PERFORMANCE OF AN ENVIRONMENTAL PROTECTION LINER AFTER LABORATORY UV EXPOSURE
Authors:
- Fernando Luiz LavoieFernando Luiz Lavoie
- Marcelo KobelnikMKMarcelo Kobelnik
- Clever ValentinCVClever Valentin
- Érica Fernanda TirelliÉTÉrica Fernanda Tirelli
- Maria LopesMLMaria Lopes
- Jefferson da SilvaJSJefferson da Silva
- 1 January 2025
- journal article
- research article
- Published by Sociedade Brasileira de Quimica (SBQ) in Química Nova
- Vol. 48 (2)
Abstract
High-density polyethylene (HDPE) geomembranes are commonly used as an environmental protection liner due to their good chemical and mechanical resistances and low cost. Ultraviolet (UV) radiation is an essential issue in durability studies for pond applications. This study evaluated a 1.5-mm thick HDPE geomembrane exposed to ultraviolet fluorescent radiation for 8760 h in a laboratory and thermoanalytical and physical analyses were conducted towards the understanding of its performance after exposure. According to the results, although the geomembrane maintained the ductile behavior, it showed a 52.48% final decrease in stress crack resistance (SCR) compared to virgin SCR. Moreover, a considerable antioxidant depletion occurred after 8760 h exposure shown by the Std. OIT (standard oxidative-induction time) results, demonstrating a Std. OIT value decrease of 89.19% compared to the virgin Std. OIT. Such a behavior contributed to the susceptibility of thermal effects in the DSC (differential scanning calorimetry) curves and the losses observed in the SCR values, attesting the geomembrane’s oxidative degradation mechanism occurred and changed the polymer’s structure.Keywords
This publication has 11 references indexed in Scilit:
- Service life of some HDPE geomembranesCase Studies in Construction Materials, 2023
- Evaluation of exhumed HDPE geomembranes used as a liner in Brazilian shrimp farming pondsCase Studies in Construction Materials, 2022
- Representative stress crack resistance of polyolefin geomembranes used in waste managementWaste Management, 2019
- Influence of U.V light on the thermal properties of HDPE/Carbon black compositesCase Studies in Thermal Engineering, 2019
- Antioxidant Depletion and Service Life Prediction for HDPE Geomembranes Exposed to Low-Level Radioactive Waste LeachateJournal of Geotechnical and Geoenvironmental Engineering, 2017
- Ageing of exposed geomembranes at locations with different climatological conditionsCanadian Geotechnical Journal, 2015
- Effect of high temperatures on antioxidant depletion from different HDPE geomembranesGeotextiles and Geomembranes, 2014
- Degradation behaviour of HDPE geomembranes with high and low initial high-pressure oxidative induction timeGeotextiles and Geomembranes, 2014
- The effects of weathering exposure on the physical, mechanical, and thermal properties of high-density polyethylene and poly (vinyl chloride)Materials Research, 2013
- Assessing the photo-degradation of geosynthetics by outdoor exposure and laboratory weatherometerGeotextiles and Geomembranes, 2003