Raşit Sezer
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Research Interests
Raşit Sezer has a total of 36 co-authors. Here are the top co-authors by number of shared publications:
- Selim Ertürk
Istanbul Technical University
7 shared publications - Ayşegül Bilen
Istanbul Technical University
6 shared publications Cüneyt Arslan
Department of Metallurgical and Materials Engineering, Istanbul Technical University, Istanbul, Turkey
5 shared publications- Bülent Öztürk
Department of Metallurgical and Materials Engineering, Karadeniz Technical University, Trabzon, Turkey
2 shared publications - Cüneyt Arslan
Metallurgical and Materials Engineering Department, Istanbul Technical University, Istanbul, Turkey
2 shared publications Emre Yilmaz
Istanbul Technical University
2 shared publications
Latest Publications
- 15 September 2026
- Published by Gumushane University Journal of Science and Technology Institute in Gümüşhane Üniversitesi Fen Bilimleri Enstitüsü Dergisi
- Vol. 16 (4) , 1117-1128
Interaction between strontium sulfate and boric acid at high temperatures in the presence of activated charcoal
In this study, the interaction between strontium sulfate (SrSO4) and boric acid (H3BO3), both in the absence and presence of activated charcoal (C), was investigated at high temperatures using an SrSO4:H3BO3 molar ratio of 1:2, which corresponds to the stoichiometric composition of strontium metaborate (SrB2O4). It was found that in the absence of C, SrSO4 and H3BO3 did not interact to form SrB2O4 upon heating at either 1073 K and 1273 K, probably due to the very high thermal stability of SrSO4. In contrast, in the presence of C, heating at 1073 K resulted in the formation of minor amounts of strontium borate phases, such as SrB6O10 and SrB4O7, whereas the SrB2O4 phase was formed upon heating at 1273 K. The formation of SrB2O4 was further confirmed by Fourier transform infrared spectroscopy analysis. Furthermore, when reagent-grade SrSO4 was replaced with natural SrSO4 (celestine) in the starting mixture containing H3BO3 and C, the formation of SrB2O4 was also achieved at 1273 K. Because of the promising results obtained for strontium metaborate, this study should be extended for the preparation other strontium and alkaline earth metal (i.e., Ca) borates from corresponding naturally abundant sulfates that are usually not preferred as the starting compounds in high-temperature solid-state synthesis studies.
- 15 September 2026
- Published by Gumushane University Journal of Science and Technology Institute in Gümüşhane Üniversitesi Fen Bilimleri Enstitüsü Dergisi
- Vol. 16 (4) , 1117-1128
Interaction between strontium sulfate and boric acid at high temperatures in the presence of activated charcoal
In this study, the interaction between strontium sulfate (SrSO4) and boric acid (H3BO3), both in the absence and presence of activated charcoal (C), was investigated at high temperatures using an SrSO4:H3BO3 molar ratio of 1:2, which corresponds to the stoichiometric composition of strontium metaborate (SrB2O4). It was found that in the absence of C, SrSO4 and H3BO3 did not interact to form SrB2O4 upon heating at either 1073 K and 1273 K, probably due to the very high thermal stability of SrSO4. In contrast, in the presence of C, heating at 1073 K resulted in the formation of minor amounts of strontium borate phases, such as SrB6O10 and SrB4O7, whereas the SrB2O4 phase was formed upon heating at 1273 K. The formation of SrB2O4 was further confirmed by Fourier transform infrared spectroscopy analysis. Furthermore, when reagent-grade SrSO4 was replaced with natural SrSO4 (celestine) in the starting mixture containing H3BO3 and C, the formation of SrB2O4 was also achieved at 1273 K. Because of the promising results obtained for strontium metaborate, this study should be extended for the preparation other strontium and alkaline earth metal (i.e., Ca) borates from corresponding naturally abundant sulfates that are usually not preferred as the starting compounds in high-temperature solid-state synthesis studies.
- Open Access
- 31 July 2026
- Published by IOP Publishing in Modelling and Simulation in Materials Science and Engineering
- Vol. 34 (6) , 065001
Investigating the role of nickel in CoCrFeMnNi x high-entropy alloys: thermodynamic analysis and molecular dynamics simulations
The influence of Ni content on phase stability and deformation mechanisms in CoCrFeMnNi x high-entropy alloys (HEAs) was investigated using high-entropy alloys predicting software descriptors, CALPHAD, and molecular dynamics (MD) simulations. Increasing Ni content raises the valence electron concentration from 7.50 to 8.00, decreases atomic-size mismatch from 3.51% to 3.27%, and shifts the mixing enthalpy and Gibbs free energy toward more negative values, indicating improved solid-solution stability. CALPHAD calculations show that Ni enhances face-centered cubic (FCC) stability while reducing the equilibrium tendency of secondary phase formation. MD relaxation reveals progressive lattice contraction and increasingly negative cohesive energies, suggesting enhanced energetic stability of the FCC-based random solid-solution models. Under constrained uniaxial-strain tensile deformation at 300 K, all compositions exhibit comparable axial stiffness (∼176–183 GPa) and ultra-high peak axial stresses (∼18–20 GPa) characteristic of defect-free single-crystals. Among the investigated alloys, equiatomic CoCrFeMnNi shows the highest ideal tensile resistance. Plastic deformation is governed primarily by Shockley partial dislocation activity, stacking-fault formation, and HCP-like faulted regions. Generalized stacking fault energy (SFE) calculations show that Ni addition increases the unstable stacking fault barrier from approximately 167.84–224.09 mJ m −2 , while shifting the intrinsic SFE from −63.59 to −30.59 mJ m −2 . The negative intrinsic stacking fault energies indicate that HCP-like faulted configurations are energetically favored relative to the FCC reference at 0 K within the employed 2NN-MEAM framework. However, the progressive shift toward less negative values with increasing Ni content shows that Ni makes these faulted configurations progressively less favorable while increasing the resistance to leading Shockley partial nucleation.
- 31 July 2026
- Published by IOP Publishing in Modelling and Simulation in Materials Science and Engineering
- Vol. 34 (6) , 065001
Open AccessInvestigating the role of nickel in CoCrFeMnNi x high-entropy alloys: thermodynamic analysis and molecular dynamics simulations
The influence of Ni content on phase stability and deformation mechanisms in CoCrFeMnNi x high-entropy alloys (HEAs) was investigated using high-entropy alloys predicting software descriptors, CALPHAD, and molecular dynamics (MD) simulations. Increasing Ni content raises the valence electron concentration from 7.50 to 8.00, decreases atomic-size mismatch from 3.51% to 3.27%, and shifts the mixing enthalpy and Gibbs free energy toward more negative values, indicating improved solid-solution stability. CALPHAD calculations show that Ni enhances face-centered cubic (FCC) stability while reducing the equilibrium tendency of secondary phase formation. MD relaxation reveals progressive lattice contraction and increasingly negative cohesive energies, suggesting enhanced energetic stability of the FCC-based random solid-solution models. Under constrained uniaxial-strain tensile deformation at 300 K, all compositions exhibit comparable axial stiffness (∼176–183 GPa) and ultra-high peak axial stresses (∼18–20 GPa) characteristic of defect-free single-crystals. Among the investigated alloys, equiatomic CoCrFeMnNi shows the highest ideal tensile resistance. Plastic deformation is governed primarily by Shockley partial dislocation activity, stacking-fault formation, and HCP-like faulted regions. Generalized stacking fault energy (SFE) calculations show that Ni addition increases the unstable stacking fault barrier from approximately 167.84–224.09 mJ m −2 , while shifting the intrinsic SFE from −63.59 to −30.59 mJ m −2 . The negative intrinsic stacking fault energies indicate that HCP-like faulted configurations are energetically favored relative to the FCC reference at 0 K within the employed 2NN-MEAM framework. However, the progressive shift toward less negative values with increasing Ni content shows that Ni makes these faulted configurations progressively less favorable while increasing the resistance to leading Shockley partial nucleation.
- Open Access
Milling-Assisted Leaching for Mercury Stabilization and Material Recovery from End-of-Life Fluorescent Lamps
The disposal of end-of-life fluorescent lamps presents significant environmental challenges due to their mercury (Hg) content and the loss of valuable rare earth elements (REEs) contained in phosphor powders, highlighting the need for sustainable recycling strategies. This study proposes an integrated hydrometallurgical process for simultaneous mercury removal and material recovery from spent fluorescent lamps. Various leaching agents were initially evaluated for mercury dissolution, and 10% NaOCl was identified as the most effective solution. The optimized system was applied to linear T8 lamps using a combined milling–leaching approach, followed by size-based separation of metallic, glass, and phosphor fractions. Dissolved mercury was precipitated at pH 11 using Na2S, forming crystalline α-HgS (cinnabar), as confirmed by XRD, and reducing the residual mercury concentration to 2.7 µg/L. The metallic fraction was recovered as an aluminum-based alloy containing 20.6 wt.% Cu and 10.9 wt.% Zn with low iron content, while the phosphor-rich fraction yielded approximately 50% REE extraction, followed by oxalate precipitation of yttrium-based compounds. The developed process enables efficient mercury stabilization and selective recovery of valuable materials, supporting environmentally secure and resource-efficient fluorescent lamp recycling.
Open AccessMilling-Assisted Leaching for Mercury Stabilization and Material Recovery from End-of-Life Fluorescent Lamps
The disposal of end-of-life fluorescent lamps presents significant environmental challenges due to their mercury (Hg) content and the loss of valuable rare earth elements (REEs) contained in phosphor powders, highlighting the need for sustainable recycling strategies. This study proposes an integrated hydrometallurgical process for simultaneous mercury removal and material recovery from spent fluorescent lamps. Various leaching agents were initially evaluated for mercury dissolution, and 10% NaOCl was identified as the most effective solution. The optimized system was applied to linear T8 lamps using a combined milling–leaching approach, followed by size-based separation of metallic, glass, and phosphor fractions. Dissolved mercury was precipitated at pH 11 using Na2S, forming crystalline α-HgS (cinnabar), as confirmed by XRD, and reducing the residual mercury concentration to 2.7 µg/L. The metallic fraction was recovered as an aluminum-based alloy containing 20.6 wt.% Cu and 10.9 wt.% Zn with low iron content, while the phosphor-rich fraction yielded approximately 50% REE extraction, followed by oxalate precipitation of yttrium-based compounds. The developed process enables efficient mercury stabilization and selective recovery of valuable materials, supporting environmentally secure and resource-efficient fluorescent lamp recycling.
- 31 January 2026
- Published by Turkish Journal of Analytical Chemistry in Turkish Journal of Analytical Chemistry
- Vol. 8 (1) , 20-28
Synthesis of high beta-phase content granules from recycled PVDF material: Effect of process parameters and ceramic fillers
Polyvinylidene fluoride (PVDF) is a high-performance polymer utilized in biomedical, electronic, and energy applications due to its piezoelectricity, thermal stability, and mechanical strength. These properties are closely linked to its ability to crystallize into several polymorphic phases, most importantly, the electroactive beta-phase. This study proposes a sustainable method to fabricate beta-phase-rich PVDF granules by recycling used PVDF rods, dissolving the material in DMF, and precipitating it into deionized water at controlled temperatures. The process conditions, including precipitation temperature and PVDF concentration, were systematically investigated for their effect on beta-phase formation. Additionally, the influence of ceramic fillers, Strontium Titanate (SrTiO₃) and Nickel Ferrite (NiFe₂O₄), on phase composition was evaluated. Fourier Transform Infrared (FTIR) Spectroscopy was used to quantify the relative content of the electroactive beta-phase and the non-polar alpha-phase. The results indicate that low precipitation temperatures (0°C) and higher PVDF concentrations (1:10 PVDF/DMF ratio) significantly enhance beta-phase formation, with beta/alpha ratios often exceeding 0.90 at 0°C. Furthermore, NiFe₂O₄ fillers considerably promoted beta-phase crystallization, especially at 0°C, achieving beta/alpha ratios up to ~1.0 for 60% loading. In contrast, SrTiO₃ fillers suppressed beta-phase formation. This upcycling approach not only contributes to waste valorization but also enables the development of functional materials for piezoelectric applications.
- 31 January 2026
- Published by Turkish Journal of Analytical Chemistry in Turkish Journal of Analytical Chemistry
- Vol. 8 (1) , 20-28
Synthesis of high beta-phase content granules from recycled PVDF material: Effect of process parameters and ceramic fillers
Polyvinylidene fluoride (PVDF) is a high-performance polymer utilized in biomedical, electronic, and energy applications due to its piezoelectricity, thermal stability, and mechanical strength. These properties are closely linked to its ability to crystallize into several polymorphic phases, most importantly, the electroactive beta-phase. This study proposes a sustainable method to fabricate beta-phase-rich PVDF granules by recycling used PVDF rods, dissolving the material in DMF, and precipitating it into deionized water at controlled temperatures. The process conditions, including precipitation temperature and PVDF concentration, were systematically investigated for their effect on beta-phase formation. Additionally, the influence of ceramic fillers, Strontium Titanate (SrTiO₃) and Nickel Ferrite (NiFe₂O₄), on phase composition was evaluated. Fourier Transform Infrared (FTIR) Spectroscopy was used to quantify the relative content of the electroactive beta-phase and the non-polar alpha-phase. The results indicate that low precipitation temperatures (0°C) and higher PVDF concentrations (1:10 PVDF/DMF ratio) significantly enhance beta-phase formation, with beta/alpha ratios often exceeding 0.90 at 0°C. Furthermore, NiFe₂O₄ fillers considerably promoted beta-phase crystallization, especially at 0°C, achieving beta/alpha ratios up to ~1.0 for 60% loading. In contrast, SrTiO₃ fillers suppressed beta-phase formation. This upcycling approach not only contributes to waste valorization but also enables the development of functional materials for piezoelectric applications.
- 28 December 2025
- Published by Elsevier in Materials Chemistry and Physics
- Vol. 351
Production and characterization of AlCuMgMnZn high entropy alloy prepared by hot pressing
- 28 December 2025
- Published by Elsevier in Materials Chemistry and Physics
- Vol. 351
Production and characterization of AlCuMgMnZn high entropy alloy prepared by hot pressing
- 5 December 2025
- Published by Walter de Gruyter GmbH in Materials Testing
- Vol. 68 (1) , 121-126
Influence of electronic wastes on the wear and corrosion properties of aluminum matrix composites
In this study, the influence of electronic waste reinforcement on the properties of aluminum was investigated. For this purpose, samples were produced with hot pressing at 600 °C. The reinforcement ratio for the composites was determined as 1 wt.%, 5 wt.%, and 10 wt.%. The wear and corrosion behavior of the samples were investigated by dry sliding wear test and electrochemical corrosion tests. The wear rate values indicated that the increasing reinforcement ratio reduced the wear rate. Moreover, it was determined that the increasing reinforcement ratio improved the corrosion behavior of the composites. The corrosion rate of the samples was reduced with an increasing reinforcement ratio, and a more stable surface was obtained in corrosion environment. In conclusion, it was deduced that Rh, Ag, Pt, and Sn containing electronic waste provided significant improvements in wear and corrosion behaviors.
- 5 December 2025
- Published by Walter de Gruyter GmbH in Materials Testing
- Vol. 68 (1) , 121-126
Influence of electronic wastes on the wear and corrosion properties of aluminum matrix composites
In this study, the influence of electronic waste reinforcement on the properties of aluminum was investigated. For this purpose, samples were produced with hot pressing at 600 °C. The reinforcement ratio for the composites was determined as 1 wt.%, 5 wt.%, and 10 wt.%. The wear and corrosion behavior of the samples were investigated by dry sliding wear test and electrochemical corrosion tests. The wear rate values indicated that the increasing reinforcement ratio reduced the wear rate. Moreover, it was determined that the increasing reinforcement ratio improved the corrosion behavior of the composites. The corrosion rate of the samples was reduced with an increasing reinforcement ratio, and a more stable surface was obtained in corrosion environment. In conclusion, it was deduced that Rh, Ag, Pt, and Sn containing electronic waste provided significant improvements in wear and corrosion behaviors.
- Open Access
- 1 March 2024
- Published by Igdir University in Iğdır Üniversitesi Fen Bilimleri Enstitüsü Dergisi
- Vol. 14 (1) , 412-421
Enhancing the Structural and Mechanical Properties of Ti-Zr Alloy through Boron Doping
This study aims to improve the structural strength of the commonly used Ti-15Zr alloy in dental applications by investigating the effects of low boron additions. Ti-15Zr alloys containing 1-4% boron have been produced by vacuum arc melting. The phase ratios in the microstructure of the produced alloys vary according to the boron content. With increasing boron content, the ratio of TiB compound in the phase structure increases. The hardness of Ti-Zr-B alloys exhibited a notable increase in correlation with rising boron content. Measured hardness values of 36.31, 39.50, 44.14, and 53.40 displayed a clear upward trend with higher boron percentages. The tensile strength of the Ti-Zr-B alloys exhibits a trend of initially increasing with boron content, reaching its highest value of 888 MPa at 1% boron. The yield strength follows a similar with tensile strengh, with an initial rise from 449 MPa at 0% boron to a peak of 562 MPa at 1% boron content. Beyond this point, the yield strength slightly decreases to 469 MPa at 2% boron but sharply drops to 186 MPa at 4% boron content. As boron content increases in the Ti-Zr-B alloys, the percentage elongation, indicating the material's plastic deformation capacity before fracture, consistently decreases from 17.03% at 0% boron to 0.70% at 4% boron content.
- 1 March 2024
- Published by Igdir University in Iğdır Üniversitesi Fen Bilimleri Enstitüsü Dergisi
- Vol. 14 (1) , 412-421
Open AccessEnhancing the Structural and Mechanical Properties of Ti-Zr Alloy through Boron Doping
This study aims to improve the structural strength of the commonly used Ti-15Zr alloy in dental applications by investigating the effects of low boron additions. Ti-15Zr alloys containing 1-4% boron have been produced by vacuum arc melting. The phase ratios in the microstructure of the produced alloys vary according to the boron content. With increasing boron content, the ratio of TiB compound in the phase structure increases. The hardness of Ti-Zr-B alloys exhibited a notable increase in correlation with rising boron content. Measured hardness values of 36.31, 39.50, 44.14, and 53.40 displayed a clear upward trend with higher boron percentages. The tensile strength of the Ti-Zr-B alloys exhibits a trend of initially increasing with boron content, reaching its highest value of 888 MPa at 1% boron. The yield strength follows a similar with tensile strengh, with an initial rise from 449 MPa at 0% boron to a peak of 562 MPa at 1% boron content. Beyond this point, the yield strength slightly decreases to 469 MPa at 2% boron but sharply drops to 186 MPa at 4% boron content. As boron content increases in the Ti-Zr-B alloys, the percentage elongation, indicating the material's plastic deformation capacity before fracture, consistently decreases from 17.03% at 0% boron to 0.70% at 4% boron content.
- 31 December 2023
- Published by Elsevier in Materials Letters
- Vol. 358
Properties of Al/Y2O3 composites produced by Y2O3-Al2O3 interaction in powder metallurgy route
- 31 December 2023
- Published by Elsevier in Materials Letters
- Vol. 358
Properties of Al/Y2O3 composites produced by Y2O3-Al2O3 interaction in powder metallurgy route