Abstract
: Earth-abundant, copper-zinc-tin-sulfide (CZTS) kesterite, is an attractive absorber material for thin-film solar cells (TFSCs). However, the open circuit voltage deficit (Voc-deficit) resulting from high recombination rate at buffer/absorber interface is one of the major challenges that must be overcome to improve the performance of kesterite-based TFSCs. In this paper, we demonstrate the relationship between device pa-rameters and performances for chemically deposited CdS buffer/CZTS-based heterojunction TFSCs as a function of buffer layer thickness, which could change the CdS/CZTS interface conditions such as conduction band or valence band offsets, to gain deeper insight and under-standing about Voc-deficit behavior from high recombination rate at CdS buffer/kesterite interface. Experimental results show that device pa-rameters and performances are strongly dependent on the CdS buffer thickness. We postulate two meaningful consequences; (i) Device pa-rameters were improved upto a CdS buffer thickness of 70 nm, while they deteriorated at thicker CdS buffer layer. The Voc-deficit in the solar cells improved up to a CdS buffer thickness of 92 nm, and then deteriorated at thicker CdS buffer layer. (ii) The minimum values of device parameters obtained at 70 nm CdS thickness in the CZTS TFSCs. Finally, the highest conversion efficiency of 8.77% (Voc: 494 mV, Jsc: 34.54 mA/cm2, FF: 51%) is obtained by applying to the Cu2ZnSn(S,Se)4 (CZTSSe) absorber layer using 70 nm thick CdS buffer.
Funding Information
  • National Research Foundation of Korea (NRF-2015R1C1A1A02036616)
  • Korea Institute of Energy Technology Evaluation and Planning (20164030201310)

This publication has 64 references indexed in Scilit: