Effect of Sintering Process on Fabrication of Porous Si3N4/SiC Composites
Authors:
- 10 September 2007
- journal article
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 353-358, 1572-1575
Abstract
Porous SiC/Si3N4 composites were fabricated by reaction between Si3N4 and C powder in 0.5 MPa nitrogen atmosphere at 1700oC, 1800oC and 1900oC for 0.5h, 1h and 2h, respectively. The characteristics of in situ porous Si3N4/SiC composites were further investigated by X-ray diffraction (XRD) and scanning electronic microscopy (SEM). Results show that the SiC particles are very fine. And the transformation from α-Si3N4 to β-Si3N4 is obvious at 1800oC for 2h and at 1900oC. Otherwise, at 1700oC, the formation of rod-like β-Si3N4 is inhibited. The compressive test was conducted at a cross-head speed of 0.5 mm/min to get the basic mechanical performance of the porous ceramics. The highest value of strength of these composites was obtained when sintered at 1800oC for 1h.Keywords
This publication has 4 references indexed in Scilit:
- Mechanical Behavior of Alumina/Poly(methyl methacrylate) NanocompositesMacromolecules, 2004
- Characterization and modeling of mechanical behavior of polymer/clay nanocompositesComposites Science and Technology, 2003
- Porosity and microstructure control of porous ceramics by partial hot pressingJournal of Materials Research, 2001
- Porous Silicon Nitride Materials as Basic CatalystsChemical Engineering & Technology, 2001