on 30KhGSA steel proceeded through a metastable two-phase stage involving competition between BCC and FCC phases, whereas the coating on AISI 430 followed a direct pathway to FCC phase formation. However, after annealing at 820 °C, the coatings reached similar structure states, confirming the thermodynamic stability of the combination of an FCC solid solution and Me₃B₂ borides in the FeCoNiCrV–20B system, regardless of steel substrate type. The coating on 30KhGSA steel had a high as-deposited hardness of 12.4 GPa, which was retained after annealing at 600 °C (12.3 GPa) and increased slightly after annealing at 700 °C (13.0 GPa). Annealing at 820 °C caused a sharp decrease in hardness to 6.6 GPa. The coating on AISI 430 steel showed similar behavior: its as-deposited hardness was 12.6 GPa, decreasing to 11.3–11.6 GPa after annealing at 600–700 °C and falling sharply to 6.6 GPa after annealing at 820 °C.
- 24 October 2026
- Published by National University of Science and Technology MISiS in Powder Metallurgy аnd Functional Coatings
Open AccessEffect of steel substrate type on the thermal stability and phase transformations of amorphous quasi-high-entropy (Fe0.25Co0.25Ni0.25Cr0.125V0.125)80B20 coatings obtained by vacuum electrospark deposition
Most studies on high-entropy and quasi-high-entropy Me–B alloys have been conducted on ribbons or bulk specimens; however, data on the crystallization, phase transformations, and thermal stability of these amorphous materials remain extremely limited. Coatings allow the advantages of amorphous and nanocrystalline states to be realized in a thin surface layer, but the substrate material has an additional effect. Local remelting and interdiffusion incorporate some of the substrate elements into the coating, altering its average chemical composition and creating local concentration gradients through its thickness. This study aimed to establish the effect of steel substrate type on the thermal stability, crystallization kinetics, and phase transformations of amorphous quasi-high-entropy (Fe 0.25 Co 0.25 Ni 0.25 Cr 0.125 V 0.125 ) 80 B 20 coatings produced by vacuum electrospark deposition on 30KhGSA and AISI 430 steels. Differential scanning calorimetry, X -ray diffraction (XRD), and electron microscopy were used, together with microhardness measurements in the as-deposited and annealed states. Crystallization of the (Fe 0.25 Co 0.25 Ni 0.25 Cr 0.125 V 0.125 ) 80 B 20 alloy coating on 30KhGSA steel proceeded through a metastable two-phase stage involving competition between BCC and FCC phases, whereas the coating on AISI 430 followed a direct pathway to FCC phase formation. However, after annealing at 820 °C, the coatings reached similar structure states, confirming the thermodynamic stability of the combination of an FCC solid solution and Me₃B₂ borides in the FeCoNiCrV–20B system, regardless of steel substrate type. The coating on 30KhGSA steel had a high as-deposited hardness of 12.4 GPa, which was retained after annealing at 600 °C (12.3 GPa) and increased slightly after annealing at 700 °C (13.0 GPa). Annealing at 820 °C caused a sharp decrease in hardness to 6.6 GPa. The coating on AISI 430 steel showed similar behavior: its as-deposited hardness was 12.6 GPa, decreasing to 11.3–11.6 GPa after annealing at 600–700 °C and falling sharply to 6.6 GPa after annealing at 820 °C.
- 31 January 2026
- Published by Elsevier in Materials Chemistry and Physics
- Vol. 354
Mechanisms limiting silver incorporation in bioactive PEO-Ag coatings on Ti6Al4V
- 31 January 2026
- Published by Elsevier in Materials Chemistry and Physics
- Vol. 354
Mechanisms limiting silver incorporation in bioactive PEO-Ag coatings on Ti6Al4V
- 30 June 2025
- Published by Ore and Metals Publishing House in CIS Iron and Steel Review
- Vol. 29, 89-96
Fe–Cr–Ni–Co–Cux coatings for marine and coastal infrastructure protection from corrosion, tribocorrosion and biofouling
The aim of this study is to investigate the effect of varying copper (Cu) content on the structure, corrosion, tribocorrosion, and bactericidal properties of FeCrNiCo–Cux coatings. Specifically, the main idea is to maximize the Cu content without secondary phases formation using Electrospark Deposition (ESD) method characterized by rapid cooling rates of the melt, while maintaining the corrosion properties of the Cu-free coating, and simultaneously enhancing its antimicrobial and tribocorrosion properties. To achieve this, thick high-entropy Fe–Cr–Ni–Co–(Cu) coatings with different Cu content (up to 24 at. %) were obtained in a protective argon atmosphere. All coatings exhibited a single-phase structure based on a solid solution with an fcc lattice, dense and homogeneous microstructure with high continuity. In tribocorrosion conditions, the FeCrNiCo coating demonstrated the lowest corrosion current, while the FeCrNiCo–12Cu coating revealed the most positive corrosion potential. However, after a certain Cu content threshold, tribocorrosion behavior deteriorated significantly. In terms of wear, coatings with high Cu content exhibited the highest wear resistance, which did not correlate with the hardness of the coatings. All coatings demonstrated a moderate antibacterial effect against B. cereus Arc30, with the FeCrNiCo–12Cu coating showing the highest ability to suppress bacterial growth and further biofilm formation. The work was financially supported by the Russian Science Foundation (Agreement No. 20-79-10104-П).
- 30 June 2025
- Published by Ore and Metals Publishing House in CIS Iron and Steel Review
- Vol. 29, 89-96
Fe–Cr–Ni–Co–Cux coatings for marine and coastal infrastructure protection from corrosion, tribocorrosion and biofouling
The aim of this study is to investigate the effect of varying copper (Cu) content on the structure, corrosion, tribocorrosion, and bactericidal properties of FeCrNiCo–Cux coatings. Specifically, the main idea is to maximize the Cu content without secondary phases formation using Electrospark Deposition (ESD) method characterized by rapid cooling rates of the melt, while maintaining the corrosion properties of the Cu-free coating, and simultaneously enhancing its antimicrobial and tribocorrosion properties. To achieve this, thick high-entropy Fe–Cr–Ni–Co–(Cu) coatings with different Cu content (up to 24 at. %) were obtained in a protective argon atmosphere. All coatings exhibited a single-phase structure based on a solid solution with an fcc lattice, dense and homogeneous microstructure with high continuity. In tribocorrosion conditions, the FeCrNiCo coating demonstrated the lowest corrosion current, while the FeCrNiCo–12Cu coating revealed the most positive corrosion potential. However, after a certain Cu content threshold, tribocorrosion behavior deteriorated significantly. In terms of wear, coatings with high Cu content exhibited the highest wear resistance, which did not correlate with the hardness of the coatings. All coatings demonstrated a moderate antibacterial effect against B. cereus Arc30, with the FeCrNiCo–12Cu coating showing the highest ability to suppress bacterial growth and further biofilm formation. The work was financially supported by the Russian Science Foundation (Agreement No. 20-79-10104-П).
- Open Access
- 3 October 2024
- Published by National University of Science and Technology MISiS in Izvestiya Vuzov. Tsvetnaya Metallurgiya (Proceedings of Higher Schools. Nonferrous Metallurgy)
- No. 3,p. 87-96
High-entropy Fe–Co–Cr–Ni–(Cu) coatings with enhanced corrosion and tribocorrosion resistance obtained by vacuum electrospark deposition
High-entropy coatings are highly promising for protecting steel parts in coastal and marine infrastructure from corrosion and tribocorrosion. This study examines the properties of medium- and high-entropy Fe–Co–Cr–Ni–(Cu) coatings produced by vacuum electrospark deposition. The coatings, with thicknesses of up to 30 μm and varying copper content, exhibit a single-phase solid solution structure with an FCC lattice and a dense, homogeneous morphology. The addition of 14 at.% Cu was found to enhance corrosion resistance, shifting the corrosion potential to 100 mV. In friction conditions within artificial seawater, the inclusion of copper also improved tribocorrosion properties, raising the corrosion potential during friction to –165 mV. This improvement is attributed to the galvanic deposition of dissolved copper on the worn areas of the coating, which also reduces the friction coefficient from 0.37 to 0.26. The Fe–Co–Cr–Ni–(Cu) coatings demonstrate high wear resistance, ranging from 5.6 to 9.6·10–6 mm3/(N·m). The findings confirm the potential of these coatings for applications in environments subject to both friction and corrosion.
- 3 October 2024
- Published by National University of Science and Technology MISiS in Izvestiya Vuzov. Tsvetnaya Metallurgiya (Proceedings of Higher Schools. Nonferrous Metallurgy)
- No. 3,p. 87-96
Open AccessHigh-entropy Fe–Co–Cr–Ni–(Cu) coatings with enhanced corrosion and tribocorrosion resistance obtained by vacuum electrospark deposition
High-entropy coatings are highly promising for protecting steel parts in coastal and marine infrastructure from corrosion and tribocorrosion. This study examines the properties of medium- and high-entropy Fe–Co–Cr–Ni–(Cu) coatings produced by vacuum electrospark deposition. The coatings, with thicknesses of up to 30 μm and varying copper content, exhibit a single-phase solid solution structure with an FCC lattice and a dense, homogeneous morphology. The addition of 14 at.% Cu was found to enhance corrosion resistance, shifting the corrosion potential to 100 mV. In friction conditions within artificial seawater, the inclusion of copper also improved tribocorrosion properties, raising the corrosion potential during friction to –165 mV. This improvement is attributed to the galvanic deposition of dissolved copper on the worn areas of the coating, which also reduces the friction coefficient from 0.37 to 0.26. The Fe–Co–Cr–Ni–(Cu) coatings demonstrate high wear resistance, ranging from 5.6 to 9.6·10–6 mm3/(N·m). The findings confirm the potential of these coatings for applications in environments subject to both friction and corrosion.
- Open Access
TiAl-Based Oxidation-Resistant Hard Coatings with Different Al Contents Obtained by Vacuum-Pulse-Arc Granule Melting
A method was proposed for increasing the oxidation resistance of promising wrought Ti2AlNb ortho-alloys by depositing γ-TiAl-based coatings. Using original vacuum pulse-arc melting of 100 μm thick granule layers, coatings with different Al/Ti ratios and a thickness of 50–60 µm were obtained on the surface of the Ti50Al25Nb25 alloy. Granules Ti50Al44Nb4.9Mo1B0.1 (at.%), 20–60 μm in size, were employed. To vary Al content, initial granules and their mixture with Al powder were used. Excellent adhesion of the coatings is ensured by the similar chemical composition and structure of the substrate and coatings, as well as micro-metallurgical reactions between granules and the substrate that occur during treatment. The resulting coatings had a submicron gradient structure consisting of TiAl and Ti3Al intermetallic compounds. During oxidation at 850 °C for 10 h, an oxide layer consisting of a mixture of α-Al2O3, TiO2, and AlNbO4 was formed on the coating surfaces. With an increase in the annealing duration to 100 h, a dense α-Al2O3 oxide layer, approximately 0.5 µm thick, was formed over the primary oxide mixture, the quality of which was higher in coatings enriched with aluminum.
Open AccessTiAl-Based Oxidation-Resistant Hard Coatings with Different Al Contents Obtained by Vacuum-Pulse-Arc Granule Melting
A method was proposed for increasing the oxidation resistance of promising wrought Ti2AlNb ortho-alloys by depositing γ-TiAl-based coatings. Using original vacuum pulse-arc melting of 100 μm thick granule layers, coatings with different Al/Ti ratios and a thickness of 50–60 µm were obtained on the surface of the Ti50Al25Nb25 alloy. Granules Ti50Al44Nb4.9Mo1B0.1 (at.%), 20–60 μm in size, were employed. To vary Al content, initial granules and their mixture with Al powder were used. Excellent adhesion of the coatings is ensured by the similar chemical composition and structure of the substrate and coatings, as well as micro-metallurgical reactions between granules and the substrate that occur during treatment. The resulting coatings had a submicron gradient structure consisting of TiAl and Ti3Al intermetallic compounds. During oxidation at 850 °C for 10 h, an oxide layer consisting of a mixture of α-Al2O3, TiO2, and AlNbO4 was formed on the coating surfaces. With an increase in the annealing duration to 100 h, a dense α-Al2O3 oxide layer, approximately 0.5 µm thick, was formed over the primary oxide mixture, the quality of which was higher in coatings enriched with aluminum.
- 5 October 2023
- Published by Elsevier in Materials Letters
- Vol. 354
Enhanced mechanical properties of Ni-based composites doped with a low amount of amorphous boron
- 5 October 2023
- Published by Elsevier in Materials Letters
- Vol. 354
Enhanced mechanical properties of Ni-based composites doped with a low amount of amorphous boron
- Open Access
- 23 September 2023
- Published by National University of Science and Technology MISiS in Powder Metallurgy аnd Functional Coatings
- Vol. 17 (3) , 67-78
TaC-based wear-resistant coatings obtained by magnetron sputtering and electro-spark deposition for wedge gate valve protection
Ta–Zr–Si–B–C coatings were deposited by magnetron sputtering (MS) of a TaSi2–Ta3B4–(Ta, Zr)B2 multi-component target in an Ar + C2H4 gas mixture. TaC–Cr–Mo–Ni based coatings were obtained by electro-spark deposition (ESD) using TaC–Cr–Mo–Ni electrode. The composition and structure of the coatings were studied using scanning electron microscopy, energy-dispersive spectroscopy, glow discharge optical emission spectroscopy and X-ray diffraction. Mechanical and tribological properties of coatings were determined using nanoindentation and pin-on-disk tests. The study showed that the coatings have a homogeneous and defect-free structure, with the main structural component being the fcc-TaC phase. The MS coating exhibited a 30 % higher concentration of the TaC phase compared to the ESD coating. The TaC crystallite sizes for the MS and ESD coatings were 3 and 30 nm, respectively. The presence of a high fraction of the carbide phase and small crystallite size for the MS coating resulted in superior hardness (H = 28 GPa) compared to the ESD sample (H = 10 GPa). Both coatings exhibited similar values of the friction coefficient (about 0.15) and demonstrated reduced wear rates (–7 mm3/(N·m)). The deposition of coatings on a steel substrate led to a decrease in the friction coefficient by five times and the wear rate by four orders of magnitude. Pilot tests were conducted on coatings applied to wedge gate valve of shut-off devices used in the oil and gas industry for pumping liquids. The results indicated that the service life of the steel wedge gate valve increased by 25 and 70 % with deposited MS and ESD coatings, respectively.
- 23 September 2023
- Published by National University of Science and Technology MISiS in Powder Metallurgy аnd Functional Coatings
- Vol. 17 (3) , 67-78
Open AccessTaC-based wear-resistant coatings obtained by magnetron sputtering and electro-spark deposition for wedge gate valve protection
Ta–Zr–Si–B–C coatings were deposited by magnetron sputtering (MS) of a TaSi2–Ta3B4–(Ta, Zr)B2 multi-component target in an Ar + C2H4 gas mixture. TaC–Cr–Mo–Ni based coatings were obtained by electro-spark deposition (ESD) using TaC–Cr–Mo–Ni electrode. The composition and structure of the coatings were studied using scanning electron microscopy, energy-dispersive spectroscopy, glow discharge optical emission spectroscopy and X-ray diffraction. Mechanical and tribological properties of coatings were determined using nanoindentation and pin-on-disk tests. The study showed that the coatings have a homogeneous and defect-free structure, with the main structural component being the fcc-TaC phase. The MS coating exhibited a 30 % higher concentration of the TaC phase compared to the ESD coating. The TaC crystallite sizes for the MS and ESD coatings were 3 and 30 nm, respectively. The presence of a high fraction of the carbide phase and small crystallite size for the MS coating resulted in superior hardness (H = 28 GPa) compared to the ESD sample (H = 10 GPa). Both coatings exhibited similar values of the friction coefficient (about 0.15) and demonstrated reduced wear rates (–7 mm3/(N·m)). The deposition of coatings on a steel substrate led to a decrease in the friction coefficient by five times and the wear rate by four orders of magnitude. Pilot tests were conducted on coatings applied to wedge gate valve of shut-off devices used in the oil and gas industry for pumping liquids. The results indicated that the service life of the steel wedge gate valve increased by 25 and 70 % with deposited MS and ESD coatings, respectively.
- Open Access
Influence of TiC Addition on Corrosion and Tribocorrosion Resistance of Cr2Ti-NiAl Electrospark Coatings
Marine and coastal infrastructures usually suffer from synergetic effect of corrosion and wear known as tribocorrosion, which imposes strict requirements on the structural materials used. To overcome this problem, novel composite wear- and corrosion-resistant xTiC-Fe-CrTiNiAl coatings with different TiC content were successfully developed. The coatings were obtained by the original technology of electrospark deposition in a vacuum using xTiC-Cr2Ti-NiAl (x = 0, 25, 50, 75%) electrodes. The structure and morphology of the coatings were studied in detail by XRD, SEM, and TEM. The effect of TiC content on the tribocorrosion behavior of the coatings was estimated using tribological and electrochemical (under stationary and wear conditions) experiments, as well as impact testing, in artificial seawater. The TiC-free Fe-Cr2Ti-NiAl coating revealed a defective inhomogeneous structure with transverse and longitudinal cracks. Introduction of TiC allowed us to obtain coatings with a dense structure without visible defects and with uniformly distributed carbide grains. The TiC-containing coatings were characterized by a hardness and elastic modulus of up to 10.3 and 158 GPa, respectively. Formation of a composite structure with a heavily alloyed corrosion-resistant matrix based on α-(Fe,Cr) solid solution and uniformly distributed TiC grains led to a significant increase in resistance to stationary corrosion and tribocorrosion in artificial seawater. The best 75TiC-Fe-CrTiNiAl coating demonstrated the lowest corrosion current density values both under stationary (0.03 μA/cm2) and friction conditions (0.8 μA/cm2), and was characterized by both a 2-2.5 times lower wear rate (4 × 10−6 mm3/Nm) compared to AISI 420S steel and 25TiC-Fe-CrTiNiAl and a high fracture toughness.
Open AccessInfluence of TiC Addition on Corrosion and Tribocorrosion Resistance of Cr2Ti-NiAl Electrospark Coatings
Marine and coastal infrastructures usually suffer from synergetic effect of corrosion and wear known as tribocorrosion, which imposes strict requirements on the structural materials used. To overcome this problem, novel composite wear- and corrosion-resistant xTiC-Fe-CrTiNiAl coatings with different TiC content were successfully developed. The coatings were obtained by the original technology of electrospark deposition in a vacuum using xTiC-Cr2Ti-NiAl (x = 0, 25, 50, 75%) electrodes. The structure and morphology of the coatings were studied in detail by XRD, SEM, and TEM. The effect of TiC content on the tribocorrosion behavior of the coatings was estimated using tribological and electrochemical (under stationary and wear conditions) experiments, as well as impact testing, in artificial seawater. The TiC-free Fe-Cr2Ti-NiAl coating revealed a defective inhomogeneous structure with transverse and longitudinal cracks. Introduction of TiC allowed us to obtain coatings with a dense structure without visible defects and with uniformly distributed carbide grains. The TiC-containing coatings were characterized by a hardness and elastic modulus of up to 10.3 and 158 GPa, respectively. Formation of a composite structure with a heavily alloyed corrosion-resistant matrix based on α-(Fe,Cr) solid solution and uniformly distributed TiC grains led to a significant increase in resistance to stationary corrosion and tribocorrosion in artificial seawater. The best 75TiC-Fe-CrTiNiAl coating demonstrated the lowest corrosion current density values both under stationary (0.03 μA/cm2) and friction conditions (0.8 μA/cm2), and was characterized by both a 2-2.5 times lower wear rate (4 × 10−6 mm3/Nm) compared to AISI 420S steel and 25TiC-Fe-CrTiNiAl and a high fracture toughness.