Enhancing the Structural and Mechanical Properties of Ti-Zr Alloy through Boron Doping
Open Access
- 1 March 2024
- journal article
- research article
- Published by Igdir University in Iğdır Üniversitesi Fen Bilimleri Enstitüsü Dergisi
- Vol. 14 (1) , 412-421
Abstract
This study aims to improve the structural strength of the commonly used Ti-15Zr alloy in dental applications by investigating the effects of low boron additions. Ti-15Zr alloys containing 1-4% boron have been produced by vacuum arc melting. The phase ratios in the microstructure of the produced alloys vary according to the boron content. With increasing boron content, the ratio of TiB compound in the phase structure increases. The hardness of Ti-Zr-B alloys exhibited a notable increase in correlation with rising boron content. Measured hardness values of 36.31, 39.50, 44.14, and 53.40 displayed a clear upward trend with higher boron percentages. The tensile strength of the Ti-Zr-B alloys exhibits a trend of initially increasing with boron content, reaching its highest value of 888 MPa at 1% boron. The yield strength follows a similar with tensile strengh, with an initial rise from 449 MPa at 0% boron to a peak of 562 MPa at 1% boron content. Beyond this point, the yield strength slightly decreases to 469 MPa at 2% boron but sharply drops to 186 MPa at 4% boron content. As boron content increases in the Ti-Zr-B alloys, the percentage elongation, indicating the material's plastic deformation capacity before fracture, consistently decreases from 17.03% at 0% boron to 0.70% at 4% boron content.Keywords
Funding Information
- Karadeniz Technical University University Scientific Research Projects Coordination Unit (FBA-2020-8810)
This publication has 24 references indexed in Scilit:
- Preparation and characterization of boron-doped titania nano-materials with antibacterial activityApplied Surface Science, 2013
- A Review of Titanium Zirconium (TiZr) Alloys for Use in Endosseous Dental ImplantsMaterials, 2012
- Evolution of microstructure and tensile properties of in situ titanium matrix composites with volume fraction of (TiB+TiC) reinforcementsMaterials Science and Engineering: A, 2012
- Streptococcus mutans Biofilm Adhesion on Composite Resin Surfaces After Different Finishing and Polishing TechniquesOperative Dentistry, 2011
- Effect of B addition to hypereutectic Ti-based alloysJournal of Alloys and Compounds, 2009
- Structure, mechanical properties and grindability of dental Ti–10Zr–X alloysMaterials Science and Engineering: C, 2009
- Structure, mechanical properties, and grindability of dental Ti–Zr alloysJournal of Materials Science: Materials in Medicine, 2008
- Grain refinement of cast titanium alloys via trace boron additionScripta Materialia, 2005
- Influence of boron addition on microstructure and mechanical properties of dental cast titanium alloysMaterials Science and Engineering: A, 2003
- Mechanical properties of the binary titanium‐zirconium alloys and their potential for biomedical materialsJournal of Biomedical Materials Research, 1995