Bruno Fayolle
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Bruno Fayolle has a total of 38 co-authors. Here are the top co-authors by number of shared publications:
Emmanuel Richaud
LIM (UMR 8006), Arts et Métiers ParisTech., Paris, France
3 shared publicationsJ. Verdu
Laboratoire Ingenierie des Matériaux, UMR 8006 CNRS–Arts et Métiers Paristech 151 Bd de l'Hôpital, 75013 Paris, France
3 shared publicationsJacques Verdu
LIM (UMR 8006), Arts et Métiers ParisTech., Paris, France
3 shared publicationsD. Piccoz
AREVA, T&D Boulevard de la résistance, BP 84019, 71040 Mâcon, Cedex 9, France
2 shared publicationsFabienne Farcas
Laboratoire Central des Ponts et Chaussées, Service Physico-Chimie des Matériaux, 58 Bd Lefebvre, 75015 Paris, France
2 shared publicationsA. Dahoun
Laboratoire de Physique des Matériaux, UMR 7556 CNRS–Nancy Université INPL, Ecole des Mines de Nancy, Parc de Saurupt, 54042 Nancy Cedex, France
1 shared publication
Latest Publications
- 13 November 2009
- Published by Springer Nature in Colloid and Polymer Science
- Vol. 288 (1) , 97-103
An experimental and analytical study of the elasticity of model polyurethane networks crosslinked by tri- and quadriisocyanate
- 13 November 2009
- Published by Springer Nature in Colloid and Polymer Science
- Vol. 288 (1) , 97-103
An experimental and analytical study of the elasticity of model polyurethane networks crosslinked by tri- and quadriisocyanate
- 1 January 2009
- Published by Elsevier
Contributor contact details
- 1 November 2008
- Published by Springer Nature in Journal of Materials Science
- Vol. 43 (22) , 6999-7012
Review: degradation-induced embrittlement in semi-crystalline polymers having their amorphous phase in rubbery state
- 1 November 2008
- Published by Springer Nature in Journal of Materials Science
- Vol. 43 (22) , 6999-7012
Review: degradation-induced embrittlement in semi-crystalline polymers having their amorphous phase in rubbery state
- 9 October 2008
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 111 (1) , 469-475
Thermooxidative aging of polyoxymethylene, part 2: Embrittlement mechanisms
The thermal oxidation at 130°C of polyoxymethylene homopolymer (H) and copolymer (C) samples of close initial molar masses has been studied by gravimetry, rheometry, X ray scattering, and tensile testing. Both samples undergo random chain scission and depolymerization. Their crystallinity ratio increases, whereas their long period decreases. All these changes are faster for H than for C. Tensile tests reveal that there is no significant change of behavior law except for the ultimate strain, which decreases abruptly when the weight average molar mass reaches a value of the order of 70 kg mol−1 for H and 90 kg mol−1 for C. At these molar masses values, the entanglement network of the amorphous phase has undergone only small damagement. In contrast, a chemi‐crystallization process has induced significant morphological changes, especially a decrease of the interlamellar thickness. It is suggested that this latter phenomenon could be responsible for embrittlement. © 2008 Wiley Periodicals, Inc. J Appl Polym Sci, 2009
- 9 October 2008
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 111 (1) , 469-475
Thermooxidative aging of polyoxymethylene, part 2: Embrittlement mechanisms
The thermal oxidation at 130°C of polyoxymethylene homopolymer (H) and copolymer (C) samples of close initial molar masses has been studied by gravimetry, rheometry, X ray scattering, and tensile testing. Both samples undergo random chain scission and depolymerization. Their crystallinity ratio increases, whereas their long period decreases. All these changes are faster for H than for C. Tensile tests reveal that there is no significant change of behavior law except for the ultimate strain, which decreases abruptly when the weight average molar mass reaches a value of the order of 70 kg mol−1 for H and 90 kg mol−1 for C. At these molar masses values, the entanglement network of the amorphous phase has undergone only small damagement. In contrast, a chemi‐crystallization process has induced significant morphological changes, especially a decrease of the interlamellar thickness. It is suggested that this latter phenomenon could be responsible for embrittlement. © 2008 Wiley Periodicals, Inc. J Appl Polym Sci, 2009
- 10 September 2008
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 110 (6) , 3313-3321
Accelerated ageing of polypropylene stabilized by phenolic antioxidants under high oxygen pressure
Polypropylene (PP) samples stabilized by a hindered phenol (Irganox 1010) were submitted to thermal ageing at 80°C in air at atmospheric pressure or in pure oxygen at 5.0 MPa pressure. Both the polymer oxidation and the stabilizer consumption were monitored by Infrared spectrometry and thermal analysis. The stabilizer efficiency, as assessed by the ratio induction time/stabilizer concentration is almost constant at atmospheric pressure even when the stabilizer concentration is higher than its solubility limit in PP (0.4% or 24 × 10−3 mol L−1). In contrast, at high pressure, the efficiency decreases almost hyperbolically with the stabilizer concentration when this latter is higher than 6.0 × 10−3 mol L−1. The results indicate the existence of a direct phenol‐oxygen reaction negligible at low oxygen pressure but significant at 5.0 MPa pressure. The reality of this reaction has been proved on the basis of a study of the thermal oxidation of a phenol solution in a nonoxidizable solvent. A kinetic model of PP oxidation in which stabilization involves three reactions has been proposed. It simulates correctly the effect of oxygen pressure and stabilizer concentration on carbonyl build‐up and stabilizer consumption. © 2008 Wiley Periodicals, Inc. J Appl Polym Sci, 2008
- 10 September 2008
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 110 (6) , 3313-3321
Accelerated ageing of polypropylene stabilized by phenolic antioxidants under high oxygen pressure
Polypropylene (PP) samples stabilized by a hindered phenol (Irganox 1010) were submitted to thermal ageing at 80°C in air at atmospheric pressure or in pure oxygen at 5.0 MPa pressure. Both the polymer oxidation and the stabilizer consumption were monitored by Infrared spectrometry and thermal analysis. The stabilizer efficiency, as assessed by the ratio induction time/stabilizer concentration is almost constant at atmospheric pressure even when the stabilizer concentration is higher than its solubility limit in PP (0.4% or 24 × 10−3 mol L−1). In contrast, at high pressure, the efficiency decreases almost hyperbolically with the stabilizer concentration when this latter is higher than 6.0 × 10−3 mol L−1. The results indicate the existence of a direct phenol‐oxygen reaction negligible at low oxygen pressure but significant at 5.0 MPa pressure. The reality of this reaction has been proved on the basis of a study of the thermal oxidation of a phenol solution in a nonoxidizable solvent. A kinetic model of PP oxidation in which stabilization involves three reactions has been proposed. It simulates correctly the effect of oxygen pressure and stabilizer concentration on carbonyl build‐up and stabilizer consumption. © 2008 Wiley Periodicals, Inc. J Appl Polym Sci, 2008
- 15 November 2007
- Published by Springer Nature in Journal of Materials Science
- Vol. 43 (3) , 1026-1032
Embrittlement of polypropylene fibre during thermal oxidation
- 15 November 2007
- Published by Springer Nature in Journal of Materials Science
- Vol. 43 (3) , 1026-1032
Embrittlement of polypropylene fibre during thermal oxidation
- 25 October 2007
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 107 (3) , 1783-1792
Thermooxidative ageing of polyoxymethylene, part 1: Chemical aspects
The thermal oxidation of unstabilised POM homopolymer has been studied at 90, 110, and 130°C under various oxygen pressures ranging from 0 to 2.0 MPa by gravimetry and IR spectrometry. This latter reveals essentially the formation of formate (F) groups and alcohols in smaller quantities. The formate growth and mass loss rates increase pseudo hyperbolically with oxygen pressure, the asymptotic level being reached at pressures up to 0.5 MPa. These results lead to propose a mechanistic scheme of radical chain oxidation in which depolymerization is initiated by hydroperoxide unimolecular decomposition, one formate and one chain scission being formed per decomposition event whereas the kinetic chain length of the depolymerization zip is of the order of 100. A kinetic model derived from the mechanistic scheme, taking into account substrate consumption, simulates correctly the shape of kinetic curves and the effect of temperature and oxygen pressure. © 2007 Wiley Periodicals, Inc. J Appl Polym Sci, 2008
- 25 October 2007
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 107 (3) , 1783-1792
Thermooxidative ageing of polyoxymethylene, part 1: Chemical aspects
The thermal oxidation of unstabilised POM homopolymer has been studied at 90, 110, and 130°C under various oxygen pressures ranging from 0 to 2.0 MPa by gravimetry and IR spectrometry. This latter reveals essentially the formation of formate (F) groups and alcohols in smaller quantities. The formate growth and mass loss rates increase pseudo hyperbolically with oxygen pressure, the asymptotic level being reached at pressures up to 0.5 MPa. These results lead to propose a mechanistic scheme of radical chain oxidation in which depolymerization is initiated by hydroperoxide unimolecular decomposition, one formate and one chain scission being formed per decomposition event whereas the kinetic chain length of the depolymerization zip is of the order of 100. A kinetic model derived from the mechanistic scheme, taking into account substrate consumption, simulates correctly the shape of kinetic curves and the effect of temperature and oxygen pressure. © 2007 Wiley Periodicals, Inc. J Appl Polym Sci, 2008
- 28 January 2005
- Published by Wiley in Polymer Engineering & Science
- Vol. 45 (3) , 424-431
EWF method to study long term fracture properties of cross‐linked polyethylene
The influence of cross‐linking on fracture properties of polyethylene has been studied by the method of essential work of fracture (EWF). Three distinct values of the cross‐link density were obtained by β irradiation with three distinct radiation doses, and characterized by sol‐gel and solvent swelling measurements. EWF tests were performed at speeds of 0.045 to 100 mm min–1 at 80 and 110°C. The fracture toughness, as defined from the EWF method, is analyzed through essential (we) and nonessential (βwp) components. Both values were found to be decreasing functions of the cross‐link density. But cross‐linking also suppresses the toughness decrease observed in linear PE at low speeds/high temperatures. It is hypothesized that cross‐linking prevents the chain disentanglement that occurs during crack growth. In conclusion, EWF tests performed at low speeds appear as an interesting method to characterize the influence of structural factors on the fracture properties of polyethylene. POLYM. ENG. SCI., 45:424–431, 2005. © 2005 Society of Plastics Engineers
- 28 January 2005
- Published by Wiley in Polymer Engineering & Science
- Vol. 45 (3) , 424-431
EWF method to study long term fracture properties of cross‐linked polyethylene
The influence of cross‐linking on fracture properties of polyethylene has been studied by the method of essential work of fracture (EWF). Three distinct values of the cross‐link density were obtained by β irradiation with three distinct radiation doses, and characterized by sol‐gel and solvent swelling measurements. EWF tests were performed at speeds of 0.045 to 100 mm min–1 at 80 and 110°C. The fracture toughness, as defined from the EWF method, is analyzed through essential (we) and nonessential (βwp) components. Both values were found to be decreasing functions of the cross‐link density. But cross‐linking also suppresses the toughness decrease observed in linear PE at low speeds/high temperatures. It is hypothesized that cross‐linking prevents the chain disentanglement that occurs during crack growth. In conclusion, EWF tests performed at low speeds appear as an interesting method to characterize the influence of structural factors on the fracture properties of polyethylene. POLYM. ENG. SCI., 45:424–431, 2005. © 2005 Society of Plastics Engineers