Thermooxidative ageing of polyoxymethylene, part 1: Chemical aspects
Authors:
- 25 October 2007
- journal article
- research article
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 107 (3) , 1783-1792
Abstract
The thermal oxidation of unstabilised POM homopolymer has been studied at 90, 110, and 130°C under various oxygen pressures ranging from 0 to 2.0 MPa by gravimetry and IR spectrometry. This latter reveals essentially the formation of formate (F) groups and alcohols in smaller quantities. The formate growth and mass loss rates increase pseudo hyperbolically with oxygen pressure, the asymptotic level being reached at pressures up to 0.5 MPa. These results lead to propose a mechanistic scheme of radical chain oxidation in which depolymerization is initiated by hydroperoxide unimolecular decomposition, one formate and one chain scission being formed per decomposition event whereas the kinetic chain length of the depolymerization zip is of the order of 100. A kinetic model derived from the mechanistic scheme, taking into account substrate consumption, simulates correctly the shape of kinetic curves and the effect of temperature and oxygen pressure. © 2007 Wiley Periodicals, Inc. J Appl Polym Sci, 2008Keywords
This publication has 17 references indexed in Scilit:
- Determination of molecular weight distributions of linear flexible polymers from linear viscoelastic material functionsJournal of Rheology, 1994
- The kinetics of thermal stabilization of polyformaldehydePolymer Science U.S.S.R., 1970
- Oxidation of polyoxymethylenesPolymer Science U.S.S.R., 1969
- Accelerated degradation of the polyformaldehyde chain on oxidationPolymer Science U.S.S.R., 1966
- Formation of peroxide radicals during the oxidation of polyformaldehydePolymer Science U.S.S.R., 1965
- Thermo and thermo-oxidative degradation of polyformaldehyde-IV. Kinetics of the thermo-oxidative reactionPolymer Science U.S.S.R., 1964
- Thermal and thermo-oxidative degradation of polyformaldehyde—III. Chain transfer reaction in the thermo-oxidative degradationPolymer Science U.S.S.R., 1964
- The effect of stabilizing additives in the degradation of polyformaldehydePolymer Science U.S.S.R., 1964
- The stabilization of polyformaldehydePolymer Science U.S.S.R., 1964
- The thermal and thermal-oxidative degradation of polyformaldehyde—I. The order of reaction in thermal degradationPolymer Science U.S.S.R., 1963